Abstract

Oxidative stability of high density polyethylene (HDPE) containing C-alkylcalix[4]pyrogallolarenes was compared with the oxidative stability of HDPE containing 1,2,3-trihydroxybenzene (pyrogallol) and 2,6-di-tert-butyl-4-methylphenol (BHT). The Arrhenius kinetic parameters (Ea, Z, k) of non-isothermal thermo-oxidative decompositions indicate that C-alkylcalix[4]pyrogallolarenes are effective antioxidants acting at temperatures above 150 °C.

Graphical abstract: Calix[4]pyrogallolarenes as novel high temperature inhibitors of oxidative degradation of polymers

Supplementary files

Article information

Article type
Communication
Submitted
19 Oct 2011
Accepted
24 Oct 2011
First published
08 Nov 2011

Polym. Chem., 2012,3, 93-95

Calix[4]pyrogallolarenes as novel high temperature inhibitors of oxidative degradation of polymers

P. Ziaja, K. Jodko-Piorecka, R. Kuzmicz and G. Litwinienko, Polym. Chem., 2012, 3, 93 DOI: 10.1039/C1PY00494H

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements