Issue 59, 2016

Catalytic cracking of n-pentane over CLD modified HZSM-5 zeolites

Abstract

With the intrinsic MFI structure well-preserved, HZSM-5 zeolite was controllably surface-modified via a CLD (chemical liquid deposition) strategy and wrapped by tailorable porous SiO2 or TiO2 overlayers. It was found that the CLD-modified catalysts brought about a (maximum 46%) promotion of catalytic activity using the catalytic cracking of n-pentane as a model reaction at 500 °C, attributed to the enhanced sorption process caused by the porous overlayer. In addition, TiO2-CLD modified zeolites exhibited a better catalytic cracking performance compared with SiO2 that was probably due to the extra Lewis acid sites generated by TiO2.

Graphical abstract: Catalytic cracking of n-pentane over CLD modified HZSM-5 zeolites

Supplementary files

Article information

Article type
Paper
Submitted
19 Apr 2016
Accepted
01 Jun 2016
First published
02 Jun 2016

RSC Adv., 2016,6, 54580-54588

Catalytic cracking of n-pentane over CLD modified HZSM-5 zeolites

X. Hou, Y. Qiu, X. Zhang and G. Liu, RSC Adv., 2016, 6, 54580 DOI: 10.1039/C6RA10102J

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements