Issue 2, 2022

Understanding the direct relationship between various structure-directing agents and low-temperature hydrothermal durability over Cu-SAPO-34 during the NH3-SCR reaction

Abstract

Cu-SAPO-34 catalysts used for the selective catalytic reduction with ammonia (NH3-SCR) reaction deteriorate when exposed to moisture at low temperature (<100 °C), which seriously hinders their commercial application prospects. In this work, Cu-SAPO-34 catalysts templated using various structure-directing agents (SDAs), i.e., DEA, TEA, PA, and TEAOH, were elegantly fabricated via a “one-pot” protocol. The direct relationship between the various SDAs and low-temperature moisture degradation were determined in this work. Via thorough characterizations, it was evidenced that the Cu-SAPO-34 catalysts with more Si–O(H)–Al bonds, more Cu(OH)+ moieties and fewer CuOx clusters exhibited higher SCR catalytic activities and N2 selectivity. After low-temperature hydration treatment, the relative crystallinity, porosity, Si–O(H)–Al density, and active Cu(OH)+ in the catalysts declined, but in varying degrees, where the Cu-SAPO-34 catalysts possessing more Si–O(H)–Al density and Cu(OH)+ moieties being the more susceptible to hydrolysis and structural degradation, and vice versa. In situ diffuse reflectance infrared Fourier transform spectroscopy (DRIFTS) analysis confirmed that both the fresh and degraded Cu-SAPO-34 catalysts primarily follow the Langmuir–Hinshelwood pathway due to its faster reaction rate and lower reaction barrier than the Eley–Rideal pathway.

Graphical abstract: Understanding the direct relationship between various structure-directing agents and low-temperature hydrothermal durability over Cu-SAPO-34 during the NH3-SCR reaction

Supplementary files

Article information

Article type
Paper
Submitted
10 Nov 2021
Accepted
13 Dec 2021
First published
15 Dec 2021

Catal. Sci. Technol., 2022,12, 579-595

Understanding the direct relationship between various structure-directing agents and low-temperature hydrothermal durability over Cu-SAPO-34 during the NH3-SCR reaction

S. Zhang, Y. Meng, L. Pang, Q. Ding, Z. Chen, Y. Guo, W. Cai and T. Li, Catal. Sci. Technol., 2022, 12, 579 DOI: 10.1039/D1CY02046C

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements