We report a facile, green and generalized method of endogenous growth of 2D boehmite nanosheets (ns) on a 3D network using Al-fibers through oxidation reaction between the Al metal and H2O (2Al + 4H2O = 2AlOOH + 3H2). Such Al-fiber@ns-AlOOH composites have substantial potential applications for microfibrous-structured catalysts and catalytic reactors, being verified by several hot-topic reactions such as CO oxidative coupling to dimethyl oxalate.

Graphical abstract: Endogenous growth of 2D AlOOH nanosheets on a 3D Al-fiber network via steam-only oxidation in application for forming structured catalysts

Supplementary files

Article information

Article type
Communication
Submitted
10 Mar 2015
Accepted
22 May 2015
First published
28 May 2015

Green Chem., 2015,17, 3762-3765

Endogenous growth of 2D AlOOH nanosheets on a 3D Al-fiber network via steam-only oxidation in application for forming structured catalysts

C. Wang, L. Han, Q. Zhang, Y. Li, G. Zhao, Y. Liu and Y. Lu, Green Chem., 2015, 17, 3762 DOI: 10.1039/C5GC00530B

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements