Giacomo Damilanoa,
Antero Laitinenb,
Pia Willberg-Keyriläinenb,
Tiina Lavonenb,
Riina Häkkinenb,
Wim Dehaena,
Koen Binnemansa and
Lauri Kuutti*b
aKU Leuven, Department of Chemistry, Celestijnenlaan 200F – P. O. Box 2404, B-3001 Leuven, Belgium
bVTT Technical Research Centre of Finland Ltd, Tietotie 4E, FI-02150 VTT, Finland. E-mail: lauri.kuutti@vtt.fi; Tel: +358 20 722 2936
First published on 19th June 2020
This study deals with an investigation of how substitution of an alcohol group by a thiol group in mixtures of choline chloride with a series of bio-sourceable molecules affects the physico-chemical properties of the mixtures and their ability to dissolve metal oxides. All of the thiol mixtures studied showed a higher affinity and selectivity for late transition metals and the physical properties of the mixtures were improved compared to their alcohol analogues (i.e. lower viscosity, wider liquid range). The metal solubility was assessed via determination of the final concentration of the metal oxides dissolved in thiol mixtures via inductively coupled plasma optical emission spectroscopy (ICP-OES). The thiol function selectively improved the solubilities of the late transition metal oxides (i.e. copper and zinc), which are valuable metals often present as residue in industrial waste. The solubility of iron oxides was much lower than that of the valuable metals, which is a significant benefit in industrial applications. The different solubilization behaviour of metal oxides in the thiol and alcohol mixtures was further investigated via UV-vis absorption and infrared spectroscopy. This study allowed the potential of these deep-eutectic solvents for the selective recovery of metals to be assessed.
Classic hydrometallurgical processes often use a large volume of water to achieve separation, which is an effective but not efficient procedure. Water is a harmless green solvent but it must be purified prior to its disposal. Although viable, the purification process is impractical due to the large volumes of waste water produced in hydrometallurgical processes. In order to shift to a more sustainable process, non-aqueous systems are being studied as alternative media for solvometallurgical processes.
Solvometallurgy is the branch of extractive metallurgy that attempts an almost complete substitution of water with an organic solvent.1 Besides reducing the consumption of water, an accurate choice of the organic solvent greatly improves the process selectivity and reactivity, allowing for the development of more efficient and sustainable processes. Amongst many, ionic liquids (ILs) and deep-eutectic solvents (DESs) are appealing as solvents for solvometallurgical applications.2,3 The interest in this category of solvents arose from both their affirmation as an environmentally benign technology, due to the low volatility and high stability, and from their fine tunability to the needs of the process via an appropriate choice of the solvent mixtures.
As the solvent is the most abundant component of a system, its low cost is often crucial to the attainment of a financially viable process. The large scale viability, reduced costs, and ease of production are reasons to often prefer deep-eutectic solvents over ionic liquids. Abbott et al. firstly introduced the definition of a deep-eutectic solvent as a eutectic mixture of two or more components with a depression in the freezing-point at about or below 100 °C (arbitrary temperature) and a composition close to the one of the eutectic point.2,4,5
The growing amount of research concerning these mixtures is urging for a more accurate definition for these materials. A number of bio-sourceable materials was investigated in the literature as mixture components. For many of these mixtures, a depression of the solidification transition temperature was recorded, but not a freezing-point. In the absence of a freezing point, we can no longer discuss about eutectic mixtures nor about deep-eutectic solvents, because the definition of the latter is dependent on the former. Therefore, low-transition-temperature mixtures (LTTMs) appears to be a more suitable term to describe these mixtures.6
Abbott et al. studied a wide array of choline chloride mixtures with various components such as oxalic acid, ethylene glycol, malonic acid, and urea.2–9 Both choline chloride DESs and DESs resulted in an effective metal dissolution, showing often remarkably high metal solubilities for a non-aqueous system.3,7,10–13 In these medias, the high metal solubility (i.e. metal salts, oxides and hydroxides) is also contributing to their high efficacy in applications such as metal extraction and recovery. For example, often a selective metal recovery can be attained via the watering down of the system, which alters the metal solubilities. Moreover, the relatively wide electrochemical window, the chemical stability, and thermal stability allow for the use of electro-winning, a simple metal recovery technique, from these mixtures.
Although, the viscosity of the pure non-aqueous solvent systems is sometimes low, the dissolution of metals in these mixtures often elicits a steep increase of their viscosity. Avoiding this is therefore of utmost importance for process scale-up economies because the adhesion of such viscous media on the undissolved materials and reactor walls causes substantial losses, that could be up to 40 wt%. Previous studies on the use of ILs and DESs in tribological applications showed a correlation between the decrease in viscosity and the inclusion of organo-sulfur groups in ionic liquids and deep-eutectic solvents.14 As the hydrogen bond interactions are the likely cause of the atypical features of low temperature-transition mixtures, the reduction in viscosity could be rationalised by a loosening of the hydrogen bond network due to a weakening of the electrostatic interactions formed with the organo-sulfur atoms.4,6
In general, most of the studied mixtures includes amino, ammonium, carboxylic acid, or alcohol groups in the molecular structure but rarely organo-sulfur groups (e.g. thio-urea DESs).15,16 However, in complexation chemistry many sulfur compounds have demonstrated a high selectivity and affinity for precious and late transition metals (i.e. group 10 and 12).17–22 This can be explained by the concept of hard and soft acid and bases (HSAB concept).23 Often these metals are also the target of industrial waste recycle processes because they contain most of the residual metal value. For example, both thio-glycolic and thio-lactic acid have been exploited in various fields (i.e. cosmetics, metal titration, metal complexation, waste-water treatment).19,20,24–29 They are synthesised easily from their bio-sourceable oxy-analogues and have a significant affinity for late transition metals (i.e. copper and zinc).24
In this paper, we describe how the introduction of thiol groups in bio-sourceable alcohols and acids can influence the physico-chemical properties of the mixture and the solubilities of metal oxides in such solvents.
HBA:HBD (molar ratio) | Appearance at 20–22 °C | t (h) | T (°C) |
---|---|---|---|
a A precipitate was observed after refrigerating the sample overnight at 6 °C. | |||
ChCl:GA (1:2) | Clear homogeneous liquid | 2 | 20–22 |
ChCl:GA (1:3)a | Clear homogenous liquid | 2 | 20–22 |
ChCl:TGA (1:2) | Clear homogenous liquid | 2 | 20–22 |
ChCl:TGA (1:3) | Clear homogenous liquid | 2 | 20–22 |
ChCl:LA (1:2) | Clear homogenous liquid | 2 | 20–22 |
ChCl:LA (1:3) | Clear homogenous liquid | 2 | 20–22 |
ChCl:TLA (1:2) | Clear homogenous liquid | 2 | 20–22 |
ChCl:TLA (1:3) | Clear homogenous liquid | 2 | 20–22 |
ChCl:MA (1:1) | Clear homogenous liquid | 2 | 60–70 |
ChCl:TMA (1:1) | Clear faint yellow homogenous liquid | 4 | 60–70 |
ChCl:DTT (1:2) | Clear homogenous liquid | 3 | 20–22 |
ChCl:DTT (1:3) | Clear homogenous liquid | 3 | 20–22 |
The formation of the DESs was studied to determine the appropriate components ratio and the softest condition for the homogenization of these mixtures. Most of the DESs were obtained via simple mixing at room temperature (22 °C), but few required higher temperatures (Table 1). The HBA:HBD ratio achieving a clear homogeneous eutectic mixture followed the empirical ratio formerly observed by Abbott et al. for other mono and di-acids.5 The formation of the DESs was eased by the mutual dispersion of the components into each other. Although time-demanding, mixing the components of the DES at room temperature allowed to have virtually no ester formation. This was verified via NMR analysis, which confirmed the virtual absence of esterification. If the homogenization was expedited, for example via the use of higher temperatures, then the 1H NMR signals of esterification side-products became noticeable.30 In order to minimize ester formation, the less energy intensive procedure was used.30 To avoid further esterification and achieve more reliable results, the prepared DES were stored at 6 °C. The acidity of the mixtures was estimated via pH strip indicators, showing an average pH of 3 for the mixtures containing an acid function (i.e. ChCl:GA(1:2), ChCl:TGA(1:2), ChCl:LA(1:2), ChCl:TLA(1:2), ChCl:MA(1:2), ChCl:TMA(1:2)) and a pH of 5 for the ChCl:DTT(1:3) mixture (Table 2). Generally, a lower acidity is experienced in this type of media because the charged protic environment inhibits the full ionization of the acidic species.8 Instead, the DESs had a slightly higher acidity with respect to the pure substances (e.g. the used acids have in average a pKa ranging from about 3.1 to 3.8). This effect may be due to the coordination of chloride anions to hydrogen through H-bond interactions. This may result in an overall weaker X–H bond (X = O, S) and a higher concentration of ionized acidic groups. The synthesised mixtures were characterised via differential scanning calorimetry. All of the mixtures showed a glass phase transition (Table 2).30
HBA:HBD (ratio) | ηa (Pa s) | g. t. p.b (°C) | pKa |
---|---|---|---|
a Viscosity measured at 25 °C (vide ESI).b Glass transition temperature according to the DSC analyses. | |||
ChCl:GA (1:2) | 0.3 ± 0.0 | −79 ± 0 | 3 |
ChCl:GA (1:3) | — | −78 ± 2 | 3 |
ChCl:TGA (1:2) | — | −95 ± 0 | 3 |
ChCl:TGA (1:3) | — | −94 ± 2 | 3 |
ChCl:LA (1:2) | 0.7 ± 0.0 | −70 ± 2 | 3 |
ChCl:LA (1:3) | — | −68 ± 2 | 3 |
ChCl:TLA (1:2) | 0.1 ± 0.0 | −88 ± 0 | 3 |
ChCl:TLA (1:3) | — | −87 ± 3 | 3 |
ChCl:MA (1:1) | 30.4 ± 0.6 | −48 ± 0 | 3 |
ChCl:TMA (1:1) | 28.1 ± 0.8 | −58 ± 1 | 3 |
ChCl:DTT (1:2) | — | −64 ± 3 | 5 |
ChCl:DTT (1:3) | 0.32 ± 0.0 | −69 ± 3 | 5 |
In order to limit the number of analyses, a subset of the synthesised DESs was used in the following tests (i.e. ChCl:GA (1:2), ChCl:TGA (1:2), ChCl:LA (1:2), ChCl:TLA (1:2), ChCl:MA (1:1), ChCl:TMA (1:1), ChCl:DTT (1:3)). Viscosimetry was carried out but the ChCl:TGA (1:2) mixture was excluded from the analyses due to safety concerns. Thioglycolic and thioglycolate toxicity is reported to be concentration dependent, which is also the reason why it is widely used in consumer products.31 To avoid any risk, we excluded the analyses of mixtures of thioglycolic acid out of a fumehood. Viscosimetry showed a marked reduction in viscosity for all the thiol derivatives with respect to the alcohol ones (Table 2). The significant reduction in viscosity is beneficial for the intended application use of these mixtures.14 Both the ChCl:MA (1:1) and the ChCl:TMA (1:1) had a remarkably higher viscosity, even at elevated temperatures (30.4 and 28.1 Pa s respectively at 25 °C). In this case, the higher viscosity impeded an effective homogenization of the sample via magnetic stirring. Therefore, these mixtures were excluded from the metal oxides dissolution study.
Metal oxide dissolution of various sample metals was tested to define a general solubility trend in the studied DESs. The solubility of a series of metal oxides belonging to the late transition metal group was studied: Ag2O, Au2O3, CdO, CoO, LiCoO2, CuO, Cu2O, FeO, Fe2O3, Fe3O4, NiO, PbO, and ZnO. These metals were selected in order to observe the effect of the heteroatom substitution on the chelating capabilities of the various mixtures. Each metal oxide was added to a separate DES sample until saturation was reached. After 48 h, the samples were centrifuged and filtered and the filtrate was tested to evaluate the dissolution process.
A preliminary test of the dissolution effects was carried out via FTIR spectroscopy. FTIR analysis was directed to analyse the interaction of the functional groups belonging to the organic complexing agent with the dissolved metals (Table 3). Only the ChCl:DTT (1:3) mixture had no remarkable variations, with respect to the pure sample, in the reflectance signals. Because for the ChCl:DTT (1:3) mixture no characteristic variation could be observed via FTIR analysis, the following discussion on the FTIR analyses will focus on the other mixtures tested.
ChCl:GA (1:2) | ChCl:TGA (1:2) | ChCl:LA (1:2) | ChCl:TLA (1:2) | ChCl:DTT (1:3) | Assignment |
---|---|---|---|---|---|
a vs. very strong, s strong, m medium, w weak, sh shoulder. ν stretching, νsy symmetric, νas asymmetric, δs bending, ρ rocking, ω wagging, τ twisting. | |||||
3280 (w) | 3280 (w) | 3279 (w) | — | 3309 (vs.) | v (OH)COOH |
2564 (w) | 2553 (w) | 2548 (w) | v (SH) | ||
1729 (vs.) | 1717 (vs.) | 1730 (vs.) | 1723 (vs.) | v (CO)COOH | |
1419 (m) | 1414 (m) | 1456 (m) | 1452 (m) | vsy (–CO2)COOH | |
1194 (vs.) | 1171 (vs.) | ω (CH2) | |||
1079 (vs.) | 1082 (m) | 1084 (m) | 1077 (m) | 1066 (vs.) | v (C–OH)COOH |
1049 (m) | 1043 (m) | 1057 (m) | 1044 (vs.) | v (C–OH)CH2OH | |
993 (w) | 1003 (w) | 1005 (m) | 1002 (w) | 1005 (w) | v (C–C) |
For the DES containing an acid group, metal oxide dissolution happens generally via the neutralization of the oxide and the formation of a metal complex. Therefore, the metal oxide neutralization was followed by the appearance of a peak at about 1550–1590 cm−1, which was caused by the asymmetric stretch of the carboxylate group. In all of the samples where dissolution of the metal oxide occurred, there was also the appearance of the carboxylate group signal. In correspondence to the appearance of the carboxylate group signal also some reduction in the intensity of the signals of the carboxylic acid group at about 1715–1730 cm−1 and of the hydroxyl group stretch at 1040–1090 cm−1 was observed.
The appearance of the carboxylate signal was generally consistent with the results obtained with the ICP-OES on metal dissolution. However, for some samples ICP-OES analyses did show only a negligible amount of dissolved metals whilst the FTIR analyses showed a marked formation of the carboxylate anion. This was observed especially for lead and to some extent also for nickel and cobalt samples. The absence of dissolved metals was suggestive of the formation of a precipitate, which was filtered off after dissolution and prior to the ICP-OES analysis. This was reasoned out by the possible formation of insoluble hydroxides and/or salts by reaction with the DES. The acidic group of the DES might have reacted with the oxides, resulting in the formation of metal salts (either chloride or carboxylate) and eventually also hydroxides. Then, these might have precipitated out because they are poorly soluble in the DES (vide ESI, Visual report). Noticeable was that nickel(II) oxide was generally insoluble in the assayed mixtures and strongly reacted with the ChCl:TLA (1:2) (determined via FTIR analysis). This resulted in the formation of a thick solid paste, which could not be filtered, impeding any further analyses.
The determination of the dissolved metal content into the mixture was carried out via ICP-MS analysis (Table 4). The ChCl:GA (1:2) mixture was able to dissolve various metals: CdO (96 g L−1), Cu2O (84 g L−1), ZnO (50 g L−1), Au2O3 (42 g L−1), Fe2O3 (27 g L−1). Substitution of glycolic with thioglycolic acid strongly affected metal solubilities. The ChCl:TGA (1:2) mixture was able to dissolve more than the double of the amount of cadmium and zinc dissolved in the ChCl:GA (1:2) and no cupric nor cuprous oxides. In the ChCl:TGA (1:2) mixture, the concentration of dissolved metals was as follows: CdO (213 g L−1), ZnO (122 g L−1), FeO (29 g L−1), Fe2O3 (23 g L−1), CoO (43 g L−1), LiCoO2 (22 g L−1). This shows a marked increase in the dissolution selectivity of the metals belonging to the Group 12 of the periodic system (i.e. Cd and Zn). Moreover, this mixture outperformed all the others in the dissolution of cobalt, both as cobalt oxide and as lithium cobalt oxide.
FeO | Fe2O3 | CoO | LiCoO2 | NiO | Cu2O | CuO | Ag2O | Au2O3 | ZnO | CdO | PbO | |
---|---|---|---|---|---|---|---|---|---|---|---|---|
a The data herein reproduced may have been obtained via a different procedure. The data were converted from ppm assuming the density of ChCl:EG (1:2) and ChCl:malonic acid (1:2) at 50 °C to be 1.10 g mL−1 and 1.17 g mL−1, respectively.11 | ||||||||||||
ChCl:GA (1:2) | 2.99 | 27.9 | 6.97 | 3.5 | 0.1 | 84.18 | 3.11 | 0.62 | 42.22 | 50.28 | 96.96 | 0.82 |
ChCl:TGA (1:2) | 29.91 | 23.79 | 43.98 | 22.11 | 2.44 | 0.62 | 0.63 | 0.67 | 0.03 | 122.07 | 213.31 | 0.51 |
ChCl:LA (1:2) | 3.86 | 29.61 | 8.3 | 11.62 | 0.27 | 77.16 | 25.36 | 0.58 | 31.22 | 13.52 | 42.09 | 0.22 |
ChCl:TLA (1:2) | 20.21 | 50.42 | 0.35 | 0 | 0 | 83.99 | 60.22 | 0.63 | 0.05 | 90.95 | 93.75 | 0.26 |
ChCl:DTT (1:3) | 9.89 | 30.68 | 1.46 | 0.93 | 4.51 | 2.93 | 3.18 | 0.27 | 3.19 | 21.85 | 12.67 | 80.81 |
ChCl:ethylene glycol (1:2)a | 0.00 | 0.00 | 0.01 | 0.00 | 0.00 | 0.36 | 0.00 | — | — | 0.43 | — | — |
ChCl:malonic acid (1:2)a | 4.28 | 0.32 | 3.10 | 0.00 | 0.13 | 15.67 | 11.97 | — | — | 13.86 | — | — |
A similar trend was observed for the mixtures of ChCl:LA (1:2) and ChCl:TLA (1:2). The ChCl:LA (1:2) mixture was able to dissolve the following metals: Cu2O (80 g L−1), CdO (46 g L−1), Au2O3 (31 g L−1), CuO (23 g L−1), Fe2O3 (23 g L−1). Differently from what was previously observed for the ChCl:GA (1:2) mixture, in the ChCl:LA (1:2) mixture the concentration of zinc oxide fell well below the concentration of cadmium (about ⅓). Conversely, in the ChCl:TLA (1:2) mixture both cadmium and zinc were well dissolved but also a higher concentration of iron was dissolved with respect to the ChCl:LA (1:2). Overall, in the ChCl:TLA (1:2) the dissolution trend was as follows: CdO (93 g L−1), PbO (90 g L−1), Cu2O (83 g L−1), CuO (60 g L−1), Fe2O3 (50 g L−1), FeO (20 g L−1). Noticeably, ChCl:TLA (1:2) was the best mixture for the dissolution of copper oxides, both as cupric and cuprous oxide.
The ChCl:DTT (1:3) had strongly different dissolution trends, corresponding with its dissimilar and less acidic dithiothreose sugar structure. In this mixture, metal oxides were dissolved to a lower extent: PbO (80 g L−1), Fe2O3 (30 g L−1), ZnO (21 g L−1), CdO (12 g L−1). Lead was the only metal with a marked solubility in this mixture, and the ChCl:DTT (1:3) was the sole mixture capable to solubilize PbO. In this case, the low dissolution could be correlated not only to the ligand structure but also to the overall reduced media acidity, which might have influenced oxide dissolution.
A similar result was observed for the dissolution of cobalt(II) oxide in the ChCl:TGA (1:2). As the graph shows, the highest dissolution of cobalt oxide is present in the ChCl:TGA (1:2) mixture, both as cobalt(II) oxide and as lithium cobalt(III) oxide. However, a few days after dissolution the filtrate of the cobalt samples presented some spontaneous precipitation. This phenomenon was further studied via the UV-vis absorption spectroscopy. The UV-vis spectra showed two groups of peaks: one group assigned to the cobalt(II) chloride complex (631 nm, 668 nm, 696 nm), the other group to the thioglycolate complex (324 nm, 405 nm, 507 nm).32,33 The sample was of a turbid dark purple/brown colour and it was filtered to remove the turbid precipitate observed. After filtration the sample had a clear light blue colour. The UV-vis spectra of the filtered sample confirmed the disappearance of the group of peaks belonging to the thioglycolate complex. When the spectra of the sample were measured as a function of time, the slow re-appearance of the thioglycolate group of peaks was observed. This indicates that the dissolved cobalt(II) was soluble as a cobalt chloride and slowly precipitated out of the solution as a thioglycolate complex.
The dissolution of coinage metal oxides was analysed. Whereas silver was insoluble in all of the samples, gold and copper oxides were soluble in a few mixtures. Gold oxide was soluble only in the mixtures not containing thiols (i.e. ChCl:GA (1:2) and ChCl:LA (1:2)). On the other hand, copper was soluble as both the copper oxides (i.e. CuO and Cu2O) in both the ChCl:LA (1:2) and the ChCl:TLA (1:2) mixtures, while only copper(I) oxide was soluble in ChCl:GA (1:2) (Table 4).
The dissolution of the late transition metals belonging to Group 12 was then investigated. For these metals, the UV-vis spectra were not of use because these divalent metal ions are spectroscopically silent. In all the samples there was dissolution of both zinc and cadmium. The highest level of dissolution was experienced in ChCl:TGA (1:2), but also ChCl:TLA (1:2) performed well (Table 4).
Iron had a marginal but still significant dissolution. Iron was mostly soluble as iron(III) but the mixtures of the thiol-acids were also capable to dissolve iron(II) oxide. The ChCl:TLA (1:2) mixture had the highest solubilizing power for iron. The selectivity analysis of the metal dissolution within the various mixtures clearly shows how the iron solubility affects metal selectivity against it (Fig. 2). Considering both the metal oxide solubility and the dissolution selectivity it can be seen that cadmium and zinc had the highest solubility in the ChCl:TGA (1:2) mixture. In this medium, we report the highest metal content and the highest selectivity for the metals belonging to the Group 12. Comparatively, copper and gold showed overall a higher dissolution and selectivity in the α-alcohol–acid mixtures with respect to the α-thiol–acid counterparts. Finally, the ChCl:DTT (1:3) mixture showed a remarkable selectivity for lead and it was the only mixture of the studied DESs to dissolve PbO to a significant extent.
Fig. 2 Graphical representation of the dissolution selectivity of the subset of the metal oxides selectively dissolved in large amounts in the DESs vs. iron oxides dissolution. This is a numerical elaboration of the data are listed within Table 4. Each of the listed metal oxide was normalized by the amount of iron oxides dissolved under the same conditions. |
Another sample analysis was done via dilution of the DES samples (1:100 or 1:1000) with an aqueous solution of nitric acid (1%) (vide ESI Table S1†). After this dilution, some samples formed a precipitate, which was filtered off. The ICP-OES analysis indicated a virtually complete precipitation of gold and a partial precipitation of few other metals (vide ESI Table S1;† i.e. Cu, Zn, Co). The complete precipitation of gold was mostly selective with respect to the other metals studied and it has potential as a gold concentration technique from mixed metals matrices.34 This behaviour can be explained by the need for a strongly complexing anion to solubilize the Group 10 metals in aqueous mixtures. The absence of a strongly complexing anion, such as the chloride anion in the aqua regia sample, resulted therefore in the precipitation of the dissolved metal in the solution where only water is present. Analogously to gold, copper precipitated but to a minor extent in most of the samples. The ChCl:TLA (1:2) mixture was an exception to such behaviour, having the highest levels of dissolution and precipitation of copper, reaching an 81% of overall copper content precipitation. Instead, zinc had a minor but consistent precipitation throughout the samples (15–25%).
All thiol-containing DESs showed improved physical properties (i.e. lower viscosity, wider liquid range). Moreover, thiol-containing DESs had improved solubilities for late transition metals (i.e. copper and zinc), which are valuable metals often present in low grade ores or metal processing residues.
Group 12 metal oxides achieved the best dissolution in β-thiolacids mixtures. These metals were dissolved in high amounts and a fair selectivity. Aqueous dilution (with nitric acid 1%) of such mixtures yielded a partial selective precipitation of zinc. A different trend was observed for Group 10 metal oxides. While gold was not dissolved in the thiol-containing DESs, the best dissolution for copper oxides was achieved in the ChCl:TLA. Over 80% of the dissolved copper could be recovered via precipitation in water (with nitric acid 1%).
In conclusion, thiol DESs have better physico-chemical properties then their alcohol analogues and metal affinities which may allow their use as agents in the selective dissolution of valuable late transition metals (i.e. copper and zinc) and toxic metals (e.g. cadmium and lead), which are incompatible with aqueous processing.35 In order to determine the applicative efficacy, further studies may be directed to test the dissolution of actual samples in the studied DESs.
Footnotes |
† Electronic supplementary information (ESI) available: characterisation, material and equipment specifications are available within supporting information. See DOI: 10.1039/d0ra03696j |
‡ Raw data files and additional ESI are available at the DOI: 10.5281/zenodo.3750813. |