Synthesis and luminescence properties of Yb3+/Er3+-doped Bi2(MoO4)3−z(WO4)z phosphors for optical thermometry†
Abstract
Yb3+/Er3+-doped Bi2(MoO4)3−z(WO4)z phosphors were synthesized via a hydrothermal method combined with subsequent calcination. Under the excitation of a light source of 980 nm, Bi2(MoO4)3:Yb3+/Er3+ phosphors exhibited strong upconversion green light and weak red light emissions. By doping WO42− in Bi2(MoO4)3:Yb3+/Er3+ phosphors, the upconversion luminescence intensity of the phosphors significantly enhanced, which is 42 times higher than that of the undoped WO42− phosphor. With an increase in WO42− doping content, the final color coordinates of Bi2(MoO4)3−z(WO4)z:Yb3+/Er3+ phosphors were (0.2352, 0.7274), which is closer to the standard green CIE coordinates. The maximum CP of WO42−-doped phosphors is as high as 116.68%, which is 74.44% higher than that of the undoped WO42− phosphor. Based on the thermally coupled energy levels (TCLs) of Er3+ (2H11/2/4S3/2 → 4I15/2) in Bi2(MoO4)2.7(WO4)0.3:14%Yb3+,3%Er3+ phosphor, the SR value reached a maximum of 0.0081 K−1 at 323 K and the SA value reached a maximum of 0.0099 K−1 at 398 K. The obtained Bi2(MoO4)3−z(WO4)z:Yb3+/Er3+ phosphors are suitable for upconversion luminescent materials for green displays and have potential advantages in optical temperature measurement.