Issue 14, 2022

Electronic influence of ultrathin aluminum oxide on the transistor device performance of binary indium/tin oxide films

Abstract

Heterostack thin-film transistors (TFTs) with an active layer comprising indium-, tin-, and aluminum oxide (ITAO) were fabricated using atomic layer deposition (ALD) to investigate the influence of aluminum oxide on the TFT performance parameters. Deposition of the quaternary heterostacks was accomplished at 200 °C using trimethylindium (TMI), tetrakis(dimethylamino)tin (TDMASn), trimethylaluminum (TMA), and water as oxidizing agent. By adjusting the number of Al2O3 cycles, while keeping the ratio of In2O3 to SnO2 constant, ITAO films with a well-defined Al2O3 content were obtained as confirmed by X-ray photoelectron spectroscopy (XPS). The stacked structure of the thin-films, as well as the uniform thickness was verified by high resolution transmission electron microscopy (HRTEM). The thin-film composition of the ternary ITAO semiconductors could be correlated to their electronic performance. Reducing the aluminum oxide content from three to one cycles in the atomic layer deposition experiment reveals a significant increase in the saturation mobility of nearly 300%, however at the expense of other important transistor parameters. The thus optimized ITAO thin-film exhibits a decent saturation mobility (μsat) of 2.28 cm2 V−1 s−1, a threshold-voltage (Vth) of 6.8 V, a high current on/off ratio (IOn/IOff) of 9.0 × 105, and a low subthreshold swing (SS) of 365.5 mV dec−1, using a large width to length ratio (W/L = 500). Furthermore, the incorporation of aluminum oxide leads to an increase in performance stability towards exposure to background irradiation under transistor operation. The critical transistor performance parameters were altered only to a minor extent when irradiated with energies of 2.0 eV to 3.7 eV. This confirms the enhanced light stability of the TFTs, through employing a wide-band gap material as part of the semiconducting layer.

Graphical abstract: Electronic influence of ultrathin aluminum oxide on the transistor device performance of binary indium/tin oxide films

Supplementary files

Article information

Article type
Paper
Submitted
19 Jan 2022
Accepted
21 Feb 2022
First published
04 Mar 2022
This article is Open Access
Creative Commons BY-NC license

J. Mater. Chem. C, 2022,10, 5447-5457

Electronic influence of ultrathin aluminum oxide on the transistor device performance of binary indium/tin oxide films

M. I. Büschges, V. Trouillet and J. J. Schneider, J. Mater. Chem. C, 2022, 10, 5447 DOI: 10.1039/D2TC00285J

This article is licensed under a Creative Commons Attribution-NonCommercial 3.0 Unported Licence. You can use material from this article in other publications, without requesting further permission from the RSC, provided that the correct acknowledgement is given and it is not used for commercial purposes.

To request permission to reproduce material from this article in a commercial publication, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party commercial publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements