Issue 18, 2011

Highly-crystallized quaternary chalcopyrite nanocrystalsvia a high-temperature dissolution–reprecipitation route

Abstract

Quaternary chalcopyrite (Cu2CoSnS4, Cu2ZnSnS4) nanocrystals displaying high crystallization and controlled morphology were synthesized via a high-temperature growth regime achieved by dissolution–reprecipitation of tailored ultrafine precursors in the temperature range 400–500 °C.

Graphical abstract: Highly-crystallized quaternary chalcopyrite nanocrystalsvia a high-temperature dissolution–reprecipitation route

Article information

Article type
Communication
Submitted
08 Feb 2011
Accepted
10 Mar 2011
First published
25 Mar 2011

Chem. Commun., 2011,47, 5229-5231

Highly-crystallized quaternary chalcopyrite nanocrystalsvia a high-temperature dissolution–reprecipitation route

J. Y. Chane-Ching, A. Gillorin, O. Zaberca, A. Balocchi and X. Marie, Chem. Commun., 2011, 47, 5229 DOI: 10.1039/C1CC10749F

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.