Activity of La0.75Sr0.25Cr0.5Mn0.5O3−δ, Ni3Sn2 and Gd-doped CeO2 towards the reverse water-gas shift reaction and carburisation for a high-temperature H2O/CO2 co-electrolysis

Abstract

The syngas mixture of CO and H2, e.g. from natural gas reforming, is currently an important feedstock supplier for the synthesis of numerous chemicals. In order to minimize fossil source dependency and reduce global warming, alternative processes to produce syngas, such as high-temperature co-electrolysis of H2O and CO2 via the internal reverse water-gas shift (RWGS) reaction, may be meaningful. In this study, the influence of the H2 : CO2 ratio on the activity, selectivity and stability of the as-prepared La0.75Sr0.25Cr0.5Mn0.5O3−δ (LSCrM) and Ni3Sn2 as well as commercial Ni and Gd-doped CeO2 (GDC20) powder materials for the reverse RWGS reaction was investigated in a tubular quartz glass reactor at 700 °C and 800 °C and ambient pressure. The highest conversion factor close to the maximum value of 50% for CO was yielded for the LSCrM, Ni and GDC20 samples by applying a 0.5 : 0.5 H2 : CO2 feed ratio at 800 °C. Similar activity was calculated for the Ni3Sn2 alloy after normalization to the Ni mass content. Moreover, all the investigated catalysts exhibited higher selectivity for CO and H2O products than Ni, with which CH4 molar concentrations up to 0.9% and 2.4% were collected at 800 °C and 700 °C, respectively. The influence of feed pressure on the carburisation process was inspected in a tubular Ni–Cr reactor. Under a carbon-rich gas mixture at 3 bar and 700 °C, large amounts of graphitic carbon were deposited solely on the Ni sample after 100 h of exposure time. After the exposure of the powder materials to 0.5 : 0.5 and 0.9 : 0.1 H2 : CO2 atmospheres for 300 h at 700 °C and 10 bar, traces of amorphous carbon were surprisingly detected only on Ni3Sn2 powder via Raman microscopy. Thus, because GDC20 ist not active for electrochemical H2 production, LSCrM or a mixture of both LSCrM and GDC20 materials appears to be the most promising candidate for Ni substitution in high-temperature H2O/CO2 co-electrolysis.

Graphical abstract: Activity of La0.75Sr0.25Cr0.5Mn0.5O3−δ, Ni3Sn2 and Gd-doped CeO2 towards the reverse water-gas shift reaction and carburisation for a high-temperature H2O/CO2 co-electrolysis

Supplementary files

Article information

Article type
Paper
Submitted
13 Jan 2020
Accepted
18 Feb 2020
First published
10 Mar 2020
This article is Open Access
Creative Commons BY-NC license

RSC Adv., 2020,10, 10285-10296

Activity of La0.75Sr0.25Cr0.5Mn0.5O3−δ, Ni3Sn2 and Gd-doped CeO2 towards the reverse water-gas shift reaction and carburisation for a high-temperature H2O/CO2 co-electrolysis

N. Bogolowski, B. Sánchez Batalla, B. Shin and J. Drillet, RSC Adv., 2020, 10, 10285 DOI: 10.1039/D0RA00362J

This article is licensed under a Creative Commons Attribution-NonCommercial 3.0 Unported Licence. You can use material from this article in other publications, without requesting further permission from the RSC, provided that the correct acknowledgement is given and it is not used for commercial purposes.

To request permission to reproduce material from this article in a commercial publication, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party commercial publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements