Issue 16, 2022

Comprehensive analysis of the temperature dependence of the crystal structure of (1−x)K0.5Na0.5NbO3xBa(Li1/4Nb3/4)O3 piezoelectric ceramics

Abstract

Much attention has been paid to the characterization of the piezoelectric properties and crystal structure of K0.5Na0.5NbO3 (KNN)-based ceramics with Li substitution for the A-site to date. In contrast, this study describes the influence of Li substitution for the B-site in KNN-based ceramics on the phase stability and of the piezoelectric properties of the ceramics. Thus, the Ba(Li1/4Nb3/4)O3 (BaLN) perovskite in which Li occupies the B-site was chosen as an additive; the crystal structure and piezoelectric properties of (1−x)KNN–xBaLN (x = 0–0.05) ceramics were investigated in this study. The introduction of a multiphase region consisting of orthorhombic (Amm2) and tetragonal (P4mm) phases was succeeded by BaLN addition. The variations in the peak intensity of X-ray powder diffraction (XRPD) patterns at room temperature and 7Li solid state NMR spectra implied that the multiphase region was stable at x ≦ 0.01, whereas the presence of a minor secondary phase was suggested at x > 0.01. The presence of a multiphase region as a function of temperature was also characterized by in situ synchrotron XRPD together with Rietveld analysis, in situ Raman spectroscopy, differential scanning calorimetry (DSC), and measurement of the dielectric constant. The disappearance of the dielectric peak around 200 °C, which corresponded to the phase transition from the orthorhombic to tetragonal phase, was observed, suggesting the broadening of the multiphase region at room temperature. Although the multiphase region at x = 0.01 was relatively stable at temperatures below 175 °C, a remarkable decrease in the fraction of the orthorhombic phase from 52.5% to 12.5% was observed in the temperature range of 175–200 °C where the presence of a DSC peak and the Raman shift of the A1g mode were also recognized. The coexistence of orthorhombic and tetragonal phases leads to the enhancement of the piezoelectric constant from 98.4 to 193.7 pC N−1 in the composition range of 0–0.01.

Graphical abstract: Comprehensive analysis of the temperature dependence of the crystal structure of (1−x)K0.5Na0.5NbO3–xBa(Li1/4Nb3/4)O3 piezoelectric ceramics

Supplementary files

Article information

Article type
Paper
Submitted
03 Nov 2021
Accepted
22 Mar 2022
First published
22 Mar 2022

J. Mater. Chem. C, 2022,10, 6444-6455

Comprehensive analysis of the temperature dependence of the crystal structure of (1−x)K0.5Na0.5NbO3xBa(Li1/4Nb3/4)O3 piezoelectric ceramics

A. Kan, R. Onishi, S. Ohashi and H. Ogawa, J. Mater. Chem. C, 2022, 10, 6444 DOI: 10.1039/D1TC05306J

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements