DOI:
10.1039/C5NR06419H
(Paper)
Nanoscale, 2016,
8, 300-308
Determining the 3D orientation of optically trapped upconverting nanorods by in situ single-particle polarized spectroscopy†
Received
17th September 2015
, Accepted 13th November 2015
First published on 16th November 2015
Abstract
An approach to unequivocally determine the three-dimensional orientation of optically manipulated NaYF4:Er3+,Yb3+ upconverting nanorods (UCNRs) is demonstrated. Long-term immobilization of individual UCNRs inside single and multiple resonant optical traps allow for stable single UCNR spectroscopy studies. Based on the strong polarization dependent upconverted luminescence of UCNRs it is possible to unequivocally determine, in real time, their three-dimensional orientation when optically trapped. In single-beam traps, polarized single particle spectroscopy has concluded that UCNRs orientate parallel to the propagation axis of the trapping beam. On the other hand, when multiple-beam optical tweezers are used, single particle polarization spectroscopy demonstrated how full spatial control over UCNR orientation can be achieved by changing the trap-to-trap distance as well as the relative orientation between optical traps. All these results show the possibility of real time three-dimensional manipulation and tracking of anisotropic nanoparticles with wide potential application in modern nanobiophotonics.
Introduction
Rare earth doped Upconverting Nanoparticles (hereafter UCNPs) have emerged during the last few years as useful fundamental building blocks in modern photonics. UCNPs are being extensively used in a large variety of research fields including solar energy, nanomedicine and bioimaging, among many others.1–8 UCNPs show the unique capability of producing visible (VIS) luminescence under near-infrared (NIR) optical excitation by a multiphoton excitation process known as upconversion.6,9 When compared to other nanomaterials also capable of NIR-to-VIS optical conversion (such as metallic nanoparticles and semiconductor nanocrystals), UCNPs present several remarkable advantages including long-term photochemical stability, narrow emission lines, long luminescence lifetimes, and size-independent spectral shape of their luminescence bands.10–14 Recent studies have also pointed out that, since in UCNPs the multiphoton excitation is assisted by real electronic states, large NIR-to-VIS efficiencies could be achieved upon cw excitation without requiring the use of expensive, ultrafast, high power laser sources (as is the case when using gold nanoparticles or semiconductor nanocrystals).9 This fact boosted the use of UCNPs for optical conversion in solar cells as well as in the development of cost-effective bioimaging equipment.15–17 In the particular field of fluorescence bioimaging, UCNPs are nowadays considered as one of the most promising in vitro luminescence probes because of the low autofluorescence generated by continuous wave NIR optical excitation.18 Moreover, recent studies have demonstrated that some UCNPs are not only capable of in vitro imaging but, in addition, they can also be used as intracellular thermal and chemical sensing units.19–22 In addition, intracellular studies based on single UCNP are nowadays a real possibility as the synthesis of ultra-small (<10 nm in diameter) UCNPs showing large NIR-to-VIS optical conversion efficiencies has been recently demonstrated.23 As a consequence, UCNPs are also being considered as promising optical probes for experiments at single-cell and single-particle levels.
As a result of the intensive research carried out on UCNPs during the last few years, a wide range of UCNPs consisting of different host lattices and dopants have appeared onto the scene.4,24,25 Modifying the different synthesis parameters different emission bands,12 particle sizes23 and morphologies3,4,13,26–28 could be achieved. Among all of them, erbium and ytterbium codoped NaYF4 UCNPs are considered as the reference combination of dopants and host materials.13,23 In particular, the recently demonstrated possibility of synthesizing NaYF4:Er3+,Yb3+ upconverting nanorods (hereafter NaYF4:Er3+,Yb3+ UCNRs) appears to be especially interesting as they constitute a unique system that could be used in a wide range of applications including security inking, cell tracking, cell manipulation, and bottom-up fabrication of nanofluidic and optical devices.14,26,29,30
However, the full exploration of the potential applications of NaYF4:Er3+,Yb3+ UCNRs would require remote three-dimensional control of their spatial arrangement. Such control becomes mandatory for, as an example, the construction of NaYF4:Er3+,Yb3+ UCNR assemblies (interesting for security inking and nanofluidic applications) as well as for controlled incorporation of single NaYF4:Er3+,Yb3+ UCNRs into living cells. At present, several techniques have been demonstrated to be capable of remote manipulation and assembly of different nanorods. These include the application of electric and magnetic fields as well as the use of laminar flows in microfluidic channels.31–33 Despite the good results obtained so far by these techniques, they lack the ability to provide real time three-dimensional spatial control. Optical tweezers are an appealing tool for real time three-dimensional manipulation of nanosized objects in aqueous environments.34,35 First demonstrated by Ashkin and co-workers, Optical Trapping (OT) of sub-micrometric structures is based on the gradient force created in the surroundings of a tightly focused laser beam.36,37 When a nanoparticle is randomly moving close to the laser focus, the optical electric field polarizes the nanoparticle so that it behaves as an electric dipole in a non-homogeneous electric field. As a consequence, the polarized nanoparticle is pushed towards the beam focus. OT and remote manipulation of a great variety of different nanostructures (including metallic nanoparticles, semiconductor nanowires, semiconductor quantum dots (QDs) and, more recently, UCNPs) have been already demonstrated.37–43 In previous experiments, the characterization of the dynamics of trapped nanostructures has been limited to accurate measurements of both the trapping force and particle incorporation rates. Nevertheless, practical applications require a deep understanding of the exact orientation of the optically trapped nanoparticles inside the optical trap. This is a challenging task since conventional approaches cannot be used: the trapped particle size is well below the resolution provided by optical microscopy. Thus, the design and development of non-direct strategies for nanoparticle tracking inside optical traps becomes necessary. As an example, Jauffred et al. determined the position distribution curve of optically trapped QDs by accurate tracking of their two-photon excited emission.37 In the case of highly asymmetric nanoparticles (such as nanorods) not only the position inside the trap is relevant but also their intra-trap orientation needs to be known. Such knowledge has been achieved in the case of optically trapped Gold Nanorods (GNRs) and niobate nanowires by the real time analysis of luminescence and by polarized Second Harmonic Generation, respectively. These pioneering experiments have demonstrated that orientation of asymmetric nanoparticles inside optical traps is far from easy to predict.39,44 Niobate nanowires were found to align along the trapping beam axis whereas GNRs orientated parallel to the polarization vector of the trapping laser beam. It is also worth mentioning that, apart from the particle material, the characteristics of the trapped particle, such as its length in the case of nanorods, deeply affect the way it is trapped.45 Despite the interest from both fundamental and applied point of view neither optical trapping of UCNRs nor their intra-trap orientation has been demonstrated so far.
In this work, a single-beam OT setup has been used to demonstrate stable optical trapping of NaYF4:Er3+,Yb3+ UCNRs, with a highly anisotropic morphology. Resonant optical tweezers, in which the laser trapping radiation is partially absorbed by the optically trapped particle, allowed for real-time detection of the sequential incorporation of NaYF4:Er3+,Yb3+ UCNRs into the optical trap by luminescence microscopy. Single NaYF4:Er3+,Yb3+ UCNR spectroscopy in a dry environment was used to reveal the strong polarization dependence of the VIS luminescence generated by NaYF4:Er3+,Yb3+ UCNRs. This property has been further used, through the analysis of the polarization state of intra-trap luminescence, to unequivocally elucidate the equilibrium orientation of optically trapped NaYF4:Er3+,Yb3+ UCNRs with respect to the laser trapping beam.
Experimental
Synthesis of NaYF4:Er3+,Yb3+ upconverting nanorods
For the synthesis of NaYF4:2%Er3+,18%Yb3+ UCNRs we used a recently published protocol.46 The hydrothermal processing using microwave radiation (MAGNUM II ERTEC MV 02-02 reactor) was used to first prepare the lanthanide nitrate precursor salt (1.2 mM), which was further mixed with 14 mL of deionized water, 0.7 g, (17.5 mM) of NaOH, 7.1 g, (22.6 mM) of oleic acid (90 wt%), 10.0 g (21.7 mM) of ethanol and 0.3 g (7.2 mM) of NaF to obtain a milky homogeneous solution. After 30 min of stirring at room temperature, the solution was transferred into a Teflon vessel, sealed and then placed in a microwave reactor, followed by 8.5 h of hydrothermal processing at 250 °C, under average pressure lower than 25 atm, the solution of NaYF4:Er3+,Yb3+ UCNRs was obtained. The synthesized NaYF4:Er3+,Yb3+ UCNRs were collected by centrifugation at 12000 rpm for 15 min, and washed twice with ethanol. The as-synthesized NaYF4:2%Er3+,18%Yb3+ UCNRs were dispersed in cyclohexane with a concentration of ca. 20 mg mL−1. In order to perform optical trapping experiments it was necessary to transfer NaYF4:Er3+,Yb3+ UCNRs to a distilled water solution, for which we used the ligand removal procedure reported by Bogdan et al.21 Briefly, 1 mL of NaYF4:Er3+,Yb3+ UCNRs in cyclohexane was mixed with 10 ml of deionized water for 2 h, while the pH of the solution was set at 4 with 0.1 M hydrochloric acid. After the reaction the aqueous solution was extracted with excess of cyclohexane to remove oleic acid molecules, further collected by centrifugation at 12000 rpm for 15 min, washed and finally dispersed in distilled water with concentration of ca. 7 mg mL−1. Taking into account the mean size of a single NaYF4:Er3+,Yb3+ UCNR and the density of the bulk NaYF4 matrix the concentration of the solution was recalculated to be ∼1011 NRs per cm3. Distilled water was used as a trapping solution since NaYF4:Er3+,Yb3+ UCNRs present a good colloidal character when dispersed in it without any evidence of agglomeration between the particles (see DLS measurements in Fig. S1†). Moreover, the low density of distilled water facilitates NaYF4:Er3+,Yb3+ UCNR manipulation when trapped since no strong optical forces are needed in order to overtake the drag force. At this point, we should note that distilled water shows a non-negligible absorption coefficient at the trapping wavelength (980 nm). This could lead to the appearance of thermal effects in the surroundings of the trap. According to previous studies, under our experimental conditions, we had estimated that the temperature increment induced by the focused laser radiation is lower than 5 °C. We state that such reduced heating does not affect the optical trapping experiments.47
Optical trapping experimental setup
A single-beam optical tweezers setup is depicted in Fig. 1a. The 980 nm laser radiation coming from a single-mode fiber-coupled laser diode is collimated by a mounted Rochester aspheric lens (Thorlabs, A230TM-B) and then expanded by a 2× beam expander (Thorlabs, BE02M). This laser radiation is used for both optical trapping and to excite NaYF4:Er3+,Yb3+ UCNR luminescence. All the experiments were performed by using the maximum laser power provided by the laser (60 mW). For multiple-beam optical trapping experiments, the single-beam optical trapping setup was modified as schematically illustrated in Fig. S2.† We experimentally observed that the total laser power provided by the 980 nm laser diode was insufficient to form two highly stable optical traps by itself. A second 1064 nm laser beam (Nd:YAG laser, Ventus, Laser Quantum, Photonic Solutions) was used to create two additional traps perfectly overlapping with the 980 nm ones. The 1064 nm beam was made collinear with the 980 nm beam using a beamsplitter (Thorlabs, BS020) to combine the two beams (as seen in Fig. S2†). Then, the collinear laser beams were both split into two by using a second beamsplitter, and then reflected off plane mirrors to recombine them as shown in Fig. S2.† By slightly changing the alignment of either of the plane mirrors it was possible to create a slight angular difference in the propagating beams, resulting in two separate optical traps when focused through a high numerical aperture microscope objective. The laser power at any of these two traps (80 mW) is the sum of the overlapping 980 and 1064 nm laser powers. The extra contribution of the 1064 nm laser beam led to two stable optical traps. In summary, in this configuration, each optical trap is composed of the 1064 nm beam and the 980 nm laser beam; the more powerful laser operating at 1064 nm is used to provide the power for stable optical trapping, while the 980 nm radiation is needed for exciting NaYF4:Er3+,Yb3+ UCNR luminescence (1064 nm absorption does not provide the sufficient emission from the trapped UCNR to perform accurate luminescence analysis). A 100× 1.25 NA oil-immersed microscope objective was used for single NaYF4:Er3+,Yb3+ UCNR experiments while a 10× 0.10 NA microscope objective was used for spectral analysis of the NaYF4:Er3+,Yb3+ UCNRs suspension in order to ensure the analysis of multiple NaYF4:Er3+,Yb3+ UCNRs. For single NaYF4:Er3+,Yb3+ UCNR polarized emission experiments, a drop of the colloidal suspension of NaYF4:Er3+,Yb3+ UCNRs (∼1011 NRs per cm3) was dried on a microscope slide and covered by a cover glass to prevent oil from coming into contact with the sample. For optical trapping experiments, a diluted colloidal suspension of NaYF4:Er3+,Yb3+ UCNRs (∼5 × 109 NRs per cm3) was placed inside a 100 μm height microchannel (Ibidi Inc., μ-Slide I 80106). For the analysis of the colloidal suspension of NaYF4:Er3+,Yb3+ UCNRs (∼1011 NRs per cm3), it was placed inside a spectrometer cuvette (2 mm × 10 mm). For optical imaging a CMOS camera was used. Luminescence analysis was performed by optically coupling to the OT setup a high sensitivity Si CCD camera (Synapse, Horiba) attached to a monochromator (iH320, Horiba). At the entrance of the spectrometer a linear polarizer (Thorlabs, LPNIR050-MP2) mounted on a graduated wheel was placed for the selection of the polarized emission collected from the sample.
|
| Fig. 1 (a). Schematic representation of the experimental setup. (b) Time evolution of the recovered luminescence at the trap position during multiple-particle trapping experiment. Sequential steps denote the incorporation of a single NaYF4:Er3+,Yb3+ UCNR to the optical trap. Luminescence images show the change in the recovered intensity. | |
Results and discussion
Fig. 2a shows a Transmission Electron Microscopy (TEM) image of the NaYF4:Er3+,Yb3+ UCNRs used all along this work. Statistical analysis of the TEM images provided the size histograms included in Fig. 2b from which the NaYF4:Er3+,Yb3+ UCNR diameter and length were determined to be 140 ± 20 nm and 1100 ± 200 nm, respectively. Details of the synthesis method and sample preparation can be found in the Experimental section. Additionally, the crystal structure and detailed spectroscopic characterization of the studied NaYF4:Er3+,Yb3+ UCNRs are published elsewhere.46Fig. 2c shows an optical image of an aqueous suspension of NaYF4:Er3+,Yb3+ UCNRs (0.7 wt%) revealing the excellent colloidal character of our NaYF4:Er3+,Yb3+ UCNRs without any evident signs of precipitation during ensuing days. Fig. 2c also includes the optical image of the same cuvette containing the non-colored solution when optically excited by a 980 nm laser beam obtained by using a 600 nm long-pass filter. A clear red emission is observed that, according to the schematic energy level diagram shown in Fig. 2d, can be attributed to the 4F9/2 → 4I15/2 transition of Er3+ ions, optically excited by an Yb3+ → Er3+ non-radiative energy transfer process.
|
| Fig. 2 (a) TEM image of the studied NaYF4:Er3+,Yb3+ UCNRs. (b) Size histograms obtained of TEM images representing diameter and length of the NaYF4:Er3+,Yb3+ UCNRs. (c) Optical images of the colloidal suspension of NaYF4:Er3+,Yb3+ UCNRs. The transparent colloidal suspension on the left presents a bright red emission when excited with a 980 nm laser beam. (d) Energy levels diagram of the upconversion energy transfer from Yb3+ to Er3+ ions. The transition of the emission levels of interest (652 and 660 nm) in the 4F9/2 band are represented. | |
Dried sample experiments
It is possible to find in the literature numerous examples revealing that highly anisotropic nanoparticles could generate a highly polarized luminescence.48–50 This was firstly demonstrated in non-spherical QDs that show well differentiated polarization states in their luminescence when their aspect ratios (length to diameter ratio) exceed 2.48 Later, a strong polarization anisotropy was discovered in codoped Tm3+ and Yb3+ NaYF4 nanorods with aspect ratios close to 7.49 The exact origin of the polarization anisotropy in rare earth doped NaYF4 UCNRs is still unclear and, up to now, it is far from being fully understood. Indeed, prior to this work, it was not clear whether or not this phenomenon is restricted uniquely to the particular case of Tm3+ and Yb3+ ions. In order to check the possible polarization dependence of the upconversion luminescence generated by NaYF4:Er3+,Yb3+ UCNRs, we have performed single-particle polarized spectroscopy experiments. For this purpose, a drop of the colloidal suspension of NaYF4:Er3+,Yb3+ UCNRs was dried on a microscope slide and imaged by a CMOS camera. The luminescence of a single NaYF4:Er3+,Yb3+ UCNR immobilized on the surface of the microscope slide was achieved by focusing on it a continuous wave 980 nm laser beam by using a high numerical aperture (1.25 NA) microscope objective. The spot size of the 980 nm excitation beam was estimated to be 500 nm in radius. The visible luminescence generated by the NaYF4:Er3+,Yb3+ UCNR was collected by the same microscope objective and, after passing through different filters and confocal apertures, was spectrally analyzed with a CCD camera coupled to a high resolution spectrometer. In this work we have focused our attention on the 4F9/2 → 4I15/2 red emission band as, under our experimental conditions, its intensity was several times higher than that of the green (2H11/2,4S3/2 → 4I15/2) emission, as it can be observed in Fig. S3a of the ESI.† The polarization state of the NIR-excited VIS-luminescence, with respect to the NaYF4:Er3+,Yb3+ UCNR axis, was selected by placing a linear polarizer at the entrance of the spectrometer. Fig. 3a shows the normalized luminescence spectra generated by a single NaYF4:Er3+,Yb3+ UCNR corresponding to polarization states parallel and perpendicular to the NaYF4:Er3+,Yb3+ UCNR axis (see inset in Fig. 3a). As can be observed, the luminescence intensities of the two main peaks (652 and 660 nm) appear to be strongly polarization dependent. This is further evidenced in the two-dimensional map shown in Fig. 3a that includes the dependence of the emitted intensity as a function of the emission polarization angle (with respect to the NaYF4:Er3+,Yb3+ UCNR axis). As can be seen, intensity peaks at 652 nm and 660 nm change with the polarization angle in a cyclic way. Fig. 3b reveals that the intensity ratio between 652 and 660 nm peaks (R652/660) is hypersensitive to the polarization state. Values under and above 1 (inside and outside the red dashed circle) denote two polarization states, one dominated by the 652 nm peak intensity and a second one characterized by reaching the maximum intensity at 660 nm. Note that the R652/660 coefficient varies from 2.5 down to 0.5 when the polarization state is driven from being parallel to perpendicular to the NaYF4:Er3+,Yb3+ UCNR axis. At this point we would like to mention that similar results were obtained when the 2H11/2,4S3/2 → 4I15/2 green emission was analyzed (see Fig. S4 in the ESI†). The large induced polarization variation (five-fold) in the intensity ratio reveals the R652/660 coefficient as a reliable and precise parameter to determine the relative orientation of NaYF4:Er3+,Yb3+ UCNRs by polarized single-particle spectroscopy.
|
| Fig. 3 (a) Emission spectra from a single NaYF4:Er3+,Yb3+ UCNR immobilized on a surface for two perpendicular emission polarization angles. Purple (blue) line represents the recovered emission parallel (perpendicular) to the optical axis of the NaYF4:Er3+,Yb3+ UCNR. Inset represents these two different polarizations of the electric field that gives the two distinct spectra. Two dimensional map represents the emission intensity of red band as a function of the emission polarization angle. (b) Polar plot of the ratio (R652/660) between 652 and 660 peak intensities as a function of the emission polarization angle. Red dashed circle delimits ratio values above and under 1. | |
A tentative explanation of the polarized luminescence of NaYF4:Er3+,Yb3+ UCNRs can be given based on the recently published work of Ping Chen et al.51 In this work, the authors demonstrated that the polarized luminescence of Erbium doped NaYF4 nanodisks is due to the deterministic orientation of the crystallographic optical axis inside the nanoparticle. They claim that the optical axis in their nanostructures is perpendicular to the hexagonal (largest) face, so that the luminescence recorded along this direction does not show any polarization dependence. On the contrary, when measuring perpendicularly to this direction, due to the existence of an anisotropic crystal field, the luminescence becomes strongly polarization dependent due to the appearance of polarization induced forbidden and allowed transitions.52 We state at this point that, very likely, the optical axis of our NaYF4:Er3+,Yb3+ UCNRs lies parallel to their longest dimensions (i.e. optical axis coincides with the geometrical axis of the UCNRs). This would lead to a non-polarized luminescence when measured along the longest dimension (as it is observed later in the Optical trapping experiments section) and to a strongly polarized luminescence when spectra are recorded perpendicular to the longest dimension of the UCNR (see Fig. 3).
Optical trapping experiments
Single-beam resonant optical trapping.
The experimental setup used for simultaneous luminescence tracking and OT of a single Er3+/Yb3+ codoped UCNR is schematically depicted in Fig. 1a. A detailed description of all the optical components can be found in the Experimental section. Briefly, a 980 nm laser beam was focused into a 100 μm height microchannel, which contains a diluted colloidal suspension of NaYF4:Er3+,Yb3+ UCNRs, by using a 1.25 NA microscope objective. The 980 nm laser beam, partially absorbed by Yb3+ ions inside the NaYF4:Er3+,Yb3+ UCNRs, was used to both trap the NaYF4:Er3+,Yb3+ UCNR and, simultaneously, to excite its luminescence when incorporated into the trap. The luminescence generated by the optically trapped NaYF4:Er3+,Yb3+ UCNR was collected with the same objective used for focusing the 980 nm excitation laser beam, and it was spectrally analyzed by optically coupling the OT setup to the a high resolution spectrometer. Simultaneously, the luminescence image of the optical trap was recorded with a CMOS camera. A 700 nm short-pass filter was used to prevent the 980 nm radiation from reaching either the CMOS camera or the spectrometer. The sequential incorporation of individual NaYF4:Er3+,Yb3+ UCNRs into the trap could be monitored in real time by recording the time evolution of the trap luminescence intensity by using the CMOS camera. A typical intensity profile is shown in Fig. 1b. From this intensity profile, it is possible to identify three sharp intensity steps at 0.6, 1 and 1.6 min after switching on the 980 nm laser beam. Each intensity step accounts for a single trapped NaYF4:Er3+,Yb3+ UCNR whose luminescence is added to that generated by a previously trapped NaYF4:Er3+,Yb3+ UCNR. The luminescence images obtained after the incorporation of each single NaYF4:Er3+,Yb3+ UCNR are shown as the inset in Fig. 1b. At this point it should be noted that the time interval between consecutive incorporation of NaYF4:Er3+,Yb3+ UCNRs has been found to be strongly dependent on the concentration of NaYF4:Er3+,Yb3+ UCNRs in the suspension and by the 980 nm laser power, as it was already demonstrated to occur for spherical shaped Er3+/Yb3+ codoped UCNPs.53 The optical force acting on NaYF4:Er3+,Yb3+ UCNRs was measured by applying the so-called hydrodynamic-drag method that is explained in detail in the ESI.† Fig. S5† includes the optical trapping force acting on a single NaYF4:Er3+,Yb3+ UCNR as obtained at different 980 nm laser powers. The minimum laser power required for OT of a single NaYF4:Er3+,Yb3+ UCNR under our experimental conditions was found to be 10 mW. This value is 5 times lower than the corresponding one previously reported by us for spherical Er3+/Yb3+ codoped UCNPs.53 Fig. S5† clearly reveals that the optical force increases linearly with the 980 nm laser power as it was, indeed, expected. From the linear fit of experimental data we have obtained an optical trapping constant close to ktrap ≈ 2 pN W−1 μm−1, which can be compared to that previously found for other UCNPs.54
Finally, it should be also mentioned that, although fluctuations in the position of NaYF4:Er3+,Yb3+ UCNRs could be taking place, the optically trapped NaYF4:Er3+,Yb3+ UCNRs remained stable inside the trap. This is evidenced by the intensity profile shown in Fig. 1b in which sharp intensity drops down to the zero level (indicating that the NaYF4:Er3+,Yb3+ UCNRs have escaped from the trap and no luminescence is recorded) are not observed. This is in contrast to the results recently published by Jauffred et al. who evidenced the escape of QDs from an optical trap by the observation of intensity drops in the intensity time profiles.37 We state at this point that the larger size of our NaYF4:Er3+,Yb3+ UCNRs led to a reduced mobility as well as to a larger optical force in such a way that the optically trapped NaYF4:Er3+,Yb3+ UCNRs remain stable in the optical trap.
Once stable OT of UCNRs was experimentally achieved, the orientation of NaYF4:Er3+,Yb3+ UCNRs inside the trap was elucidated. This has been accomplished by performing polarized spectroscopy on a single optically trapped NaYF4:Er3+,Yb3+ UCNR. The emission spectra generated by an optically trapped NaYF4:Er3+,Yb3+ UCNR were systematically analyzed for different polarization states. At variance with the experimental results shown in Fig. 3, we observed that the luminescence spectra generated along the trapping direction was only slightly polarization dependent. This is evidenced in Fig. 4a that includes the emission spectra generated by a single optically trapped NaYF4:Er3+,Yb3+ UCNR as obtained for two arbitrary orthogonal polarizations. Within experimental error, they have been found to be virtually the same. In the emission spectra shown in Fig. 4a, the 660 nm line clearly dominates over the 652 nm peak, this being behavior independent of the polarization state as shown in the two-dimensional map where the emission intensity of the red band is represented as a function of the emission polarization angle. According to the data shown in Fig. 3, this fact suggests that the collected luminescence is polarized orthogonally to the axis of the trapped NaYF4:Er3+,Yb3+ UCNR. This unequivocally implies that the NaYF4:Er3+,Yb3+ UCNR axis is parallel to the k vector of the trapping laser beam, i.e. the NaYF4:Er3+,Yb3+ UCNR is aligned parallel to the propagating direction of the trapping beam (see Fig. 4b). Fig. 4c shows the polar plot of the R652/660 ratio with the emission polarization angle. When analyzing in detail the polar plot obtained for R652/660, we observed that a nearly circular plot is obtained. This reveals that, when the luminescence is collected along the direction of the trapping beam, an isotropic scenario is obtained. This also concludes that the NaYF4:Er3+,Yb3+ UCNR aligns parallel to the propagation direction of the trapping laser beam.
|
| Fig. 4 (a) Emission spectra from a single optically trapped NaYF4:Er3+,Yb3+ UCNR for two arbitrary perpendicular emission polarization angles. Two dimensional map represents the emission intensity of the red band as a function of the emission polarization angle. (b) Schematic representation of the trajectory of a NaYF4:Er3+,Yb3+ UCNR moving towards the optical trap. NaYF4:Er3+,Yb3+ UCNR longitudinal axis is parallel to the laser propagation direction when trapped. (c) Polar plot of the ratio between 652 and 660 nm peak intensities as a function of the emission polarization angle. Red dashed circle delimits ratio values above and below 1. | |
At this point it should be noted that near circular plot diagrams of the R552/660 intensity ratio would be achieved if the NaYF4:Er3+,Yb3+ UCNR was orientated perpendicular to the trapping beam while rotating inside the trap with a rotation period much smaller than the acquisition time of luminescence spectra. In this scenario, the collected luminescence spectra result from a combination of the spectra obtained for the two polarization states shown in Fig. 3a, as it does occur when polarized spectroscopy is performed on a colloidal suspension of randomly oriented NaYF4:Er3+,Yb3+ UCNRs (see Fig. S3b in the ESI†). Nevertheless, the emission spectra generated by an optically trapped NaYF4:Er3+,Yb3+ UCNR does not show any relevant contribution of parallel polarized emission. Thus, the rotation of NaYF4:Er3+,Yb3+ UCNR in a plane perpendicular to the laser trapping beam can be disregarded.
Multiple-beam optical trapping.
The potential application of single particle polarized spectroscopy for three-dimensional monitoring of optically trapped UCNRs has been further explored by using a multiple-beam optical trap. A two beam optical tweezer setup was used to three dimensionally manipulate a single optically trapped NaYF4:Er3+,Yb3+ UCNR. For this purpose a modification of the optical tweezers setup depicted in Fig. 1a was used (for more details see the Experimental section and Fig. S2†). Such a setup allowed for an accurate control over the distance and relative position between the two optical traps. Two different situations were found to take place. When optical traps are separated by a distance longer than one micron (approximately), they behave as two independent single-beam optical traps. When a single NaYF4:Er3+,Yb3+ UCNR is optically trapped within one of the traps it aligns and remains parallel to the propagation axis of the beam (see Fig. 5a–c where a single UCNR is trapped in the bottom trap). Orientation of the UCNR is again evidenced by the luminescence spectrum in which the 652 nm and 660 nm emission peaks are of similar intensity, independent of the polarization angle. This is exactly the same result obtained in single-beam optical trap experiments. When the traps are close enough (distance between traps close to 1 μm), the trapped NaYF4:Er3+,Yb3+ UCNR is subjected to the force field resulting from the superposition of both traps. Under these conditions, the force field becomes anisotropic and, as a consequence, the NaYF4:Er3+,Yb3+ UCNR flips and orientates parallel to the line connecting both the traps. Thus, the proximity of both traps orientates the NaYF4:Er3+,Yb3+ UCNR in the plane perpendicular to the trap beam propagation direction. This is evidenced in the fluorescence image shown in Fig. 5d as well as in the associated single-particle luminescence spectrum acquired with the selection polarized parallel to the inter-trap connection line (see white arrows in Fig. 5a–d that indicate the analyzed polarization angle). Under these conditions, the emission spectrum is dominated by the 652 nm emission line indicating that the NaYF4:Er3+,Yb3+ UCNR is aligned parallel to the polarizer direction, i.e. the NaYF4:Er3+,Yb3+ UCNR is aligned parallel to the inter-trap connection line. The relative orientation of the UCNR and the two traps is schematically shown in Fig. 5e and f.
|
| Fig. 5 Evolution of the emitted spectra of a trapped NaYF4:Er3+,Yb3+ UCNR when the distance between traps is reduced. The recorded emission polarization angle is fixed to that indicated by white arrows. It can be seen that the emission spectra changes from that attributed to perpendicular polarization (a–c) to that for the parallel polarization state (d). Scale bar corresponds to 1 μm in all images. Panels (e–f) are schematic representations of the two NaYF4:Er3+,Yb3+ UCNR positions. | |
Further manipulation of the two trap positions by keeping this inter-trap distance close to 1 μm allows, in principle, for full control/rotation of the NaYF4:Er3+,Yb3+ UCNR within the plane perpendicular to the laser beams’ direction. This possibility has been demonstrated by rotating one trap around the other by 90° and keeping the inter-trap distance fixed at 1 μm (see schematic drawings in the right column of Fig. 6). Rotation of the optically trapped UCNR is shown by the fluorescence images in the central column of Fig. 6. This in-plane rotation is further evidenced by the changes observed in the spectral shape of the polarized upconversion spectrum obtained by keeping the measured polarization angle fixed as indicated by arrows shown in Fig. 6. Rotation of the optical traps causes a shift from an emission spectrum dominated by the 652 nm emission line to an emission spectrum in which both 652 and 660 nm emission lines are of comparable intensity. This unequivocally reveals a complete 90° in-plane rotation of the NaYF4:Er3+,Yb3+ UCNR. Note that the data shown in Fig. 5 and 6 do not only reveal the possibility of accurate three-dimensional optical manipulation of single UCNRs but also the continuous monitoring of their three-dimensional orientation by single particle spectroscopy.
|
| Fig. 6 Evolution of the emitted spectra when rotating the longitudinal axis of the NaYF4:Er3+,Yb3+ UCNR. Emission polarization angle is fixed to that indicated by white arrows. Perpendicular polarization is measured when the NaYF4:Er3+,Yb3+ UCNR axis happen to be perpendicular to the emission polarization angle (lower panel). An intermediate state is observed when the NaYF4:Er3+,Yb3+ UCNR axis form approximately 45° with the emission polarization angle and both polarization states are measured (middle panel). Scale bar corresponds to 1 μm in all images. | |
Conclusions
In summary, resonant stable optical trapping of NaYF4:Er3+,Yb3+ upconverting nanorods has been demonstrated. The efficient excitation of the Er3+ visible luminescence by the partially absorbed 980 nm trapping radiation of the Yb3+ ions, allowed for real time tracking of the optically trapped NaYF4:Er3+,Yb3+ upconverting nanorods by simple luminescence imaging microscopy. The time evolution of the luminescence images from the optical trap evidenced the sequential incorporation of single NaYF4:Er3+,Yb3+ upconverting nanorods as well as their stable localization inside the trap. Single-particle polarized spectroscopy experiments performed on immobilized NaYF4:Er3+,Yb3+ upconverting nanorods revealed that their two-photon excited luminescence is strongly polarized, evidence for the existence of two well-defined polarization states corresponding to the polarization of luminescence perpendicular and parallel to the axis of NaYF4:Er3+,Yb3+ upconverting nanorods. This strong polarization dependence of luminescence has been used to unequivocally determine the orientation of optically trapped NaYF4:Er3+,Yb3+ upconverting nanorods inside single and double beam optical traps. It has been concluded that, under our experimental conditions, NaYF4:Er3+,Yb3+ upconverting nanorods orientated parallel to the propagation direction of the trapping laser beam in a single-beam optical tweezers setup. Two beam optical trapping allowed for controlled three-dimensional manipulation of single NaYF4:Er3+,Yb3+ upconverting nanorod whose three-dimensional orientation was unequivocally determined by the analysis of the polarization state of their single particle luminescence.
The possibility, demonstrated here, of applying simple experimental approaches to achieve three-dimensional manipulation of the upconverting nanorods, whilst knowing their exact position and orientation, opens up a new avenue into their use in numerous applications ranging from biology to nanofluidics.
Authors contribution
The manuscript was written through contributions of all the authors. All the authors have given approval to the final version of the manuscript.
Conflict of interest
The authors declare no competing financial interest.
Acknowledgements
This work was supported by the Spanish Ministerio de Educación y Ciencia (MAT2013-47395-C4-1-R) and by Banco Santander for “proyectos de cooperación interuniversitaria” (2015/ASIA/06). Patricia Haro-González thanks the Spanish Ministerio de Economía y Competitividad (MINECO) for the Juan de la Cierva program. Paloma Rodríguez-Sevilla thanks the Spanish Ministerio de Economía y Competitividad (MINECO) for the “Promoción del talento y su Empleabilidad en I+D+i” statal program. Dominika Wawrzyńczyk, Marcin Nyk and Marek Samoć acknowledge the support from the National Science Centre under grant DEC-2012/04/M/ST5/00340, by a statutory activity subsidy from the Polish Ministry of Science and Higher Education for the Faculty of Chemistry of Wroclaw University of Technology, as well as from the Foundation for Polish Science under START 2014 programme. This work has received funding from The Royal Society (IE130466). Mark D. Mackenzie acknowledges funding from EPSRC (grant no EP/J500227/1).
Notes and references
- A. P. Bartko, L. A. Peyser, R. M. Dickson, A. Mehta, T. Thundat, R. Bhargava and M. D. Barnes, Chem. Phys. Lett., 2002, 358, 459–465 CrossRef CAS.
- M. Gregor, A. Kuhlicke and O. Benson, Opt. Express, 2009, 17, 24234–24243 CrossRef CAS PubMed.
- W. Gao, S. Sattayasamitsathit, J. Orozco and J. Wang, J. Am. Chem. Soc., 2011, 133, 11862–11864 CrossRef CAS PubMed.
- S. Hao, G. Chen and C. Yang, Theranostics, 2013, 3, 331–345 CrossRef PubMed.
- Y. Zhang, W. Wei, G. K. Das and T. T. Y. Tan, J. Photochem. Photobiol., C, 2014, 20, 71–96 CrossRef CAS.
- W. Zheng, P. Huang, D. Tu, E. Ma, H. Zhu and X. Chen, Chem. Soc. Rev., 2015, 44, 1379–1415 RSC.
- J. C. Goldschmidt and S. Fischer, Adv. Opt. Mater., 2015, 3, 510–535 CrossRef CAS.
- C. Miao, C. Chen, Q. L. Dai, L. Xu and H. W. Song, J. Colloid Interface Sci., 2015, 440, 162–167 CrossRef CAS PubMed.
- L. M. Maestro, E. M. Rodriguez, F. Vetrone, R. Naccache, H. L. Ramirez, D. Jaque, J. A. Capobianco and J. G. Solé, Opt. Express, 2010, 18, 23544–23553 CrossRef CAS PubMed.
- L. Martinez Maestro, E. Martin Rodriguez, F. Vetrone, R. Naccache, H. Loro Ramirez, D. Jaque, J. A. Capobianco and J. Garcia Sole, Opt. Express, 2010, 18, 23544–23553 CrossRef PubMed.
- F. Wang, Y. Han, C. S. Lim, Y. Lu, J. Wang, J. Xu, H. Chen, C. Zhang, M. Hong and X. Liu, Nature, 2010, 463, 1061–1065 CrossRef CAS PubMed.
- A. Bednarkiewicz, D. Wawrzynczyk, M. Nyk and M. Samoc, J. Rare Earths, 2011, 29, 1152–1156 CrossRef CAS.
- M. Ding, S. Yin, D. Chen, J. Zhong, Y. Ni, C. Lu, Z. Xu and Z. Ji, Appl. Surf. Sci., 2015, 333, 23–33 CrossRef CAS.
- F. M. Mor, A. Sienkiewicz, L. Forró and S. Jeney, ACS Photonics, 2014, 1, 1251–1257 CrossRef CAS.
- F. Wang, D. Banerjee, Y. S. Liu, X. Y. Chen and X. G. Liu, Analyst, 2010, 135, 1839–1854 RSC.
- R. Naccache, F. Vetrone and J. A. Capobianco, ChemSusChem, 2013, 6, 1308–1311 CrossRef CAS PubMed.
- X. Xie and X. Liu, Nat. Mater., 2012, 11, 842–843 CrossRef CAS PubMed.
- K. König, J. Microsc., 2000, 200, 83–104 CrossRef.
- D. Jaque, B. del Rosal, E. Martin Rodriguez, L. Martinez Maestro, P. Haro-Gonzalez and J. Garcia Sole, Nanomedicine, 2014, 9, 1047–1062 CrossRef CAS PubMed.
- D. Jaque and F. Vetrone, Nanoscale, 2012, 4, 4301–4326 RSC.
- N. Bogdan, F. Vetrone, G. A. Ozin and J. A. Capobianco, Nano Lett., 2011, 11, 835–840 CrossRef CAS PubMed.
- G. Chen, H. Qiu, P. N. Prasad and X. Chen, Chem. Rev., 2014, 114, 5161–5214 CrossRef CAS PubMed.
- D. J. Gargas, E. M. Chan, A. D. Ostrowski, S. Aloni, M. V. P. Altoe, E. S. Barnard, B. Sanii, J. J. Urban, D. J. Milliron, B. E. Cohen and P. J. Schuck, Nat. Nanotechnol., 2014, 9, 300–305 CrossRef CAS PubMed.
- A. Gnach and A. Bednarkiewicz, Nano Today, 2012, 7, 532–563 CrossRef CAS.
- G. S. Yi, H. C. Lu, S. Y. Zhao, G. Yue, W. J. Yang, D. P. Chen and L. H. Guo, Nano Lett., 2004, 4, 2191–2196 CrossRef CAS.
- Y. Zhang, L. Zhang, R. Deng, J. Tian, Y. Zong, D. Jin and X. Liu, J. Am. Chem. Soc., 2014, 136, 4893–4896 CrossRef CAS PubMed.
- L. Zhihua, L. Ying, W. Yanan, M. Haixia, D. Yu and L. Hong, J. Alloys Compd., 2014, 613, 18–24 CrossRef.
- Z.-Q. Liang, S.-L. Zhao, Y. Cui, L.-J. Tian, J.-J. Zhang and Z. Xu, Chin. Phys. B, 2015, 24, 037801 CrossRef.
- R. Karnik, R. Fan, M. Yue, D. Li, P. Yang and A. Majumdar, Nano Lett., 2005, 5, 943–948 CrossRef CAS PubMed.
- D. J. Sirbuly, M. Law, H. Yan and P. Yang, J. Phys. Chem. B, 2005, 109, 15190–15213 CrossRef CAS PubMed.
- P. A. Smith, C. D. Nordquist, T. N. Jackson, T. S. Mayer, B. R. Martin, J. Mbindyo and T. E. Mallouk, Appl. Phys. Lett., 2000, 77, 1399–1401 CrossRef CAS.
- M. Chen, L. Sun, J. E. Bonevich, D. H. Reich, C. L. Chien and P. C. Searson, Appl. Phys. Lett., 2003, 82, 3310–3312 CrossRef CAS.
- B. Messer, J. H. Song and P. Yang, J. Am. Chem. Soc., 2000, 122, 10232–10233 CrossRef CAS.
- K. Svoboda and S. M. Block, Annu. Rev. Biophys. Biomol. Struct., 1994, 23, 247–285 CrossRef CAS PubMed.
- J. E. Molloy and M. J. Padgett, Contemp. Phys., 2002, 43, 241–258 CrossRef CAS.
- A. Ashkin, Biophys. J., 1992, 61, 569–582 CrossRef CAS PubMed.
- P. M. Bendix, L. Jauffred, K. Norregaard and L. B. Oddershede, IEEE J. Sel. Top. Quantum Electron., 2014, 20, 15–26 Search PubMed.
- M. Dienerowitz, M. Mazilu and K. Dholakia, NANOP, 2008, 2, 021875–021832 CrossRef.
- M. Pelton, M. Liu, H. Y. Kim, G. Smith, P. Guyot-Sionnest and N. F. Scherer, Opt. Lett., 2006, 31, 2075–2077 CrossRef CAS PubMed.
- C. Selhuber-Unkel, I. Zins, O. Schubert, C. Sonnichsen and L. B. Oddershede, Nano Lett., 2008, 8, 2998–3003 CrossRef CAS PubMed.
- P. J. Reece, W. J. Toe, F. Wang, S. Paiman, Q. Gao, H. H. Tan and C. Jagadish, Nano Lett., 2011, 11, 2375–2381 CrossRef CAS PubMed.
- F. Wang, W. J. Toe, W. M. Lee, D. McGloin, Q. Gao, H. H. Tan, C. Jagadish and P. J. Reece, Nano Lett., 2013, 13, 1185–1191 CrossRef CAS PubMed.
- P. Rodríguez-Sevilla, H. Rodríguez-Rodríguez, M. Pedroni, A. Speghini, M. Bettinelli, J. G. Solé, D. Jaque and P. Haro-González, Nano Lett., 2015, 15, 5068–5074 CrossRef PubMed.
-
R. Grange, F. Dutto and A. Radenovic, Niobates nanowires: synthesis, characterization and applications, In Tech, 2011 Search PubMed.
- A. Irrera, P. Artoni, R. Saija, P. G. Gucciardi, M. A. Iatì, F. Borghese, P. Denti, F. Iacona, F. Priolo and O. M. Maragò, Nano Lett., 2011, 11, 4879–4884 CrossRef CAS PubMed.
- D. Wawrzynczyk, D. Piatkowski, S. Mackowski, M. Samoc and M. Nyk, J. Mater. Chem. C, 2015, 3, 5332–5338 RSC.
- P. Haro-Gonzalez, W. T. Ramsay, L. M. Maestro, B. del Rosal, K. Santacruz-Gomez, M. D. Iglesias-de la Cruz, F. Sanz-Rodriguez, J. Y. Chooi, P. R. Sevilla, M. Bettinelli, D. Choudhury, A. K. Kar, J. G. Sole, D. Jaque and L. Paterson, Small, 2013, 9, 2162–2170 CrossRef CAS PubMed.
- J. T. Hu, L. S. Li, W. D. Yang, L. Manna, L. W. Wang and A. P. Alivisatos, Science, 2001, 292, 2060–2063 CrossRef CAS PubMed.
- J. Zhou, G. Chen, E. Wu, G. Bi, B. Wu, Y. Teng, S. Zhou and J. Qiu, Nano Lett., 2013, 13, 2241–2246 CrossRef CAS PubMed.
- G. Dong, H. He, Q. Pan, G. Chen, J. Xie, Z. Ma and M. Peng, ChemPlusChem, 2014, 79, 601–609 CrossRef CAS.
- P. Chen, M. Song, E. Wu, B. Wu, J. Zhou, H. Zeng, X. Liu and J. Qiu, Nanoscale, 2015, 7, 6462–6466 RSC.
- K. Binnemans, Coord. Chem. Rev., 2015, 295, 1–45 CrossRef CAS.
- P. Haro-Gonzalez, B. del Rosal, L. M. Maestro, E. Martin Rodriguez, R. Naccache, J. A. Capobianco, K. Dholakia, J. G. Sole and D. Jaque, Nanoscale, 2013, 5, 12192–12199 RSC.
- H. Rodríguez-Rodríguez, P. Rodríguez Sevilla, E. Martín Rodríguez, D. H. Ortgies, M. Pedroni, A. Speghini, M. Bettinelli, D. Jaque and P. Haro-González, Small, 2015, 11, 1555–1561 CrossRef PubMed.
Footnote |
† Electronic supplementary information (ESI) available: Polarized emission of the colloidal suspension of NaYF4:Er3+,Yb3+ UCNRs, green emission band, optical force measurement and optical manipulation by two beam optical tweezers setup. See DOI: 10.1039/c5nr06419h |
|
This journal is © The Royal Society of Chemistry 2016 |
Click here to see how this site uses Cookies. View our privacy policy here.