Aging behavior of the silicone dielectric elastomers in a simulated marine environment

Abstract

A series of silicone–barium titanate composites (multiple specimens of each sample), designed as dielectric elastomeric films to be used as active elements in wave energy conversion devices, were immersed in artificial sea water in pseudo-dynamic conditions. While some of specimens were extracted after half a year and subsequently subjected to UV irradiation for 500 h (ASW1/2 + UV procedure), the rest were kept in the saline environment for one year (ASW procedure). The changes that occurred in the structure and morphology as well as in mechanical and dielectric properties were assessed by comparing the obtained results to those of the original samples. Thus, the surface and cross-section morphology was studied by Scanning Electron Microscopy (SEM) having an attached Energy Dispersive X-ray system (EDX), which was used for qualitative elemental analysis and elemental mapping. Changes in surface roughness due to the aging of samples were estimated on the basis of Atomic Force Microscopy (AFM) measurements. The thermal transitions were identified from the Differential Scanning Calorimetry (DSC) data and based on these, the crystallinity degree of the samples was evaluated in each of the three stages. The changes in the structural order were also verified by Wide Angle X-ray Diffraction (WAXD). The tensile toughness, as the amount of energy per volume unit that the material can absorb until failure, was estimated by the area under tensile stress–strain curves. The toughness at 100% elongation was determined on the basis of cyclic stress–strain curves of the original samples as an indirect measure of the energy that the elastic material could release when force that acted on it is removed, like in an energy harvesting system. The aging effect on the viscoelasticity of the samples was evaluated by dynamic mechanical analysis (DMTA), while dielectric spectroscopy was used to estimate the changes in dielectric properties.

Graphical abstract: Aging behavior of the silicone dielectric elastomers in a simulated marine environment

Supplementary files

Article information

Article type
Paper
Submitted
30 Oct 2015
Accepted
12 Jan 2016
First published
15 Jan 2016

RSC Adv., 2016,6, 8941-8955

Author version available

Aging behavior of the silicone dielectric elastomers in a simulated marine environment

A. Bele, G. Stiubianu, S. Vlad, C. Tugui, C. D. Varganici, L. Matricala, D. Ionita, D. Timpu and M. Cazacu, RSC Adv., 2016, 6, 8941 DOI: 10.1039/C5RA22780A

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements