Tony
Jin
a,
Tracy
Liu
a,
Edmond
Lam
*b and
Audrey
Moores
*ac
aCenter in Green Chemistry and Catalysis, Department of Chemistry, McGill University, 801 Sherbrooke St. West, Montreal, Quebec H3A 0B8, Canada. E-mail: Audrey.moores@mcgill.ca
bAquatic and Crop Resource Development Research Centre, National Research Council of Canada, Montreal, Quebec H4P 2R2, Canada. E-mail: edmond.lam@cnrc-nrc.gc.ca
cDepartment of Materials Engineering, McGill University, 3610 University Street, Montréal, Québec H3A 0C5, Canada
First published on 10th May 2021
In a matter of decades, nanomaterials from biomass, exemplified by nanocellulose, have rapidly transitioned from once being a subject of curiosity to an area of fervent research and development, now reaching the stages of commercialization and industrial relevance. Nanoscale chitin and chitosan, on the other hand, have only recently begun to raise interest. Attractive features such as excellent biocompatibility, antibacterial activity, immunogenicity, as well as the tuneable handles of their acetylamide (chitin) or primary amino (chitosan) functionalities indeed display promise in areas such as biomedical devices, catalysis, therapeutics, and more. Herein, we review recent progress in the fabrication and development of these bio-nanomaterials, describe in detail their properties, and discuss the initial successes in their applications. Comparisons are made to the dominant nanocelluose to highlight some of the inherent advantages that nanochitin and nanochitosan may possess in similar application.
As opposed to the acetamide group found in chitin, chitosan, a derivative of chitin, contains repeat units of β-(1 → 4)-2-amino-2-deoxy-β-D-glucose and features a primary amine functionality (Scheme 1). This functionality is typically afforded through deacetylation of chitin in basic media, resulting in hydrolysis of the acetamide group to form chitosan and acetic acid. A known unit of measurement to quantify this procedure is the degree of deacetylation (DDA), where pure chitin has a DDA of 0–15%, primarily containing acetamide groups at the C2 position, while chitosan has a DDA of 75–80%, with mostly amine functionalities on the C2 position.13 For the purpose of this review, anything referred to as “partially deacetylated chitin” will not be viewed as chitosan, as long as the DDA is below 30%. Due to this chemical modification via deacetylation, chitosan has a noted advantage in solubility in acidic, aqueous media compared to chitin, making chitosan highly applicable to current challenges.14 For example, chitosan is known to possess beneficial antimicrobial15 and antioxidant16 properties, while also displaying characteristics that are attractive for applications involving hydrogel formation for drug delivery,17 water purification,18 and metal ion scavenging,19 among others.
Both chitin and chitosan have been explored extensively as bulk systems. More recently, the idea to explore their properties at the nanoscale has emerged. Similar to envisaging the conversion of biowaste materials to value-added chemicals, the creation of functional nanomaterials is another major avenue in the pursuit to create a shell biorefinery. The forestry biorefinery serves as a model here, as it was discovered that treating cellulose pulp with various strong acids enabled the hydrolysis of the amorphous regions of the material and allowed for the release of well-defined nanocrystalline particles with high aspect ratios (on average 5 × 150 nm).20 These materials feature remarkable capabilities, such as mechanical strength greater than Kevlar,21 adhesive capabilities,22 and long-range nematic ordering behaviour23 among many others.24 Based on this initial framework, CNCs are now commercially produced worldwide by companies such as Celluforce (Canada), American Process (USA), and Melodea (Israel), with more applications and strengths being discovered.24,25 Applications for CNCs have been researched extensively26 in a number of domains, including agriculture,27 biomedicine,28 adhesives,22 and food packaging.29 Within this mind-set, exploration of both chitin and chitosan on the nanoscale is imperative to develop and even enhance current bio nanomaterial technology based on CNCs as a pathway to addressing similar challenges towards shell biorefinery.30
While terminologies vary in the literature, for the sake of this review, we will consider three main types of chitin and chitosan-based nanomaterials: nanocrystals, nanoparticles, and nanofibers. Nanocrystals are defined as nanorod-shaped biopolymers that are crystalline, spanning between 5–20 nm in width and hundreds of nm in length, depending on the source and treatment. Nanoparticles are nano-scaled materials, yet they do not feature the high aspect ratio and crystallinity typical of nanocrystals. While maintaining one of their dimensions in the nanoscale, nanofibers reach much larger dimensions in length, typically to micron sizes. For both chitin and chitosan, all three types of nanomaterials have been developed. Yet, chitosan in the nanoscale has seen fewer developments. Since the deacetylation treatment of chitin into chitosan typically comes with major structural and morphological changes in the bulk material, relying on naturally occurring order to develop these nano-scaled materials is more challenging. Recent developments are showcasing exciting avenues to achieve this goal.31,32
In Section 2, various fabrication procedures will be outlined for nanochitin such as chitin nanofibers (ChNFs), chitin nanocrystals (ChNCs), and chitin nanoparticles (ChNPs), as well as nanochitosan in the form of chitosan nanofibers (ChsNFs), chitosan nanocrystals (ChsNCs), and chitosan nanoparticles (ChsNPs). From this, Section 3 will address specific properties of these nanomaterials such as liquid crystalline behaviour, antibacterial properties, and also thermal and mechanical stability. Section 4 will highlight applications in which these nanostructures can be used, including tissue engineering, wound dressing, drug delivery, and catalysis. Finally, a future outlook in Section 5 will be provided on addressing future challenges and directions. Throughout the text, we have highlighted communalities and differences between chitin and chitosan versus cellulose to draw comparisons with the well-established field of nanocellulose.
Scheme 2 Depiction of the various subsections in this review and the pathways from the raw resources to the nanomaterial. In this review, the term “top-down” is used for methods whereby bulk materials are deconstructed down to the nanoscale, while “bottom-up” is used for methods where the material is dissolved before reshaping, for instance by crosslinking or electrospinning. Electron microscopy images are reprinted with permission from ref. 36–41. |
Two main types of approaches are used for nanochitin/chitosan formation. The first type is called “top-down” approaches and consist of extracting the nanomaterial by deconstruction of the bulk phase (Scheme 2), taking advantage of the inherent crystalline structure of the starting material as detailed in Section 2.1. For reasons explained below, this strategy is only accessible for chitin. The second type of approaches, referred to as “bottom-up” approaches, involve a dissolution step, followed by some form of “nanoshaping,” using crosslinking of electrospinning or ionotropic gelation (Scheme 2). Finally, deacetylation may be used as a means to convert chitin to chitosan in the nanoscale and is the method of choice of ChsNC fabrication.
Fig. 1 Representation of the exoskeleton structure of crab. Adapted and formatted from ref. 49. |
Extracting chitin nanofibers from bulk chitin through mechanical force is a common procedure and draws common features found in the production of cellulose nanofibers.50 In 2008, Isogai and coworkers prepared ChNFs from β-chitin extracted from squid pens through mechanical disintegration via ultrasonication.46 By testing conditions at various pH and concentration, ChNFs were produced at a pH of 3–4 and at a relatively low concentration of chitin at 0.1–0.3 wt % in aqueous conditions. They reported a width of the ChNFs at 3–4 nm, with an aspect ratio greater than 500.
Furthermore, Ifuku et al. have also reported a simple grinding technique to cause fibrillation to yield ChNFs with 10–20 nm widths.51 The authors indicated that an acidic condition is key to fabricating ChNFs, as a very small number of amino groups on the ChNFs can be charged, promoting electrostatic repulsion and subsequently fibrillation of the bulk fibrillar matrix.
The use of a purely chemical methodology can also be used to make ChNFs. For instance, Isogai and coworkers used 2,2,6,6-tetramethylpiperidine-1-oxyl radical (TEMPO) as an oxidant to fabricate ChNFs from β-chitin extracted from tubeworms.37 β-Chitin found in tubeworms contains higher crystallinity than those found in squid pens, which explains the retention of its structure to form ChNFs after TEMPO oxidation, instead of depolymerizing further into nanocrystallites and subsequent formation of ChNCs. Fig. 2 shows the transmission electron microscopy (TEM) of the as-synthesized ChNFs, along with electron diffraction.
Fig. 2 Bright-field TEM micrograph of ChNFs prepared by TEMPO-oxidation of tubeworm chitin. (top) White arrows depict “twists” in the ChNFs (top). (bottom) Bright-field TEM micrograph of ChNF, with electron diffraction diagram shown in insert, with labelled Miller indices. Adapted from ref. 37. |
For “bottom-up” approaches, the most crucial aspect lies in the ability to obtain highly solubilized chitin, essential for effective electrospinning.52 For example, Min et al. used γ-radiation to depolymerize bulk chitin to a tenth of its original molecular weight (∼900 kDa to 91 kDa) such that it can be soluble in aqueous media.53 Other works, such as Barber et al. involve the use of ionic liquids to dissolve higher molecular weight chitin, such as 1-ethyl-3-methylimidazolium acetate.48
Product | Method | Dimensions (length/width) (nm) | Advantages | Ref. |
---|---|---|---|---|
ChNCs | Chitin extraction followed by acid hydrolysis with 2.5–3 M HCl | 50–600/8–50 | “Classic method” | 38 and 56–70 |
Chitin extraction followed by acid hydrolysis with H2SO4 | 100–400/10–50 | Similar to HCl method | 72–74 | |
Using acidic deep eutectic solvents (DES) to induce acid hydrolysis | 206–1000/12–44 | Avoid excess usage of mineral acid | 82 and 83 | |
Acidic medium becomes recyclable | ||||
Carboxylated ChNCs | Radical oxidation pathway via TEMPO | 480/24 | More sustainable compared to classic method | 76–78 |
O2-laccase–TEMPO system | 400/24 | More sustainable compared to classic method | 77, 79 and 80 | |
Oxidation through ammonium persulfate (APS) | 239 ± 7/4.60 ± 0.06 | Milder, greener conditions, Cheaper reagent | 42 |
Marchessault and co-workers first prepared ChNCs using 3 M hydrochloric acid as the acidic medium, while also evidencing the liquid crystalline behaviour of these ChNCs.38 Based on this methodology of acid hydrolysis, numerous papers have described the preparation of ChNC.56 Chitin extracted from various sources such as squid pen,57 riftia tubes,58 crab shells,59–63 and shrimp shells,64–70 were then treated with HCl solutions at concentrations of 2.5 to 3 M to produce ChNC of lengths varying from 50 to 600 nm, and widths between 8 and 50 nm. Variability in this context originates from the chitin source.71 Since 2011, numerous modifications to this extraction procedure have been conducted to include exchanging the mineral acid used for hydrolysis. Sulfuric acid was first used instead of hydrochloric acid for the synthesis of ChNCs by Qin et al., with a broad distribution of ChNCs extracted, from 100 to 400 nm in length and 10–50 nm in width.72 This technique has gained traction as other groups have adapted this method for ChNC synthesis using chitin from crab shells.73,74 Similar to what has been reported for cellulose-based nanocrystals, these methods have afforded sulphate half-ester functionalities at the surface of the as-made ChNCs.75
However, the above-described mineral acid hydrolysis for ChNCs synthesis is potentially detrimentally with respect to sustainability due to the hazards associated with corrosive solution handling and wasteful effluents. Other more sustainable, yet more expensive, synthetic methods include a method by Isogai and coworkers to employ a radical oxidation pathway via TEMPO to selectively oxidize amorphous regions of chitin.76–78 In their study, TEMPO was added to NaClO as a co-oxidant, which led to the cleavage of ether linkages within the polysaccharide, and the oxidation of the C6 hydroxyl group into the carboxyl moiety. Isogai and coworkers noticed that increased NaClO concentration caused decreased ChNC length through more intense depolymerization at the ends of the ChNC.
Isogai and co-workers also demonstrated that a O2-laccase/TEMPO system could yield carboxylated ChNCs.77 In the presence of oxygen, laccase enzymes have been shown to catalyse the oxidation of phenols, anilines, and aliphatic amines.79,80 However, macromolecules such as chitin cannot access the laccase site due to their large size. Therefore, TEMPO is used as a shuttle to mediate this one-electron reaction. With this method, the fabrication of ChNCs with dimensions of 400 nm and 24 nm in length and width, respectively, was made possible.
Other methods for ChNC synthesis involve milder treatments, with the goal of sustainability and minimizing environmental waste. We demonstrated the use of ammonium persulfate (APS) as a mild oxidant in the fabrication of ChNCs.42 Like TEMPO, APS afforded fully carboxylated ChNCs, while relying on milder conditions and the use of a more economical reagent. This process was adapted from previous works that converted bulk cellulose into CNCs, highlighting a typical example of how inspiration from CNC research can be applied towards ChNCs.81
Recently, strategies using acidic deep eutectic solvents (DES) have been developed to fabricate ChNCs.82,83 While this method also induced acid hydrolysis to form ChNCs, it avoided the use of stoichiometric amounts of mineral acid during synthesis and made the acidic medium recyclable. For example, Cao et al. prepared ChNC with p-toluenesulfonic acid/choline chloride (pTA–ChCl) DES, yielding ChNCs with a width between 12–44 nm and length between 206–399 nm.82 Furthermore, Mukesh et al. prepared ChNC using choline chloride/urea DES.83 They demonstrated the recyclability of the DES by preparing a subsequent batch of ChNCs with the same DES, with the composition and morphology of the second batch of ChNC being similar to the first batch.
In one approach, an ionic crosslinker such as tripolyphosphate (TPP) reacts with the few protonated amino groups on chitin to form a nanosized particle. Critically, these methodologies rely on the presence of amine groups within the chitin polymer. Thus, they are restricted to chitins which have undergone sufficient deacetylation to possess enough of this functional group, and which have been amorphized, so that that can be solubilized and reacted with the crosslinker. For instance, Jayakumar and coworkers reported the synthesis of amorphous ChNPs using a 1 wt% TPP solution added dropwise to a 0.01 wt% solution of amorphous bulk chitin with a DDA of 40%.84 The as-synthesized ChNPs have a relative diameter of 120 ± 50 nm. Later, Jayakumar and coworkers used a similar procedure with 35% DDA–chitin starting material.85 The average size of the ChNPs produced were 324 ± 17 nm, which is on the boundary between nano and micro dimensions.
Other ChNP formation procedures include using chemically modified chitin as the substrate. Jayakumar and coworkers reported the fabrication of carboxymethyl (CM) ChNPs for use in drug delivery via a cross-linking method that uses CaCl2 and FeCl3.86 It can be noted that CM ChNPs are of particular interest for biomedical applications due to their higher solubility for hydrogel fabrication. In the case of drug delivery, crosslinking of the CM ChNPs can help decrease the rate of CM ChNP degradation within the body, which directly affects the rate of drug delivery within the body. Further, the nanoscale range of the CM ChNPs is required for elective passive targeting, such as a diameter between 200–300 nm needed for passive liver targeting. From their procedure, they succeed in producing CM ChNPs with a diameter between 200–250 nm.
Fig. 3 Bright-field TEM micrographs of (a) ChNCs and (b) the as-prepared chitosan nanoscaffold. XRD patterns of (1) ChNCs, (2) chitosan nanoscaffold, (3) lactose-conjugated chitosan nanoscaffold, and (4) maltose-conjugated chitosan nanoscaffold. Black arrows represent notable reflections of interest. Adapted from ref. 32. |
The same group further analysed synthesized ChNCs through gel permeation chromatography (GPC) measurements and observed that the obtained chitosan nanoscaffold featured increased molecular weight (137 kDa) compared to the original ChNCs (63 kDa).69 This is in stark contrast to bulk chitin reactivity, since concentrated NaOH solutions cause molecular weight reduction in bulk chitin deacetylation.
In order to prevent destruction of the ChNC morphology, careful tuning of parameters and much milder conditions are needed. As such, Hsieh and co-workers studied ChNC deacetylation with much milder conditions to retain a rod-like shape.90 Instead of deacetylation at reflux temperatures approaching 120 °C, they used a mild temperature of 50 °C. DDA reached 40% after 6 h of reaction and plateaued thereafter, even beyond 24 h. Importantly, the rod-like morphology was retained after this treatment at 6 h (Fig. 4a). The authors suggested that with these milder conditions, only the surface of the ChNC was deacetylated into chitosan, while the interior remained as ChNC, thus creating a core–shell structure. The XRD of the core–shell chitin–chitosan (Ch–Chs) nanocrystal also retained the structure found for the α-chitin polymorph, additionally implying the interior ChNC structure had not be altered by this treatment.
Fig. 4 (a) Bright-field TEM micrograph of chitin–chitosan core–shell nanocrystals. 2% uranyl acetate was used as a staining agent. (b) 2-D heteronuclear single quantum coherence (HSQC) NMR experiment of chitin–chitosan core–shell nanocrystals. (c) Kinetic curves of DD (degree of deacetylation) at different reaction temperature. (d) Curve-fitting results to deduce rate constants at different temperatures. Adapted from ref. 90–92. |
A subsequent report from the Hsieh group used high resolution liquid-state 1H NMR as a spectroscopic tool to provide further evidence of the chitin–chitosan core–shell configuration.91 To do so, they used 2-D heteronuclear single quantum coherence (HSQC) since in a 1H–13C HSQC experiment, mobile polymer strands are more susceptible to magnetization as compared to H-bonded ones (Fig. 4b). Thus, they used this method to specifically analyse mobile chains floating at the surface of prepared Ch–Chs core–shell nanocrystals, while the ChNC core remained silent. Thus, this method effectively deduced the differences between the outer chitosan shell of Ch–Chs core–shell nanocrystals and the interior chitin core.
Further works on the study of chitin–chitosan core–shell structures involved plotting kinetic curves towards the deacetylation procedure, where the rate of ChNC deacetylation could be determined at various temperatures (Fig. 4c and d).92 In addition, Arrhenius plots were conducted to determine the activation energy of deacetylation for ChNC, which was 28 kJ mol−1, a much lower number than the one for bulk chitin at 92 kJ mol−1. This has been ascribed to the higher surface area of ChNC, which made deacetylation more accessible to the surface of the ChNC.
A challenge in all of these works has been the ability to reach a DDA >75%, while also keeping the morphology of ChNCs intact in order to truly obtain rod-like ChsNCs. To solve this, our group used NaBH4 as an additive to combat nanorod degradation39 and inhibit the “end-peeling” phenomenon known for polysaccharides in a basic environment.93,94 This phenomenon is based on the alkaline pulping process of cellulose, which involves the elimination of the reducing end-groups via β-alkoxy elimination to carboxylic acids, thus degrading the polysaccharides one monomeric unit at a time.93 Simply, the hydrides from NaBH4 can reduce the alditol ends, thereby preventing end-peeling from occurring.
This method allowed for the retention of the nanorod morphology with DDA values well over 80% (Fig. 5a). Without NaBH4, aggregated spheres of what is likely degraded chitin/chitosan oligomers were imaged by TEM imaging (Fig. 5b). Currently, this is the only known synthesis path towards the formation of ChsNCs with both rod-like morphology and DDA > 80%.
Fig. 5 Bright-field TEM micrographs after deacetylation of ChNCs (a) with NaBH4 and (b) without NaBH4. Adapted from ref. 42. |
Alternatively, Tokumistu et al. used an emulsion-droplet coalescence technique to prepare ChsNPs loaded with gadopentetic acid for gadolinium neutron-capture cancer therapy.104 This was achieved by first combining a chitosan solution with an emulsifier agitated at high speed, followed by mixing the emulsion with another NaOH emulsion. Upon stirring and centrifugation, this emulsion-droplet coalescence method afforded ChsNPs of 426 nm in size. A similar method using an emulsifier was employed by Tang et al. where 1% chitosan solution was poured into a medium of petroleum ether, mineral oil, and an emulsifier.98 This dispersion medium was then stirred for 10 min at 1000–2000 rpm before isolating the desired ChsNPs. The group then compared this emulsion polymerization method with the ionic cross-linking method using TTP solution previously described. It was observed that the emulsion method produced larger nanoparticles (>200 nm), compared to the nanoparticles made in water phase using TTP solution which were too small to be collected by super-centrifugation.
While the diverse application of ChsNPs in various fields will be discussed in the sections ahead, much less can be said of the fundamental research on the mechanisms of the synthesis for these nanomaterials. Similar to the best practices in reporting inorganic colloidal nanomaterials, much more work must be done in achieving a similar level of control and characterization on these organic nanoparticles.105 For example, further studies that implement control in creating monodisperse nanoparticles are crucial in controlling directed delivery of pharmaceuticals via nanoparticles. Details regarding the structural arrangements of the ChsNP can be more thoroughly developed with tools such as XRD and solid-state NMR, which can directly probe the crystalline and amorphous nature of these nanoscale objects.
Nanofibers | Nanocrystals | Nanoparticles | ||||
---|---|---|---|---|---|---|
ChNFs | ChsNFs | ChNCs | ChsNCs | ChNPs | ChsNPs | |
Shape | Long fibers | Short rods | Spheres | |||
Average dimensions | 3–20 nm in width, 50–100 μm in length | 10–40 nm in width, 50–100 μm in length | 8–44 nm in width, 50–1000 nm in length | 5–20 nm in width, 150–250 nm in length | 100–300 nm in diameter | 50–200 nm in diameter |
Surface charge (ξ-potential) at neutral pH | −20 to −25 mV | +10 to +20 mV | 0 to −10 mV | +15 to +20 mV | +20 mV | +50 mV |
Crystallinity | Moderate – low | Low | High | Low | Moderate | Low |
The average dimensions and length-scales for each type of nanomaterial are generally consistent within the literature, though there is a dependence on which raw biomass the initial bulk chitin was extracted from (e.g., shrimp, crab, squid, fungi). Table 1 goes into more detail on specific types of ChNCs in Section 2.1.2. Similar to nanocellulose, the aspect ratios for nanofibers and nanocrystals vary significantly depending on chitin source.56
One unique property that differs between the chitin and chitosan nanomaterials is the surface charge which is quantified by measuring the zeta-potential of a suspension of the nanomaterials. In Table 2, there are distinct differences in zeta potential between the nanomaterial types associated with the variance in DDA between chitin and chitosan. There is a pH dependency on the zeta potential of chitosan linked to the presence of the amine functionality. The zeta potential of chitosan-based nanomaterials reached values up to +60 mV in acidic conditions, while values of −10 to −20 mV were found for chitosan nanomaterials at pH > 8. Most chitosan nanomaterials form very stable colloidal solutions in slightly acidic aqueous conditions (pH ≈ 5) due to the pKa of bulk chitosan being ∼ 6.2.106 Chitin nanomaterials do not show this dramatic increase in zeta potential at low pH due to the limited number of amines that can be protonated.
The last parameter is the crystallinity of the material, which can be quantified by calculating the crystallinity index (CrI) based on the XRD diffractogram of the nanomaterial. In general, it can be seen that for chitin nanomaterials, moderate to high crystallinities are seen with respect to their chitosan-based counterparts. In the macroscale, it is noted that bulk chitin has relatively high crystallinity while chitosan is amorphous, due to the fact that the fabrication of chitosan involves harsh conditions of deacetylation from chitin, which disrupts the inherent crystalline structure of chitin. Therefore, chitosan nanomaterials made from bulk chitosan will always be amorphous. Other parameters include surface functionalization groups, which depends on the process used to make the nanomaterials, or if further surface functionalization has been performed. For example, carboxylated ChNCs have been covered in Section 2.1.2, while carboxylated ChNFs are also known and reviewed in Section 2.1.1.
Fig. 6 Optical micrograph (with crossed polars) of the anisotropic phase of a 5 wt% suspension of ChNCs. The fingerprint-like pattern, characteristic of a cholesteric texture, exhibits periodic lines with a spacing of ∼30 μm, corresponding to half the cholesteric pitch (p/2). Inset depicts a visualisation of how the nanocrystals arrange to produce this pattern, subsequently showing how the spacing depicts p/2. Adapted from ref. 38. |
Further work from the same group investigated the mechanism of phase separation and self-assembly of ChNCs, as well as the role that electrostatic repulsion plays in the ChNC structure.113 Through phase diagrams, it was shown that varying the NaCl concentration (and thereby the ionic strength of the medium) did not change the overall phase diagram for concentrated samples of ChNCs, as the contribution of the ChNCs themselves were large. They also reported zeta potential measurements as well as interaction energy calculations that were comparable to theoretical calculations made using Onsager theory.
Based on this framework, Belamie et al. further examined the chirality of ChNC suspensions by quantifying nematic properties such as the nematic order parameter and cholesteric pitch.114 Measurements of the cholesteric pitch as a function of HCl concentration were conducted (Fig. 7) by measuring optical micrographs of the anisotropic phase. From these measurements, it was observed that the liquid-like positional order is stronger at lower ionic strengths, which is very common with electrostatically stabilized colloids. Phase diagrams were also reported with a ChNC concentration range between 1 to 7 wt% and ionic strength ranging between 10−5 to 10−2 M, which further confirms the experimental results of Marchessault and coworkers that the system exhibits bulk phase separation with a large pH range, but there is minimal contribution to ionic strength.113
Fig. 7 (a) Variation in the average cholesteric pitch in biphasic samples prepared at different HCl concentrations. Each data point is the average value of data taken along a dilution series in the biphasic domain. The entire set of pitch values is shown for HCl = 2.5 × 10−3 M (crosses). The line represents a visual guide of the trend. The inset shows the evolution of the pitch as a function of chitin concentration for the case where HCl = 10−4 M. Every pitch value reported in the graph is an average taken over 10–50 measurements made along the capillary tube axis. The measurements were made through measuring (b) an optical image of the anisotropic phase. The T axis depicts the capillary axis. A and P vectors represent the crossed polars. Adapted from ref. 114. |
Polarized optical microscopy (POM) is an extensively-used technique to investigate the optical birefringence typically observed for lyotropic liquid crystalline phases.115 As seen in work by Liu et al., the optical birefringent patterns of ChNC dispersions appear at 5 wt% concentration in aqueous media (Fig. 8a).116 Further POM imaging of ChNC suspension droplets in silicone oil (Fig. 8b–e) demonstrated the formation of the cholesteric phase, indicating that self-assembly occurred due to concentric ordering within the droplet surrounded by an oil medium. This feature is similar to the observations made with CNCs.117
Fig. 8 POM images of different concentrations (top) of ChNC dispersions in (a) capillary form; (b) ordinary light images of the droplets of ChNCs dispersions in silicone oil with different concentrations; (c–e) POM images of the droplets of different concentrations of ChNCs dispersion in silicone oil with varying magnifications. Reproduced with permission from ref. 116. |
More recently, Oh et al. explored the formation of the chiral nematic phase with ChNFs as opposed to ChNCs.118 A “natural” method was used involving the dispersion of bulk chitin into a Ca–methanol gel, which was then solvent exchanged with other isopropyl alcohol (IPA) and water. While a nematic liquid crystalline phase could be observed after solvent exchange with IPA, a chiral nematic phase formed after solvent exchange with water. The incorporation of Ca2+ cations was key during the formation of the chiral nematic phase, likely due to the high binding affinity of Ca on chitin, which can then screen the hydrogen-bonding interactions that make ChNFs aggregate in the bulk form. These gels were then incorporated into an epoxy resin, whereby Young's modulus and toughness tests demonstrated that the ChNF hydrogel featured the highest mechanical durability, likely due to the highly ordered nature of the gel.
Recently, further investigations have been performed in studying how specific fabrication parameters and conditions can affect the self-assembly behaviours of ChNC. These parameters include acid concentration and hydrolysis time during ChNC formation, as well as DDA, pH, and ionic strength conditions when making the liquid crystalline phases. Vignolini and coworkers conducted an in-depth study on these parameters, in which they used ChNC synthesized from the acid hydrolysis of prawn shell chitin.119 In general, increasing reaction time and concentration of HCl during acid hydrolysis results in smaller ChNCs, which increased the cholesteric pitch of the liquid crystalline suspension. Further, ultrasonic tip sonication was also a variable, in which larger energy and time spent on tip sonication of the ChNC suspension could break up large bundles present in the suspension. Thus, sonication can induce a smaller twist and higher pitch value. Specifically, they compared using raw chitin (DDA ∼ 2%) and partially deacetylated raw chitin (DDA ∼ 11%) to produce ChNCs. However, after acid hydrolysis, it was evidenced that the DDA for both synthetic variations of ChNC produced similar values, and that hydrolysis conditions exfoliated the crystalline areas in a way to remove deacetylated portions of the chitin. The main parameter in changing the cholesteric pitch value was the adjustment of ionic strength and pH, producing opposing effects on the self-assembly characteristics. When the HCl concentration was increased while maintaining a similar ionic strength with NaCl, the pitch increased. This relationship was expected due to the repulsive forces involved with the protonation of the few amines present at low pH. When ionic strength is not controlled with increasing HCl concentration, a non-linear trend in pitch emerges: the pitch increases up to a certain peak concentration, and then substantially shortens at elevated HCl concentrations beyond this peak concentration, indicating that ionic strength is the dominant factor in determining pitch rather than the repulsive forces that were previously dominant.
However, there is one existing report by the group of MacLachlan to organize ChsNFs into a left-handed chiral nematic structure within a hydrogel.120 The ChsNFs were prepared through sequential soaking of shrimp with acid and alkali baths to remove protein and minerals, and then treated three times with concentrated NaOH at 80 °C. Interestingly, the ChsNFs were then acetylated with acetic anhydride to create a hydrogel with reversible swelling behaviour through water absorption. This swelling substantially increased the thickness of the hydrogel by several-fold, which is reported to be much higher than the pristine ChsNF hydrogel with nematic ordering. Further experiments included the incorporation of a poly(methylmethacrylate) (PMMA) polymer into the acetylated ChsNF matrix increases the response to swelling behaviour as well as mechanical durability. The PMMA–ChsNF hydrogel exhibited varied colours based on the swelling of the gel, as well as retention of the left-handed chiral nematic structure.
Fig. 9 Minimum inhibitory concentration (MIC) as a function of (a) DDA and (b) quantity of cationic amino groups on the ChNC. Adapted from ref. 122. |
These results are further supported by another study from Oh and coworkers, in which they also demonstrated the importance of the positively charged protonated amino group.125 Through comparison of as-made partially deacetylated ChNCs with other types of nanochitin material such as ChNF, ChNCs, and carboxylated ChNCs made through TEMPO-mediated oxidation, they showed excellent antibacterial behaviour of the partially deacetylated ChNC based on presence of positive charges.
Much of the literature of the antibacterial properties of ChNCs and ChNFs have been based on blending these nanomaterials with other polymers to make polymer nanocomposite materials. For instance, Shankar et al. investigated using ChNCs as nanofillers for carrageenan to create a homogeneous nanocomposite film.126 In this study, the incorporation of ChNCs promoted antibacterial activity towards L. monocytogenes and E. coli bacteria. While a clear mechanism for antibacterial behaviour has yet to be proven, the authors suggested a possible pathway in which the ChNFs made the bacteria flocculate, thereby preventing growth through a lack of nutrients and dioxygen.
Copello and co-workers further investigated the use of ChNCs in antimicrobial finishings of textiles.127 In this case, ChNCs were used primarily for their durability, biocompatibility, and high surface area for methylparaben adsorption, which was the antimicrobial agent of choice. A major challenge with antimicrobial coatings of textiles is leaching during washing cycles (i.e., laundering the textile after use). Controlled release of methylparaben was observed after 20 washing cycles, indicating that the ChNCs embedded in a silica matrix can act to reduce leaching of methylparaben in textiles, thus prolonging the antimicrobial finishing. Further, consistent bacterial reduction for various bacteria strains such as P. aeruinosa and S. aureus were seen for the composite material, as opposed to control variables without ChNCs (Fig. 10). This demonstrates that ChNCs have enormous potential in antimicrobial coatings, with potential for further development with other systems.
Fig. 10 Bacterial reduction (%) versus washing cycle number for (a) P. aeruginosa and (b) S. aureus. FM = only methylparaben mixed with textile, FMW = methylparaben adsorbed onto ChNC mixed with textile, FMT = FM immersed in mixture of tetraethyl orthosilicate (TEOS) then mixed with textile, FMWT = FMW in mixture of TEOS then mixed with textile. Adapted from ref. 127. |
Other applications for antibacterial and antioxidant properties of ChNCs involve food packaging material, where microbial spoilage is a major issue in food quality and preservation.128 Sun and coworkers demonstrated that, compared to free lysozymes, lysozymes immobilized onto ChNCs can promote antimicrobial activity.129 This study spurred the possibility of ChNCs as a key nanomaterial for use as an antibacterial agent in food preservation.
Due to the water solubility of ChsNPs, Anitha et al. further investigated antibacterial activity of chitosan's water-soluble derivatives, O-carboxymethyl chitosan (O-CMC) and N,O-carboxymethyl chitosan (N,O-CMC), in nanoparticle form.100N,O-CMC was found to have the strongest antibacterial effect for its higher degree of carboxymethyl substitution, most likely due to its greater solubility in aqueous media.136 A study conducted by Xing et al. on oleoyl-chitosan nanoparticles (OCNPs) also found that this material exhibited an ability to permeate E. coli and S. aureus cells, causing pore formation on the cell membrane and the release of intracellular components.137 Based on this work, OCNP was shown to be a novel antibacterial dispersion system with great potential.
Nanochitosan has also been explored for its antifungal properties. Divya et al. found ChsNPs inhibit four different strains of fungi, mostly with increased inhibition rates at higher concentrations (Fig. 11).138 Its antifungal activity was also shown to be more effective than amphotericin, a common antifungal medication. The group elucidated the antifungal mechanism of ChsNPs through microscopic observation, and concluded that disruption of the cell membrane, and thus cell lysis, was caused by the ChsNP's cationic character, as was explained previously for bacteria. Sathiyabama and Parthasarathy also observed higher antifungal activity for nanochitosan than for bulk chitosan against multiple phytopathogens, and assumed that it is a result of the material's increased permeability towards cell membranes in the nanoscale.139 The higher zeta potential and lower polydispersity index of the ChsNPs also contributed to the improved stability and effectiveness of its antifungal activity. Furthermore, antifungal properties were also observed in nanochitosan blended with Zn and Cu, along with additional benefits such as enhanced plant defence enzymes.140 In a biomedical context, Mubarak Ali et al. compared the antimicrobial activity of ChsNPs against pathogenic bacteria and fungi and found that C. albicans required a higher concentration of the ChNPs for effective fungicidal activity.141 The thick cell wall was hypothesized to explain this finding, as the complex components can delay or hinder cellular lysis more effectively against the ChsNPs, further supporting the postulated antimicrobial mechanism for ChsNPs.
Fig. 11 Percent rate inhibition against four strains of fungi (a) by increasing concentration of ChNP (10–50 mg ml−1) (b) by ChNPs grown in potato dextrose agar. Adapted from ref. 138. |
Nanochitosan's anti-pathogenic properties against bacteria and fungi have been exploited for many agricultural products, including as a coating material for refrigerated fish fillets, as an edible coating for bell pepper, and as a supplement for plant growth and protection – all of which aim to improve or maintain product quality.140,142,143 The material is also ideal for many biomedical applications. For instance, Ikono et al. used ChNPs for inhibition of S. mutans and C. albicans, the bacterium and fungus responsible for dental caries.144 Bone cement has also been impregnated with ChNPs as a promising candidate for combating infection from a joint implant.145
There have also been many composite materials produced that incorporate nanochitosan, and then applied as antimicrobial agents. For example, Ngo et al. observed that pectin:nanochitosan films for functional packaging inhibited growth of spoilage bacteria, fungus, and yeast while also altering water and oxygen permeability.146 Furthermore, nanochitosan-grafted flocculants were synthesized by Chen et al., and were used to successfully treat low turbidity and salmonella in water and had a superior performance to traditional organic flocculants.147
Lastly, nanochitosan has antioxidant activities. Oxidation occurs through the action of highly unstable free radicals, causing chain reactions that can damage living cells in organisms and food product quality. Antioxidant substances inhibit or delay oxidation by quenching environmental free radicals. In 2018, Alboghbeish et al. explored the effects of coating refrigerated fish with chitosan and ChsNPs for storage. 2-Thiobarbituric acid (TBA) reactive substances were used as an indicator for lipid peroxidation through the detection of fat degradation products.142 Results demonstrated that not only did the ChsNP have stronger antibacterial activity, but it also seemed to effectively protect against lipid oxidation in fish: the concentration of breakdown products was significantly reduced in ChsNP coated samples, compared to bulk chitosan. The group hypothesized that compared to bulk chitosan, the larger surface area per volume in nanoscale chitosan improved the scavenging power for OH radicals, thereby further reducing lipid oxidation. Divya et al. and Mohammed et al. also observed significant antioxidant activity in ChsNPs with different assays and reached a similar conclusion, with the intent of applying ChsNPs as an edible coating on vegetables to extend shelf-life, displaying favourable properties for the agricultural industry.34,138 In addition, in a study of ChsNPs synthesized from a fungal enzyme (T-CSNP), their antioxidant activity also appeared promising when evaluated with four different tests, including total antioxidant assay, 2,2-diphenyl-1-picrylhydrazyl (DPPH) radical scavenging, total reducing power and H2O2 radical scavenging.100 A positive correlation was again observed between increasing T-CSNP concentration and antioxidant activity, yet none of the synthesized systems surpassed the positive standard, ascorbic acid.131 The free-radical scavenging ability of T-CSNPs was attributed to their amine and amino group, which explained why their antioxidant activity is higher than that of TPP-crosslinked ChsNPs.131 The antioxidant and antimicrobial effect of ChsNPs has also been exploited for biomedical purposes, such as treatment for cutaneous leishmaniasis, a skin lesion caused by a single-celled parasite.141,148,149
Overall, the amine group confers to ChsNCs their unique functionalities, which include antibacterial, antifungal, and antioxidant properties, in contrast to un-modified nanocellulose, providing a distinct advantage for nanochitin and nanochitosan to be deployed preferentially in different biological applications, as reviewed in Section 4. As seen in Section 3.2.1, any significant antimicrobial activity for nanochitin was due to partial deacetylation in order to increase the number of amines groups on the surface of the nanomaterial. Scheme 4 summarizes the trends in functional properties of all nanochitin and nanochitosan recently reported in the literature, along with the bacteria strains that were studied.
Initial tests using ChNC-incorporated composites as thermoplastics were done by Paillet and Dufresne in 2001.57 They fabricated a nanocomposite film of latex mixed with colloidal ChNCs, with a weight fraction of ChNCs between 0–20%. No noticeable effect on the shear modulus was observed for temperatures below the glass transition temperature (Tg). However, above Tg, the relaxed modulus increased by 160 times with 10 wt% (w/w) ChNC. The authors attributed this finding to the high aspect ratio of the ChNC.
ChNCs have also been incorporated into hydrogels for use as cell scaffolds and drug delivery vehicles as studied by Chen and coworkers151 Specifically, injectable hydrogels have received a lot of attention as a tool for the creation of tissue scaffolds as they can successfully offset the need for surgeries.152 To this end, hydrogels featuring high tensile strength and elastic modulus are in high demand.153 This study found that with 5% (w/w) incorporation of ChNCs into a beta-glycerophosphate-based hydrogel, gelation time of the hydrogel decreased from 6038 s to 25 s. Furthermore, the same study also observed increased mechanical durability for the hydrogels. The authors attributed these remarkable mechanical enhancements to the hydrogen bonding interactions between the glycerophosphate hydrogel and ChNC. Drug release behaviour of this hydrogel composite has also been studied, with in vitro acetylsalicylic acid (ASA) release done as the model test. With the incorporation of ChNCs, there was a much slower release of ASA likely due to the much greater crosslinking densities of the hydrogel nanocomposite. Similar results were found by Pang et al. while using ChNCs as an additive for a chitosan/dextran-based hydrogel, including shortened gelation time, increased compressive stress, as well as higher bonding strength to tissues, indicating a potential application in tissue adhesives.74 Other properties that can seemingly be enhanced by ChNCs have been demonstrated in the work of Xiong and coworkers in which gelation temperature, as well as salt and pH resistance, was increased for the ChNC enhanced gelatin.73
ChNCs can also be chemically modified using available functional groups to support other substrates. Gu and co-workers described a process in which poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) can be grafted onto ChNCs via chlorination. The polymeric ends of PHBV are chlorinated with thionyl chloride before covalently bonded to the ChNCs through the hydroxyl group. The authors reported higher melting point temperatures for ChNC-incorporated PHBV nanocomposites compared to the native PHBV. In these examples, ChNCs were able to afford the desired heightened mechanical durability due to their high aspect ratio (similar to CNCs), as well as the tuneable handle of both their acetamide and amine functionalities.
Aside from mechanical tests, the thermal parameters of these nanomaterials have also been reported. These properties include thermal expansion determined using a thermomechanical analyser, onset and peak temperature determined using differential scanning calorimetry, and thermal stability profiles determined using thermogravimetric analysis (TGA). Thermal properties are very important in applications where a material needs to be very resistant to degradation at high temperatures, such as food packaging films. Qin et al. incorporated ChNCs of up to 5 wt% into maize starch films and saw an overall increase in both onset temperature and peak temperature, showing an optimal ChNC loading of 0.5 wt% with respect to the maize film.72 Interestingly, TGA measurements showed that the maximum degradation temperature decreased with incorporation of ChNCs into the films, which the authors attributed to the decreased flexibility of the amylopectin chains in starches with ChNCs as a filler.
The mechanical durability of ChNFs have also been reported and tested for a variety of applications by Ifuku et al.154 A ChNF–(meth)acrylic resin nanocomposite film was created that was optically transparent (Fig. 12a) and exhibited good tensile strength of at least 30 MPa, depending on the type of resin used. With the inclusion of ChNF within the (meth)acrylic resin, the film's Young's modulus increased by up to 3.0 GPa, as seen in Fig. 12b. Fan et al. also observed this finding with ChNC–poly(lactic acid) (PLA) films as the thermal degradation point decreased with respect to bulk α-chitin.155 In general, this is to be expected since the nanoscale structure of ChNCs, along with all other types of nanochitin and nanochitosan, confers higher surface area, and therefore a lower threshold for withstanding higher temperature. Similar results have also been reported by Salaberria et al. by incorporating ChNCs into a starch-based thermoplastic156 and for CNC composites as well.157,158
Fig. 12 (a) Photo of Tricyclodecanedimethanoldimethacrylate (DCP) film with ChNF; (b) Young's modulus of various meth(acrylic)–ChNF films and their nanocomposites. Error bars show standard deviation. Adapted from ref. 154. |
Gelatin-based nanocomposites were also reported to be reinforced by ChNFs. For instance, Rolandi and coworkers demonstrated that the incorporation of ChNFs within gelatin methacryloyl increased the hydrogel elastic modulus 1000-fold, while also increasing stress-to-strain failure by more than 200%.159 Surface deacetylation of the ChNFs were observed to be an important parameter, as Li and co-workers had demonstrated using ChNFs with surface deacetylation to produce gelatin-based nanocomposites.160 Namely, the Young's modulus of the surface-deacetylated ChNF-containing gelatin increased 2.5-fold compared to gelatin on its own. Neat ChNFs that did not undergo a deacetylation treatment showed less pronounced results than the surface-deacetylated ChNFs. The authors suggested that improved hydrogen bonding from the amines played an important role in increasing the tensile strength of the nanocomposite.
ChNFs have also been directly applied to enhance CNC-based films used for packaging materials. The group of Meredith have shown that the incorporation of ChNFs into CNC-based films can greatly augment the film's ultimate tensile strength (UTS), with a 1:3 ratio of CNC:ChNF being the optimum conditions.161 Interestingly, even though the mixed CNC/ChNF film performed the best, a film based only on ChNF demonstrated only slightly lower UTS results. Furthermore, authors also reported that lower acetylation of the ChNF (i.e., more amines instead of acetamides) provided better results for both UTS and breaking strain. These results indicated that the positive electrostatic charge of the low acetylation ChNF can enhance aggregation with the negative charge of the CNC, therefore creating a much more compact film. Another study from the same group further validated the enhancement that ChNFs provided to CNC-based films through O2 permeability tests, in which the combination of ChNF and CNC layers could provide much less O2 permeability for use as barrier materials for food packaging.162
The coefficient of thermal expansion was also analysed for ChNF-containing nanocomposites, which typically possess an inverse relationship with the Young's modulus of a material. Ifuku et al. reported a decrease in the coefficient of thermal expansion with the incorporation of ChNFs into chitosan-based films, which is an improvement from neat chitosan films.163 This was further validated by the same group with the incorporation of glycerol in a ChNF-based film.164 This improvement was in contrast to the previously noted negative performance for ChNC-incorporated polymeric films. A direct comparison between ChNF and ChNCs was made by Salaberria et al., in which the authors realized an increase in the thermal degradation temperature in a starch-based nanocomposite with ChNFs as nano-fillers, while a decrease occurred when using ChNCs.156 They hypothesized that the as-made ChNFs contained more amino groups that can interact with the hydroxyl groups of the starch matrix, along with the minor accumulation of glycerol due to its web-like morphology.
Aside from ChNF–polymer composites, Nam et al. measured the thermal degradation behaviour of ChNFs with varying DDA values, and observed a decrease in the maximum degradation temperature of ChNFs with respect to bulk chitin.165 Furthermore, they noticed that with increasing DDA value, the maximum degradation temperature decreased. The authors attributed this finding to the lower crystallinity for the ChNFs at higher DDA.
In general, the thermal stability of ChsNPs has been observed to decrease with respect to bulk chitosan, similar to that of ChNCs. For instance, Sivakami et al. reported a decrease in thermal stability of ChsNP made using ionic gelation compared to bulk chitosan.167 Furthermore, Shajan and coworkers also indicated that the addition of ChsNPs decreased the thermal stability of a plasticized polymer nanocomposite electrolyte based on poly(ethylene oxide) for application in lithium ion batteries.168 Indeed, as more developments in the field of nanochitosan are made, much more analysis and determination of these fundamental physical properties must be assessed and understood.
On a similar vein to LCA, biodegradation is a characteristic that is often touted for materials made from polysaccharides.175 While bulk chitin and chitosan have been tested for biodegradation in soil, nanochitin and nanochitosan studies have not yet been reported.176 The impacts of their end of life treatment, handling, and performance in various environments also needs to be understood and mitigated in order to realize a net environmental benefit and enable a circular shell bioeconomy. Thus, following the framework of research that led to the development and commercialization of nanocellulose-based materials, we believe it is imperative that this gap in the literature must be filled in order to move forward in making materials sustainably as well as maintaining commercial value.
Table 3 lists the variety of drugs that currently use nanochitin- and chitosan-based delivery systems. This list is only a representative portion of the amount of literature found for using chitin- and chitosan-based nanomaterials in drug delivery with the oldest being from 2012.
Nanomaterial | Type of drug encapsulated | Application of drug | Ref. |
---|---|---|---|
ChsNP via ionic gelation | Ellagic acid | Anticancer | 194 |
ChsNP via ionic gelation | Lansoprazole | Antiulcer | 195 |
ChsNP on polycaprolactone nanofibers | Ferulic acid and resveratrol | Non-melanoma skin cancer | 196 |
ChsNP via ionic gelation | Chlorogenic acid | Antioxidant/anticancer | 197 |
Quaternary ammonium palmitoyl glycol ChsNPs | Leucine–enkaphaline peptide | Anticancer | 198 |
ChsNPs with hyaluronic acid | Curcuminoid | Anticancer | 199 |
ChsNP via ionic gelation | Jasmine oil | Anticancer | 200 |
ChsNP via ionic gelation | Recombinant antigens rEIT and rStx2B | E. coli vaccine candidate | 201 |
ChsNP via filtration | Plasmid DNA vaccine | Swine flu vaccine | 202 |
Thiolated ChsNP | Insulin | Oral delivery of insulin | 203 |
ChsNP via ionic gelation | Eugenol | Rheumatoid arthritis | 204 |
Carboxymethyl chitosan and ChsNP | Doxorubicin | Colorectal cancer therapy | 205 |
ChsNP via succinic anhydride | Herceptin targeted antibody and doxorubicin | Breast cancer | 206 |
ChsNP via ionic gelation | Curcumin with epidermal growth factor conjugation | Anticancer | 207 |
ChsNP with EGFR antibody shell | Curcuminoids | Anticancer | 208 |
Biotin-conjugated ChsNP | Bufalin | Anticancer | 209 |
ChsNP via ionic gelation | IL-2 | Colorectal cancer | 210 |
Cetuximab-conjugated ChsNP | Paclitaxel | Anticancer | 211 |
ChsNP with hyaluronic acid | MiR-34a and doxorubicin | Breast cancer | 40 |
cm-ChNPs | 5-Fluorouracil | Anticancer | 86 |
Poly(lactic acid)–Chs NP composite | Lamivudine | Anti-HIV | 212 |
ChNC–glutaraldehyde gel | Circumin loaded with Tween 20 surfactant | Anticancer | 213 |
In order to move away from molecular target therapy which focuses on a specific kinase or receptor within cancer cells, much of the research for ChsNP relies on the enhanced permeability and retention (EPR) effect, coined by Matsumura et al.214 The EPR effect relies on the fact that many solid tumours have defect sites located in their blood vessels. These defect sites produce vascular permeability factors such that large macromolecules will accumulate in tumour tissues, passing through the tumour blood vessels instead of the normal blood vessels.215,216 Fang and coworkers utilized this effect when fabricating ChsNPs with biotin, a substance known to enhance binding of macromolecules to tumour cells.209,217 This material was then loaded with bufalin, a candidate drug for cancer chemotherapy. Bufalin induces cell arrest and apoptosis in many cancer cells, yet it also has the central problem of all chemotherapeutic agents: the severe toxic effect it has on cells across the entire body.218 This application makes selective targeting especially important, which can be achieved by a dual-targeting mechanism of the EPR effect of the ChsNPs, as well as selectively binding to tumour cells that express biotin receptors. The biotin–ChsNP material loaded with bufalin demonstrated much higher cytotoxicity to MCF-7 cells, as well as improved therapeutic effects in a human MCF-7 breast cancer nude mice model.
Co-encapsulation is also possible with ChsNPs, as reported by Deng et al. with the loading of doxorubicin and microRNA-34a (miR-34a) into ChsNPs made via ionic gelation with hyaluronic acid and TPP (Fig. 13).40 An important factor in this dual loading capability is the oppositely charged nature of doxorubicin (DOX), which is positive, and miR-34a, which is negative, which can electrostatically bind to each other within the ChsNP–TPP matrix. Another notable factor is that hyaluronic acid is also known to bind to the CD44 molecule on the MDA-MB-231 breast cancer cells, making it another ideal candidate in creating targeted drug therapeutics.219Fig. 13 depicts the process of how the ChsNPs loaded with DOX and miR-34a are delivered into tumour cells directed by the CD44 receptor.
Fig. 13 Schematic illustration of the construction of ChsNPs made from chitosan (CS) and ionic gelation with hyaluronic acid (HA) and TPP (top right in the figure) for the simultaneous co-delivery of DOX and miR-34a to MDA-MB-231 human breast cancer cells for enhanced anti-cancer effects. Retrieved from ref. 40. |
As opposed to using only one form of chitosan for ionic gelation to form ChsNPs, Feng et al. implemented the use of both carboxymethyl (CM)-chitosan and “pure” chitosan to form a NP through electrostatic interactions between the positively charged chitosan and negatively charged CM-chitosan.205 Furthermore, CM-chitosan has higher aqueous solubility than chitosan, along with having a higher chance of binding Ca2+, increasing parallular permeability of the epithelium.220 Thus, CM-chitosan provides a unique access to higher solubility as well as chelating ability in NP form. The group reported a surface charge effect of loading DOX, with the positively charged CM-chitosan/pure-chitosan NP cross-linked with TPP outcompeting the negatively charged CM-chitosan/pure-chitosan NP cross-linked with Ca2+, with the former achieving enhanced cellular uptake.
Among other applications for ChsNPs in drug delivery, a wide breadth of literature exists for DNA conjugated ChsNPs as well as gene therapy, on which an excellent review was written.221 Further, other types of nanochitosan such as ChsNFs acquired from electrospinning have also received some attention in drug delivery, which has been highlighted in a recent review.222
To a lesser extent, nanochitin has also been explored for use in drug delivery. Jayakumar and coworkers fabricated magnetic CM–ChNPs crosslinked with CaCl2 and FeCl3 for in vitro delivery of 5-fluorouricil.86 This system combined the drug delivery capabilities of ChNPs with potential drug-tracking potential due to its magnetic nature, with sustained and controlled drug release as well as enhanced toxicity with KB cells. In an effort to increase mechanical durability of hydrogel for drug delivery and prolong the sustained release of the loaded drugs, ChNCs have been incorporated into the hydrogel itself. The first report of ChNC usage was claimed by Liu and coworkers in 2018, in which they used ChNCs as a cross-linker with glutaraldehyde to form a hydrogel drug carrier for the incorporation of Tween-20 loaded curcumin.213 Improved stiffness as well as mechanical strength of the hydrogel was observed. They also proposed hydrogen-bond interactions between curcumin and the hydrogel itself which enabled its prolonged release in phosphate-buffered saline (PBS). Yet, a direct mechanism for such a release was not proposed. Additional work has also been done on reinforcing alginate-based hydrogels reported by Petrova et al.,223 as well as reinforcing a chitosan/β-glycerophosphate injectable hydrogel done by Wang et al.151 The use of ChNCs conferred high mechanical durability to the materials, thanks to the highly crystalline nature of nanochitin, while ChsNPs’ amorphous nature afforded a loose structure conducive to high drug loading and sustainable release. Due to the high crystalline nature of ChNCs relative to other types of nanochitin, it is the ideal nanofiller for strengthening other composites in drug delivery vehicles.
Importantly, chitosan is one of the major polysaccharides used in current research, with ChsNPs being at the forefront of nanomedicinal efforts.
Indeed, there is still huge potential in advancing this field, as many aspects such as direct functionalization of ChsNPs or ChNCs have not been done. More specifically, thorough in-depth surface characterizations are needed for synthesized ChsNPs to determine factors such as DDA and surface functional groups and how they affect both binding and release capabilities of the drug within ChsNPs. As for the use of ChNCs as a mechanical filler for the reinforcement of gel-like systems, a molecular-level guide on how these nanomaterials behave within these gels must be characterized to its fullest extent. Importantly, the advantages of using ChsNCs which combine aspects of mechanical filler reinforcement as well as the primary amine group for drug binding can be a distinct avenue for future research.
Fig. 14 (a) Image of lap-shear measurement set-up (top) and two pieces of adhered porcine skins after tensile breaking; (b) the lap-shear adhesion strength using wet porcine as the adherent. POEC-d (50%) and POEC-d (25%) are the catechol-based adhesive with aqueous weight concentration in water in brackets. POEC-d-5%, POEC-d-10%, and POEC-d-15% are the POEC-d adhesives with 5, 10 and 15% (w/w) ChNCs with respect to POEC-d. (c) Proposed mechanism of heightened adhesion caused by addition of ChNC. (*p < 0.05). Adapted from ref. 229. |
Electrospinning is an effective and simple technique for the fabrication of nanofibers from polymers for wound healing.226 The ultrafine fiber webs formed with this technique allows for good absorption of wound exudates, prevention of dehydration and infection, gas permeability, and a sustained release of loaded drug, making this technology highly suitable for wounded tissue regeneration.224 While both chitin- and chitosan-based nanomaterials have both been used for wound healing applications, the latter has seen more use due to its higher solubility. Naseri et al. developed a crosslinked nanocomposite fiber mat based on chitosan and polyethylene oxide for wound dressing that is also reinforced with 50 wt% ChNCs.230 This mechanically and thermally strong material also had relatively low water vapor transmission rates (WVTR), controlling water loss while considering the accumulation of exudates from the wound. Besides physical reinforcement, it was hypothesized that the ChNCs improved susceptibility to lysozyme, as the breakdown product of chitin into chito-oligomers stimulated macrophage activity and collagen deposition, and thus the entire process of wound healing improved.66,225 This demonstrates the unique capabilities of ChNCs that other systems would not have, including that of nanocellulose. Fibroblast action and proliferation of injured tissues was also stimulated with wound treated with nanofibrous membranes, due to the high surface area and porosity of the electrospun nanomaterial which simulates the natural extracellular matrix.230,231 Nanofibrous membranes based on collagen, chitosan, and polyethylene oxide fabricated by Chen et al. also showed similar beneficial effects for wound healing, and authors observed that the nanofibrous membranes reduced wound area faster than traditional gauze and commercial collagen sponges in animal studies.232
This accelerated healing demonstrated that the biomaterial promoted the growth of skin tissues in a comparable way to commercial products. Izumi et al. also explored using deacetylated ChNFs on wound healing, although they did not use the electrospinning process.233 The group discovered that much greater fibroblast and collagen proliferation and re-epithelium was induced by the surface-deacetylated ChNFs in a circular excision wound model compared to bulk chitin, ChNFs, and ChsNFs.
In terms of chitosan-based nanomaterials, one study evaluated the healing efficiency of electrospun, chitosan-blend nano-Bioglass through acute skin trauma in rats and diabetic chronic wounds in mice.234 Accelerated wound healing, complete re-epithelialization, collagen deposition and alignment, and regeneration of skin appendages were observed in vivo. The complex and synergistic effect that the chitosan-based nanomaterial exerted at different stages of healing are presented in Fig. 15.232
Fig. 15 Mechanism of chitosan-blend nanomaterial at different stages of wound healing leading to accelerated and enhanced wound healing. Adapted from ref. 234. |
Kossovich et al. also found electrospun ChsNFs to be effective for treating burn wounds, most of which are often quite severe, as they involve large skin surface areas and thus have the potential to be lethal.235 As reviewed by Jayakumar et al., the material seemed to address many crucial aspects of wound healing, including moisture control, wound ventilation, protection from infection, stimulation of tissue regeneration, and degradation of material to minimize mechanical damage.225 Many other chitosan–blend nanofibers produced by electrospinning have also been explored and found to be effective for the purpose of wound healing and skin cell proliferation, such as with silk fibroin,236 poly(ethylene oxide),237 poly(vinyl alcohol),225,238,239 polyaniline,240 and gelatin.241
Besides nanofiber mats, other forms of nanoscale chitin and chitosan-based wound dressings have also been explored including hydrogels, sprays, films, and sponges.224,242 For example, Guo et al. constructed ChNP-based hydrogels through electro-assembly to be dried into porous and tough aerogels. The observed effects of the aerogel on wound healing in vivo included acceleration of macrophage migration, and promotion of granulation and vascularization.243 Mattioli-Belmonte compared the effectiveness of ChNF/chitosan glycolate-based material of wound healing in the form of a spray, gel, and gauze to find that each form provided optimal treatment effects for different types of wounds.242
Similar to epithelial tissue regeneration, chitin-based nanomaterials have also been explored as support for various disease treatments through regenerative medicine. Much work has been done in the use of hydrogels to produce cartilage tissue,244 bone tissue,245–248 tracheal tissue,249 liver tissue,87 and myocardial tissue, which is usually non-proliferative.250 The fabricated hydrogel or scaffolding material is often intended to mimic the corresponding extracellular matrix and specific environment of the tissue of interest, thus supporting cell proliferation for functional medical purposes.
Based on current literature, it appears that the use of ChsNPs in bone regeneration is relatively more developed than in other areas of regenerative medicine.251 In fact, Tao et al. specifically reviewed bone regeneration applications using nanofibers based on chitin and chitosan.252 For example, Sedghi et al. used the MTT assay, an in vitro cell viability test, to find their non-cytotoxic, antibacterial PCL-chitosan/magnesium-hydroxyaptite electrospun nanofiber scaffolds proliferated osteoblast cells at a higher rate compared to the control with no nanofiber scaffolds.246 Some studies have also addressed the regeneration of cartilage tissues relevant to the treatment of osteoarthritis.244 As bone regeneration is a main constraint for bone grafting during surgery for bone conditions, this novel, tuneable technology can potentially remove this large limitation.253
Fig. 16 Changes in skin appearance of subjects before and after in vivo treatment of nanocomposite injection. Adapted from ref. 257. |
Out of all derivatives, the results of carboxymethyl caproyl chitosan seem to be especially remarkable as they can form nano-network or nanospheres self-assemblies with strong antioxidant and antibacterial activity and good water retention properties.254 Jimtaisong et al. summarized five major functions for the material to be applied to the cosmetic dermatology: moisture retention, antimicrobial and antioxidant activity, delivery system and natural-derived emulsion stabilizer.258 In the work of Anitha et al., their carboxymethyl ChsNPs (80–100 nm in diameter) also exhibited stronger antibacterial activity against S. aureus compared to ChsNPs.100 Considering the applicability and versatility of CNCs currently being researched for cosmeceutical applications, nanochitin and nanochitosan have high potential for being used commercially with further research.259,260
There have been a few studies that propose nanochitin as a more sustainable alternative to pesticides and fertilizers to achieve similar results. Xue et al. observed that a low concentration of ChNPs in soil improved yield of winter wheat by 23.0% and 33.4%, for two different varieties.265 In the grain filling stage of growth, there were also significant increases in rate of photosynthesis, nutrient uptake, and transpiration during growth. Based on their large surface and strong properties, nanoparticles were previously reported to enhance nutrient absorption in plants. This could enable them to promote plant absorption of water from soil, along with possible organic compounds and ions attached to the nanoparticles.266 In addition, the quality of the winter wheat products in terms of zinc, iron, and grain protein content was found to have improved – one of the most important indexes for grain quality. A follow-up study by Cheng et al. concluded that the applications of nanochitin appears to significantly increase nitrogen content and promote its metabolism in the wheat plant, as the increased nitrogen supply enriches the nutritional value and enhances the yield.267 Protein, zinc, and iron deficiencies are nutrition-related health problems at a global scale.268 The capability of nanochitin at low doses to enhance the quality of a globally consumed grain provides the material with immense agricultural potential.
Zhou et al. has also explored the use of ChNCs in tobacco plants.269 The group found that low concentrations (0.001–0.005% w/v) of nanochitin suspensions shortened time for tobacco seed germination, increased stem girth and length, and increased leaf number and area (Fig. 17). For example, the incorporation of a 0.001 wt% suspension of ChNCs saw increase in the stem girth, leaf number, and maximum leaf area of tobacco seedlings by 27.28%, 19.12%, and 10.68%, respectively. Interestingly, when the concentration of the ChNC suspension was increased to 0.005 wt%, the increase in seed germination and plant growth decreased in comparison with the 0.001 wt% experiment, indicating that ChNCs have a low-dose dependence effect on plant growth. When mixed with small amounts of fungicides, nanochitin also exhibited synergistic effects on inhibiting tobacco root rot disease. Similar results of reduced time for germination and fungistatic properties are observed in a study on pepper plants (Capsicum annuum), where the effects of nanochitin were compared to that of bulk chitosan.270 Although the exact mechanism of the enhancement is unclear, nanochitin significantly reduced the mean time to germination compared to chitosan. It was hypothesized that this finding could be due to the increased permeability of nanochitin due to its smaller size, causing greater uptake of nutrients into the organelles in seed embryo relevant to germination.269,270 The use of nanochitin to replace traditional germination methods also provides antifungal properties, which can simultaneously reduce the use of traditional chemical fungicides, which can cause environmental damage.
Fig. 17 Effect of applying nanochitin on tobacco plant seedling growth. Control sample uses tap water, while nanochitin suspensions are applied in NC samples. Adapted from ref. 269. |
Similar to studies of nanochitin, many studies of nanochitosan show similar effects of enhanced plant growth and quality. Bulk chitosan has also been shown to contribute to plant growth by enhancing the plant defence system. This appears to occur through stimulating of plant-specific mechanisms, such as hydrogen peroxide production in rice.271 A few reports indicate that nanochitosan also has this effect. By primarily stimulating activity in plant defence and antioxidant enzymes, Chandra et al. found a significantly improved immune response in C. sinensis.272 The enzymes assayed showed a reduction in oxidative stress, via reactive oxygen species (ROS) scavenging. ROS are compounds oxidizing the phenolic content responsible for resisting pathogens in plants. Those enzymes include peroxidase, polyphenol oxidase, phenylalanine ammonia lyase, β-1,3-glucanase and superoxide dismutase (SOD), all of which showed 0.3% to more than 400% increase in activity.
This result echoed the study of Choudhary et al., which examined the boost in defence responses in maize upon the application of Cu–ChsNPs.273 In the same study, Curvularia leaf spot, a common disease in maize, was also significantly controlled, as the authors also stated that the sustained release profile of Cu from the nanomaterial additionally contributed to the result for the metal's antifungal effect. ChsNPs have also been found to be a positive modulator of plant immune response by elevating the total phenolic content of plants. Chandra et al. observed that the increased enzyme activity and phenolic content came from increased gene expression of defence enzymes and compounds due to the ChsNP treatment.272
The fabrication of ChsNPs using chitosan and TPP is a common strategy for the encapsulation of agricultural plant ingredients such as plant growth regulators (PGRs) and biocides. PGRs are molecules that can alter plant hormonal homeostasis and signalling to enhance plant development, increase production, improve the visual and nutritional aspects of food, and increase shelf life.274 Pereira et al. used this method to encapsulate a well-known PGR, gibberellic acid (GA3), which can stimulate the synthesis of hydrolases to increase the availability of endosperm reserves for the embryo.275,276 They evaluated the effects of seed priming on tomatoes (Solanum lycopersicum) and found that the nanoALG/CS-GA3 formulation consisting of chitosan and alginate exhibited the best growth for plants cultivated under field conditions, improving fruit production almost 4-fold. The authors hypothesized that the ChsNPs formed a coating on the tomato seeds that maintained hydration and extended the period of release of GA3 after initial seed priming process. Plant uptake of the GA3-loaded ChsNPs continued to release GA3 within the plant tissues which increased the bioavailability of the PGR compared direct application of GA3.
Chauhan et al. investigated the fabrication of ChsNPs from chitosan and TPP to encapsulate hexaconazole [(R,S)-2-(2,4-dichlorophenyl)-1-(1H-1,2,4-triazole-1-yl)hexane-2-ol], a fungicide commonly used for controlling fungal pathogens that affect crops.277 Authors studied different concentrations of chitosan and TPP to produce fungicide-loaded ChsNPs and determined a relationship with the resulting ChsNPs size. Using response surface plot analysis, an optimal nanocapsule formulation was determined to be 100 nm nanocapsules with a 73% encapsulation efficiency at a chitosan concentration of 0.10% and a TPP concentration of 0.08%. As expected, release of hexaconazole from the nanocapsules was fastest in acidic soil due to the solubility of chitosan at lower pH. In comparison to a commercial hexacoanzole formulation which released its fungicidal payload in 5 days, the ChsNPs exhibited a far slower release of hexaconazole in 14 days. The efficacy of the nanocapsules were demonstrated against the soil-borne pathogen, R. solani. Maluin et al. also used TPP to formulate ChsNPs of different sizes to encapsulate the fungicides hexaconazole and dazomet against the G. boninense, a fungus that causes basal stem rot disease in oil palms.278 Similar to the work by Chauhan, as the concentration of TPP increased, the resulting size of the dual-loaded fungicidal ChsNPs also decreased. The smaller ChsNPs (5 nm) exhibited the highest antifungal efficacy against G. boninense, attributed to the higher surface area of the nanoparticles to interact with the fungal cell wall. The synergistic effect for the dual-loaded antifungal ChsNPs resulted in a 4-fold increase in antifungal activity, compared to single-loaded hexaconazole and dazomet ChsNPs.
ChNPs loaded with avermectin have been investigated as a means to control pinewood nematodes that cause the death of millions of pine trees from pine wilt disease.279 Current control measures to combat pine wilt disease include removal of infected trees, aerial application of insecticides, and direct trunk injection of anti-nematodal compounds such as avermectin. Unfortunately, the poor solubility of avermectin in water and its rapid photolysis results in poor bioavailability. This has led to its excessive application, contributing needlessly to environmental pollution. Liang et al. developed a nanocapsule (∼60 nm) consisting of anionic poly-γ-glutamic acid and cationic chitosan, crosslinked by TPP, with an encapsulation efficiency of 30.5% for avermectin.279 Interestingly, in contrast to ChsNPs fabricated from chitosan and TPP alone that breakdown under acidic conditions, these nanoparticles were more resilient under acidic pH which was attributed to the electrostic interaction of chitosan and poly-γ-glutamic acid. The encapsulation matrix was able to protect the avermectin from photolysis loss by 20%, while increasing the efficacy of the biocide from 69.9% in the free form to 98.6% while encapsulated.
Research has explored the direct effects of nanochitosan on food quality. The assessment of quality is usually completed microbiologically for bacterial and fungal count, physiochemically for pH and degree of oxidation, and sometimes with sensory evaluation for consumer consideration. Ramezani et al. investigated the coating effects of ChsNPs and chitosan on silver carp fish fillets. While both materials enhanced preservation of the fillets, ChsNP had lower antibacterial activity starting at day 9 of refrigerated storage.281 An overall indicator for spoilage in fish is the total volatile basic nitrogen value (TVB-N). Its value for ChsNP-treated samples was significantly lower than that of chitosan-treated samples on day 9 and 12 – implying that ChsNP may be a more appropriate coating for maximal shelf-life extension (Fig. 18). However, in terms of lipid oxidation, pH, and sensory evaluation, results showed that ChsNP and chitosan shared the same degree of preservative effect.
Fig. 18 TVB-N values changes measured at 3-day intervals. Different lower-case letters in the same day represent a statistically significant difference at P < 0.05. Adapted from ref. 281. |
ChsNP has also been coated onto cucumber,282 sprayed onto freshly-cut apple slices,283 incorporated into fish surimi,284 dispersed in ice for tilapia to be submerged in285 and all studies found similar results, where ChsNP had significant effects in delaying microbial, oxidative spoilage and retaining quality compared to control samples, measured by respective microbiological and physiochemical assessments. This effect is primarily due to the antimicrobial and antioxidant properties of ChsNPs.
Another rising technology involved in food preservation is loading antibacterial agents, most notably plant essential oils, onto ChsNPs for a controlled release, in an effort to create a more potent and sustained antimicrobial and antioxidative environment for the product.286 As an alternative to the traditional washing product for sanitation of chlorinated water (NaOCl) Martínez-Hernández et al. produced carvacrol-loaded ChsNPs and washed fresh-cut carrot slices with the solution.286 Carvacrol is a major component in the essential oils of several herbs. Its strong bactericidal action comes from how its phenolic compounds can interact with proteins of microorganisms, leading to their precipitation, cell content leakage, and cell lysis. Nanoencapsulation was achieved through first dissolving carvacrol in ethanol, then adding it dropwise into aqueous chitosan during homogenization, followed by TPP ionic gelation. This emulsified formulation was performed in hopes of improving the dispersibility, solubility, and stability of carvacrol in the aqueous system during application, as the compound is naturally aromatic and hydrophobic. The authors observed that the treatment of carvacrol loaded ChsNPs produced the best sensory and physicochemical qualities in carrot-specific parameters, as well as highly reducing the whitening effect and microbial levels, by 0.6–3.0 log units. The reduced whitening effect of carrots possibly comes from the inactivation of discoloration enzymes, induced by the antioxidant activity of carvacrol and chitosan. While the whitening is equally reduced in samples directly treated with carvacrol solution, this solution leads to more off-flavour and odours.
The release of carvacrol played an important role in the preservative effect of the carrots. Hosseini et al. concluded that the release profile of carvacrol in ChsNPs was biphasic. As carvacrol was adsorbed on the nanoparticle surfaces, the faster dissolution at the surface causes the compound to release in an initial burst followed by continuously slower release.287 For a more optimal extension of carrot shelf-life, the initial burst must be controlled for a slower, more gradual release. Additional research demonstrated that in a more acidic medium, the greater ionic repulsion between cationic amino groups on chitosan chains caused a greater dispersion, and thus longer release.288 The solution in which the carvacrol-loaded ChsNPs were fabricated was thus adjusted to a higher pH (pH = 4.3), allowing for a more optimal, efficient release of carvacrol and ensuing preservative effect.
Similar positive results for this nanoencapsulation technology of essential oils or other compounds in nanochitosan was observed in many different settings, including cinnamon–ChsNP in beef patties and on cucumber,289,290 rosemary essential oil in chitosan–benzoic acid nanogel in beef cutlet,291 nitric oxide–ChsNPs on sweet cherry fruits,292 and cumin seed essential oil–ChsNP on button mushrooms.293 All of these studies observed enhanced antibacterial and antioxidant activity, a reduction in microbial population and lipid oxidation, stability in colour and sensation, and shelf-life extension. Many studies have also compared using the essential oil in free form to an encapsulated from. In the case of cinnamon essential oil in beef patties, Ghaderi-Ghahfarokhi et al. observed that bacterial counts remained similar for all treatments, but started to significantly differ on day 8 of storage.289 The 0.1% encapsulated cinnamon essential oil sample had the highest log decrease in S. aureus counts, compared to its 0.05% encapsulated oil sample and unencapsulated counterparts. The inhibitory effect for fungal growth, lipid oxidation, and discolouration was also the most notable in the 0.1% encapsulated sample, mostly for its sustained release. Ultimately, this natural and novel additive seemed to provide a promising delivery system that served to effectively preserve many types of food products.
Specific parameters become crucial in food packaging for its function in food preservation, most notably water-vapor permeability, film tensile strength, light absorption, and thermal degradation. The incorporation of nanomaterials has been found to improve these film properties, and also play an active role in food preservation in the case of nanochitin or nanochitosan. Ifuku et al. explored the effects of reinforcing chitosan-based high-strength transparent films with surface-deacetylated ChNFs.163 With only a 10% blending of the ChNFs, the group observed significant improvements in light transparency and tensile strength, and significant reductions in thermal expansion (Fig. 19). Increasing the content of ChNF was also found to increase the chitosan film's tensile strength. It was hypothesized that the strong extended crystalline structure of the chitin core, along with the slow drying process, lead to the formation of hydrogen bonds between the ChNFs resulting in good mechanical properties of the films. Ultimately, the results show that ChNFs act as an effective filler for novel, biodegradable films that often lack strong properties needed for food packaging. In a study by Satam et al., films with ChNF and CNC blends were found to be mechanically stronger than both neat cellulose and chitin films, as the blending of two materials led to aggregation which supported the fibrous networks.161 Similar results of reinforcement were observed with ChsNPs as nanofillers for sago starch film.296 Due to changes in chemical structure, the nanocomposite film brought significant increases in its mechanical properties including tensile strength, Young's modulus, and elongation at break. This was postulated to be mostly due to the proper dispersion of the nanofillers throughout the film, yielding a strong and reliant film. Thermogravimetric analysis also demonstrated the film to be capable of sustaining heat-sealing applications. Many other studies also showed strengthening effects of ChsNPs on various films, and some even had an enhanced antimicrobial effect.103,297
Fig. 19 Changes in (a) light transmittance (b) thermal expansion (c) tensile strength with increasing incorporation of chitin nanofibers in chitosan film. Adapted from ref. 163. |
Water-vapor permeability is another property important to applications of food packaging. Often measured by water-vapor diffusion coefficient (WVDC), the incorporation of ChsNPs showed a decrease in WVDC when incorporated in a variety of potential packaging materials, including chitosan/montmorillonite films,298 propolis–ChsNP films,299 and banana puree films.103 This is speculated to be due to the increased compacting of the film as the ChsNPs fill the empty spaces in the porous film matrix, making it less likely for water to permeate and thus enhancing its barrier properties.103,299,300 On the other hand, Bao et al. observed that the addition of ChsNPs increased the water vapor permeability in gelatin films.301 However, the gelatin film is a protein-based film, while the previously mentioned are all polysaccharide-based films. The group postulated that protein–protein crosslinks became further away from each other due to the dispersion of large nanoparticles in the network, causing penetration of water to be easier.
Azarifar et al. studied the shelf-life characteristics of refrigerated raw beef using gelatin–CMC films incorporated with ChNFs.302 By sealing beef fillet cubes with this active composite film, the samples were shown to inhibit psychotropic bacteria throughout 15 days of storage, delaying lipid oxidation and protein decomposition, and overall prolonging the shelf life of the beef. This is a result of the reduced oxygen permeability of the film. There are many proposed mechanisms for this reduced oxygen permeability, such as the formation of amide and hydrogen bonds between ChNFs and gelatin chains to increase cohesiveness, and the more tortuous film matrix, reducing the speed of oxygen travel through the film. Ultimately, chitin-based nanomaterials have shown to effectively improve film properties, a key feature for the production of more sustainable alternatives to plastic food packaging.
Guo et al. have also explored the fate of chitin-based nanomaterials in the gastrointestinal tract.305 The authors assessed the transformations that ChsNPs go through in the GI tract through a simulated digestion and found that while bulk chitosan dissolves in weakly acidic environment and during digestion, TPP-crosslinked ChsNPs do not. These results imply that ChsNPs remain stable from strongly to weakly acidic solutions, indicating that they would be suitable for drug delivery. The group observed that the surface zeta potential of the ChsNPs went from positive to negative when moving from the gastric to the small intestinal phase. This would be important to consider for certain applications, as the positive surface charge is often what provides the material with cell-adhesive properties. In fact, using ChsNPs, Diop et al. managed to increase bioefficiency of insulin by oral administration.306 Insulin is often destroyed by enzymes and the harsh environment of digestion and therefore cannot be taken orally. By freeze drying insulin-loaded ChsNPs for stabilization, followed by cross-linking with TPP to increase bioefficiency, the procedure appeared to effectively protect insulin and reduce glycemia in insulinopenic rats.307 This nanoencapsulation technique using chitosan-based nanomaterials has also shown to successfully improved bioavailability of bioactive food components, including carotenoids, vitamins, and essential oils - as reviewed by Akbari-Alavijeh et al.308
Fig. 20 Scanning electron microscopy (SEM) analysis of S. aureus on nanofibrous membranes at low (top row) and high (bottom row) magnifications. (a and e) PCL only, (b and f) 25% chitosan, (c and g) 50% chitosan and (d and h) 75% chitosan. The samples were fixed after 24 h of culture with an initial bacteria density of 5 × 104 cells per mL in tryptic soy broth medium. Scale bars represent 5 μm (top row) and 2.5 μm (bottom row). Note the excessive fiber swelling in h. Adapted from ref. 310. |
ChsNFs have been used to bind many heavy metals, such as Cr(VI),312,313 Cu(II) and Pb(II).314 For instance, Desai et al. observed Cr(VI) binding capacities of up to 35 mg chromium per g chitosan and 2–3 log reduction in E. coli count.309 Furthermore, Haider and Park examined the metal adsorption of electrospun ChsNF.314 Mono-layer adsorption was observed on the nanofiber mats, as there was good erosion stability and high affinity for adsorbing metal ions in aqueous solutions. It was also observed that Cu(II) adsorption with ChsNFs is six times higher than that of chitosan microspheres, and 11 times higher than bulk chitosan, implying that size is another crucial factor responsible for the high adsorption capacity of the material. Desai et al. also related the physical filtration efficiency, antimicrobial properties, and metal binding capabilities to the surface chitosan content of the nanofiber mats.309 Moreover, as Makaremi et al. used polyacrylonitrile (PAN) nanofibers for water filtration, they found that an additional layer of electrospun chitosan membrane increased tensile strength and elasticity modulus, while significantly improving heavy metal adsorption, bacteria filtration, and antibacterial action.315 Bai also explored filtration of porcine parvovirus, a water-borne virus causing diarrhoeal disease, by functionalizing the nanofibers to form chitosan chloride and blending the electrospinning solution with graphene.316 This modification increased the removal of the virus to a minimum of 99% in solution. In addition to water filtration, electronspun ChsNFs have also been explored to be effective at air filtration.317
Reaction | Catalyst | Rate constant, k, s−1 | Turnover frequency, h−1 | Ref. |
---|---|---|---|---|
Reduction of congo red | Ag NPs supported on ChNCs | 50.2 × 10−3 | — | 329 |
Reduction of 4-nitrophenol | Au NPs supported on ChsNCs | 4.75 × 10−3 | 8557 | 39 |
Aldehyde–amine–alkyne coupling | Au NPs supported on ChsNCs | — | 8.3 | 39 |
Heck coupling | Pd NPs supported on ChNCs | — | 4.2 | 331 |
Knoevenagel condensation | ChNF aerogel | — | 22 | 330 |
Yang et al. used ChNCs as a support for Ag NPs as a catalyst for environmental waste removal, using the reduction of congo red as a model reaction (Scheme 5).329 Sodium lignosulfonate (NaLS) was combined with ChNCs and AgNO3 to produce Ag NPs with a diameter of 15 ± 5 nm, upon NaBH4 reduction. The authors further showed a good rate constant for the congo red reaction at 50.2 × 10−3 s−1, while also maintaining catalytic efficiency of up to 90% even after 5 reaction cycles.
We recently reported the use of carboxylated ChsNCs as a versatile catalyst support for Au catalysis (Scheme 6).39 By using the catalytic reduction of 4-nitrophenol as a model reaction, it was demonstrated that Au supported on ChsNCs had better catalytic activity than ChNCs, proving the effectiveness of the amine functionality in stabilizing highly disperse metal NP catalysts. Further comparisons with Au supported on bulk chitin and chitosan also proved that the nanoscale nature of ChsNCs were crucial in yielding high surface area for metal NPs to deposit onto. Interestingly, by comparing with other literature values for the same reaction, ChsNCs were the most effective catalyst support for Au, outperforming all other carbon-based supports including CNCs.
Scheme 6 Catalytic reduction of 4-nitrophenol and multicomponent A3 coupling reaction catalysed by Au supported on ChsNC. |
Nanochitin itself has also been used as a base catalyst for the aqueous Knoevenagel condensation reaction, as reported by Isogai and coworkers in 2014 (Scheme 7). A flow system was implemented with ChNF-based hydrogel and aerogels, showing exceptional turnover frequencies of 22 h−1 at a flow rate between 0.03–0.04 mL min−1. Importantly, control tests using aerogels made with cellulose showed virtually no product yield, highlighting the importance of the amine units on the ChNFs. Aerogels made from bulk chitosan were also tested to yield no product, further indicating the importance of the increased surface area from making aerogels from ChNFs.330
Recently, our group has also used ChNCs as a support for PdNPs to catalyse the Heck coupling reaction (Scheme 8). Full product yield was observed after 24 h and 90 °C.331
The immobilization of enzymes is a large field under development to promote the sustainable usage of costly enzymes, ensure easy separation from products (akin to heterogeneous catalysis), and prevent deactivation in the presence of deviations from the ideal condition such as pH, temperature, and reaction media.332 ChNCs have been shown to effectively immobilize enzymes for biocatalysis. For instance, Cao et al. immobilized porcine pancrease lipase (PPL) onto ChNC using a crosslinking procedure with glutaraldehyde.82 In a model reaction, the reduction of N-α-benzoyl-D,L-arginine-pnitroanilide to 4-nitroaniline (Scheme 9) showed that ChNC prevented deactivation of the PPL enzyme when subjected to changes in pH and temperature, as compared to free PPL.
Similarly, a chitosan/poly(vinyl alcohol) nanofibrous membrane was prepared by Huang et al. for the immobilization of lipase from Candida rugosa.333 The activity after use, pH, and thermal stability were all improved compared to free enzymes. Other enzymes that have been immobilized on electrospun ChsNFs include trypsin and acetylcholinesterase, with trypsin showing long-term activity and recyclability for the reduction of N-α-benzoyl-D,L-arginine-pnitroanilide (Scheme 9) compared to free enzyme.334,335 Park et al. also immobilized lysozyme on electrospun, stabilized chitosan/poly(vinyl alcohol) nanofibrous membranes as it was shown to be effective for continuous antibacterial function.336 While free lysozymes lost all activity after 80 days of room temperature storage, 75.4% of initial activity was retained in the immobilized lysozymes, all while having bacteriostatic properties.
With these few notable examples, it is apparent that there is a huge gap within the literature to expand upon the use of nanoscale chitin and chitosan as metal catalyst supports compared to CNCs or as an organocatalyst themselves. One important aspect to consider is the wide variety of functionalization that can be done via the acetamide or amine on chitin and chitosan, respectively. While this has been done with bulk chitin and chitosan, it will be of notable interest to understand how manipulating these nitrogen handles on the nanoscale can drastically alter their properties, as it has been seen within the cellulose literature. Important properties of chitin and chitosan to augment include, but are not limited to, metal binding, solubility, thermal and mechanical durability, and catalytic effectiveness (e.g., by hydrophobic moieties to boost interaction of reacting substrates). A litany of reactions may be used to accomplish this including reductive amination, Schiff base formation, thiolation, among many others that can introduce a variety of unique ligands, which have already been done with bulk chitosan.328 With this in mind, it is hopeful that this field will offer both the promising advantages of heterogeneity in using a catalyst support, along with green chemistry principles such as sustainability and waste valorisation in making the next generation of catalytic materials.
The functional properties of nanochitin and nanochitosan may provide these materials the opportunity to supercede nanocellulose. As physical reinforcing agents, the additional nitrogen-bearing groups on nanochitin and nanochitosan are able to contribute to additional electrostatic or chemical crosslinking interactions. We anticipate that nanochitin and nanochitosan will specifically benefit from this increase reactivity imparted by the nitrogen-bearing groups in areas such as wound healing, tissue adhesion, drug delivery, drug encapsulation, and environmental remediation. We anticipate with more refined processing, nanochitosan (specifically ChsNCs and ChsNFs) can have a greater role in food packaging and biomedicine, due to its natural antimicrobial characteristics. Furthermore, the area of organocatalysis also has huge potential for development, as nanochitosan features high surface area characteristics along with amine groups that can be used as a Lewis base, or participate in the formation of imine- and enamine-type organocatalytic reactions. In such a small period of time, the literature has shown a wealth of initial applications using nanochitin and nanochitosan materials, reminiscent of the surge in publications associated with nanocellulose. We anticipate that future research will not only advance some of these identified application areas, but begin to address the core challenges related to economics and sustainability, key factors to commercial viability for nanochitin and nanochitosan.
This journal is © The Royal Society of Chemistry 2021 |