Preparation of water soluble poly(aniline) and its gas-sensitivity

Abstract

Water soluble poly(aniline) was prepared using the chemical oxide method by adding a small amount of poly(sodium-p-styrenesulfonate). Poly(aniline) composite film on interdigital electrodes of carbon was formed via the spin-coating approach. After pretreatment of exposure in an alkalescence atmosphere and desorption with high-purity N2, the film showed an excellent sensitivity to trimethylamine of 5.14 × 10−7 mol mL−1. Moreover, this film also had a good selectivity to analogous gases and a fast response while exhibiting a good reproducibility. It was easily recovered by high-purity N2.

Graphical abstract: Preparation of water soluble poly(aniline) and its gas-sensitivity

Article information

Article type
Paper
Submitted
11 Feb 2005
Accepted
04 Apr 2005
First published
22 Apr 2005

Green Chem., 2005,7, 507-513

Preparation of water soluble poly(aniline) and its gas-sensitivity

X. Ma, M. Wang, H. Chen, G. Li, J. Sun and R. Bai, Green Chem., 2005, 7, 507 DOI: 10.1039/B502192H

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements