Experiments about single pit initiation and propagation were performed on 316L stainless steel with the aim to determine the pitting corrosion behaviour for nuclear waste containers. The experimental setup permits to control the pit development at will and to create reproducible single pits in three dimensions. Radial and deep evolutions of a disc shaped pit were studied for propagation times of up to 10 hours. These evolutions were used to determine what limiting mechanism takes place during long-term pit propagation. Special attention has been paid to the chloride ion action on pitting. A minimum chloride concentration was found to be necessary in the bulk electrolyte to support pit propagation. The existence of a critical pit depth of 230 μm was also underlined.

Associated articles

Supplementary files

Article information

Article type
Paper
Submitted
08 Dec 2014
Accepted
02 Feb 2015
First published
04 Feb 2015
This article is Open Access
Creative Commons BY license

Faraday Discuss., 2015,180, 267-282

Author version available

Initiation and propagation of a single pit on stainless steel using a local probe technique

S. Heurtault, R. Robin, F. Rouillard and V. Vivier, Faraday Discuss., 2015, 180, 267 DOI: 10.1039/C4FD00252K

This article is licensed under a Creative Commons Attribution 3.0 Unported Licence. You can use material from this article in other publications without requesting further permissions from the RSC, provided that the correct acknowledgement is given.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements