Abstract

Metallic inks with superior conductivity and printability are necessary for high-throughput manufacturing of printed electronics. In particular, gallium-based liquid metal inks have shown great potential in creating soft, flexible and stretchable electronics. Despite their metallic composition, as-printed liquid metal nanoparticle films are non-conductive due to the surrounding metal oxide shells which are primarily Ga2O3, a wide-bandgap semiconductor. Hence, these films require a sintering process to recover their conductivity. For conventional solid metallic nanoparticles, thermal and laser processing are two commonly used sintering methods, and the sintering mechanism is well understood. Nevertheless, laser sintering of liquid metal nanoparticles was only recently demonstrated, and to date, the effect of thermal sintering has rarely been investigated. Here, eutectic gallium–indium nanoparticle films are processed separately by laser or thermal sintering in an ambient environment. Laser and thermally sintered films are compared with respect to electrical conductivity, surface morphology and elemental composition, crystallinity and surface composition. Both methods impart thermal energy to the films and generate thermal stress in the particles, resulting in rupture of the gallium oxide shells and achieving electrical conductivity across the film. For laser sintering, extensive oxide rupture allows liquid metal cores to flow out and coalesce into conductive pathways. For thermal sintering, due to less thermal stress and more oxidation, the oxide shells only rupture locally and extensive phase segregation occurs, leading to non-liquid particle films at room temperature. Electrical conductivity is instead attributed to segregated metal layers and gallium oxide which becomes crystalline and conductive at high temperatures. This comprehensive comparison confirms the necessity of oxidation suppression and significant thermal stress via instantaneous laser irradiation to achieve conductive patterns in liquid form.

Graphical abstract: Oxide rupture-induced conductivity in liquid metal nanoparticles by laser and thermal sintering

Supplementary files

Article information

Article type
Paper
Submitted
07 May 2019
Accepted
30 Jun 2019
First published
01 Jul 2019

Nanoscale, 2019,11, 17615-17629

Author version available

Oxide rupture-induced conductivity in liquid metal nanoparticles by laser and thermal sintering

S. Liu, S. N. Reed, M. J. Higgins, M. S. Titus and R. Kramer-Bottiglio, Nanoscale, 2019, 11, 17615 DOI: 10.1039/C9NR03903A

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements