Towards the development of safer by design mineral photocatalytic paint: influence of the TiO2 modifications on particle release

Abstract

The development of safe nanomaterials has become a significant concern in various industry sectors using advanced materials. While there is variability in the definitions of Safe(r) by Design (SbD), the general concept is to minimise environmental, health and safety concerns implementing appropriate measures at an early stage of product design to control exposure and hazard, thus reducing risks. The SbD product strategy applied in this paper refers to the mitigation of exposure by the identification of release scenarios during the use and the end of life of the nano-enabled products (NEPs) that include engineered nanomaterials (ENMs). This strategy was applied to the development of a photocatalytic mineral paint containing TiO2 engineered nanomaterial. This ENM was then incorporated into a mineral matrix-based paint for photocatalytic application. The different paint formulations were applied to standardised substrates and artificially weathered in an accelerated weathering chamber with controlled parameters. Mechanical solicitation that simulate end of life (EoL) of the paint, through abrasion tests, were performed to assess the potential emission of airborne particles that could lead to human or environmental exposure. The release evaluation confirms that paints with TiO2 nanoparticles without SbD coating release more nanometric particles due to strong matrix degradation. The TiO2 nanoparticles coated with PEG or grafted onto CNC does not completely prevent the degradation of the paint surface during ageing. However, this degradation does not necessarily lead to an increase in aerosol emission. The coating degradation during accelerated ageing limits the degradation of the paint matrix, preventing the release of unbound TiO2 nanoparticles. Understanding the mechanisms of release and how they are influenced by the ENMs, the matrix material and the process characteristics is crucial for the exposure and risk assessment approach in occupational settings involving engineered nanomaterials. Moreover, establishing release rates makes it possible to increase the reliability of SbD e-infrastructure for performance testing and the implementation of Safe-by-Design approaches in the nanotechnology supply chain.

Supplementary files

Transparent peer review

To support increased transparency, we offer authors the option to publish the peer review history alongside their article.

View this article’s peer review history

Article information

Article type
Paper
Submitted
26 iyl 2024
Accepted
16 dek 2024
First published
18 dek 2024

Environ. Sci.: Nano, 2025, Accepted Manuscript

Towards the development of safer by design mineral photocatalytic paint: influence of the TiO2 modifications on particle release

A. Rosset, I. Michaud-Soret, I. Capron, H. Voisin, G. Brochard, V. Bergé, A. Benayad, A. Guiot, S. Clavaguera and S. Artous , Environ. Sci.: Nano, 2025, Accepted Manuscript , DOI: 10.1039/D4EN00681J

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements