aState Key Laboratory of Radio Frequency Heterogeneous Integration (Shenzhen University); College of Physics and Optoelectronic Engineering, Key Laboratory of Optoelectronic Devices and Systems of Ministry of Education and Guangdong Province, Shenzhen University, Shenzhen 518060, P. R. China. E-mail: songjun@szu.edu.cn
bMedical Engineering and Technology College, Xinjiang Medical University, Urumqi 830011, P. R. China. E-mail: jlqu@szu.edu.cn
First published on 21st October 2024
Lead halide perovskite nanowires (NWs) have garnered increasing attention owing to their unique properties, including axial carrier transportation, low pumping thresholds, and polarized emission. However, their intrinsic instability significantly limits their applications. In this study, heterostructured CsPbBr3/PbSe NWs with a diameter of 10 nm and lengths ranging from several to tens of microns were successfully synthesized via a one-pot solution-phase process. Photoluminescence measurements revealed that the CsPbBr3/PbSe NWs emitted green fluorescence with a narrow width of 16 nm and a high photoluminescence quantum yield (PLQY) of 37.6%. The obtained CsPbBr3/PbSe NWs underwent anion exchange with I− ion precursors to transform into CsPbBr3−xIx/PbSe, but not with Cl− ion precursors. Remarkably, these heterostructured CsPbBr3/PbSe NWs remained stable when immersed in water or exposed to air for several months, demonstrating excellent humidity stability. This study offers an effective approach for preparing stable CsPbBr3 NWs and fosters their future applications in optoelectronic devices.
Numerous studies have been conducted in the past decade to enhance the stability of perovskite NCs. For instance, all-inorganic perovskite QDs (CsPbX3) have been extensively explored. Common strategies for enhancing the stability of CsPbX3 QDs involve their encapsulation within a hydrophobic matrix or coating with protective shells, isolating them from the surrounding environment.16,17 More recently, a variety of heterostructured CsPbX3 QDs have been developed, significantly improving their stability.18–20 These heterostructured CsPbX3 QDs are typically synthesized using straightforward methods. For instance, Zhang et al. employed an effective sol–gel process to prepare CsPbX3-based heterostructures with ZrO2 or SiO2.21,22 Wang et al. sulfureted the surface of CsPbX3 QDs with hexamethyldisilathiane at room temperature to produce heterostructured CsPbX3–PbS (X = Cl, Br, I) QDs.23 Manna et al. reported a simple hot-injection method for fabricating CsPbX3–Pb4S3Br2 QDs heterostructures.24
These successful strategies for fabricating CsPbX3 QDs can also enhance the stability of CsPbX3 NWs. However, relatively few related studies have been conducted to date. Core–shell CsPbBr3/MoO3 NWs were synthesized by a vapor–liquid–solid (VLS) process.25 The MoO3 shell effectively passivated the surface of the CsPbBr3 NW cores, thereby reducing the diffusion of harmful water and oxygen molecules and enhancing air stability. Additionally, core–shell PbSe@CsPbBr3 wire heterostructures were prepared through conformal epitaxy of a CsPbBr3 shell on a PbSe wire core using chemical vapor deposition (CVD).26 Compared to the VLS and CVD processes, the solution-phase process is simpler, more economical, and widely used for preparing perovskite NWs. Here, we propose a one-pot strategy for synthesizing heterostructured CsPbBr3/PbSe NWs using a solution-phase process. The resulting CsPbBr3/PbSe NWs had a diameter of approximately 10 nm and lengths ranging from several to tens of microns. They remained stable even after immersion in water or exposure to air for several months, exhibiting excellent humidity stability.
The formation mechanism of CsPbBr3/PbSe NWs was investigated initially. Samples were quenched at various stages during the preparation process, and their morphologies and absorption spectra were analyzed (see Fig. 1 and S5, and Table S2†). During the heating stage from room temperature to 160 °C (Fig. 1a–e), the products exhibited diverse morphologies at different temperatures. Products quenched at 80 °C (Fig. 1a) displayed complex morphologies and non-uniform sizes, with many nanocrystals smaller than 5 nm, resulting in weak cyan fluorescence (Fig. S5a†). When the reaction temperature was increased to 100 °C (Fig. 1b), the products predominantly consisted of hexagonal nanocrystals with uniform sizes and irregularly shaped nanosheets. Analysis of the absorption spectrum (Fig. S5b†) showed a characteristic peak centered at 311 nm, suggesting that the hexagonal nanocrystals were Cs4PbBr6. Further raising the temperature to 120 °C (Fig. 1c) led to the nanosheets becoming regular squares with widths of approximately 40 nm, resulting in a change in the emission color of the products to green. Additionally, hexagonal Cs4PbBr6 nanocrystals were present. NWs several hundred nanometers in length were initially observed in products quenched at 140 °C (Fig. 1d), with their lengths increasing as the temperature was raised to 160 °C (Fig. 1e). During the heat-holding stage at 160 °C (Fig. 1f), more NWs nucleated and grew, while the hexagonal nanocrystals and square nanosheets disappeared over time. However, the NWs gradually transformed into larger crystals as the time increased beyond 20 min (Fig. 1g–i). Consequently, intermediates with various morphologies were obtained and gradually transformed under the given conditions during the formation of CsPbBr3/PbSe NWs. The formation mechanism of CsPbBr3/PbSe NWs closely resembled that of pure CsPbBr3 NWs reported by Yang et al., wherein the NWs were nucleated and grown through a surfactant-directed 1D mode, rather than by the oriented attachment of NCs or seed-mediated anisotropic growth.28 Notably, CsPbBr3/PbSe NWs were formed within 20 min, considerably faster than the time required for pure CsPbBr3 NWs (90 min).
The microstructure of the colloidal CsPbBr3/PbSe NWs was characterized using X-ray diffraction (XRD). The XRD pattern in Fig. 2a indicates that the synthesized NW samples exclusively comprised the CsPbBr3 and PbSe phases. As is known, CsPbBr3 exhibits three different phases, namely cubic, tetragonal, and orthorhombic, with phase transitions occurring at 130 °C from cubic to tetragonal and at 88 °C from tetragonal to orthorhombic.29 The distinct double peaks at approximately 30° corresponding to the (002) and (200) lattice planes (JCPDS 18-0364) confirmed the orthorhombic CsPbBr3 phase in the CsPbBr3/PbSe NWs. Additionally, diffraction peaks at 25.1° and 28.5° corresponded to the (111) and (200) lattice planes, respectively, of the cubic PbSe phase (JCPDS 06-0354), indicating the presence of the PbSe phase. The morphologies of the CsPbBr3/PbSe NWs were examined using transmission electron microscopy (TEM) (Fig. 2b and c). The synthesized CsPbBr3/PbSe NWs formed bundles, with each bundle consisting of separate NWs with a uniform size of approximately 10 nm. The CsPbBr3/PbSe NWs ranged from several microns to tens of microns in length. The high-resolution high-angle annular dark-field scanning TEM (HAADF-STEM) image in Fig. 2d depicted single crystal CsPbBr3/PbSe NWs in the [100] direction, with an interplanar distance of ∼0.58 nm corresponding to the (100) plane of CsPbBr3. Furthermore, tiny PbSe nanoparticles (1–3 nm in size) were embedded in the CsPbBr3 matrix. The XPS spectrum (Fig. S6†) also confirmed the coexistence of Cs+, Pb2+, Br−, and the peak at 59.2 eV in the XPS spectrum was assigned to the Se 3d signals of Se2−, indicating that Se2− had been incorporated into the NWs. EDS analysis (Fig. S7†) further confirmed the coexistence of Cs, Pb, Br, and Se in the CsPbBr3/PbSe NWs. Another experiment involved reacting the PbBr2 precursor solution solely with the Se precursor solution at 160 °C for 5 min, resulting in cubic PbSe nanoparticles with sizes in the range of 5–10 nm (Fig. S8†). This experiment confirmed the formation of PbSe nanoparticles under the reaction conditions used to prepare the CsPbBr3/PbSe NWs. Combined with the aforementioned formation mechanism, it can be inferred that the nucleation and growth of CsPbBr3/PbSe NWs occurred. In the early stages, CsPbBr3 and PbSe seeds formed simultaneously. The number of CsPbBr3 seeds was considerably higher than that of PbSe seeds due to the higher Br concentration compared to the Se concentration in the precursor solution. During the growth process of the NWs, the PbSe seeds grew into PbSe NCs and were gradually surrounded by growing CsPbBr3 seeds, forming CsPbBr3/PbSe heterostructures. These heterostructures inhibited the growth of PbSe NCs, resulting in a smaller size of the PbSe NCs in the CsPbBr3/PbSe NWs than in the PbSe NCs (Fig. S8†).
![]() | ||
Fig. 2 Structural characterization of colloidal CsPbBr3/PbSe NWs: (a) XRD pattern, (b–c) TEM images, and (d) HAADF-STEM image. |
The optical properties of the synthesized CsPbBr3/PbSe NWs were characterized (Fig. 3). The absorption spectrum of CsPbBr3/PbSe NWs (Fig. 3a) revealed an absorption peak at 510 nm. In contrast to the sharp edges of pure CsPbBr3 QDs or NWs, an absorption tail in the long-wavelength direction was observed for CsPbBr3/PbSe NWs, attributed to the growth of PbSe nanoparticles within the CsPbBr3/PbSe NWs. The photoluminescence (PL) spectrum of CsPbBr3/PbSe NWs displayed a single narrow emission peak at 516 nm with a width of 16 nm, similar to that of CsPbBr3 QDs. The PL quantum yield of the CsPbBr3/PbSe NWs was measured at 37.6% (Fig. 3b), which closely approximates the value reported for pure 10.0 nm thick CsPbBr3 NWs (∼38%) by Manna et al.30 Time-resolved PL measurements of the CsPbBr3/PbSe NWs (Fig. 3c) revealed bi-exponential decay traces, with an average lifetime of only 6.88 ns, 42% lower than that of pure 10.0 nm thick CsPbBr3 NWs (16.4 ns).30 To further investigate the optical properties, the CsPbBr3/PbSe NWs were deposited onto a glass slide and imaged using confocal microscopy under excitation by a 488 nm continuous-wave laser (Fig. 3d–f). The 10 nm thick CsPbBr3/PbSe NWs were sufficiently long to be observed in bright field, with strong fluorescent signals detected in the fluorescence field. The merged images in Fig. 3d and e indicate fluorescence emitted by the CsPbBr3/PbSe NWs.
In prior studies,31 anion exchange was utilized to adjust the emission band of halide perovskite nanocrystals. Similarly, the emission band of the synthesized CsPbBr3/PbSe NWs could be tuned via anion exchange. Fig. 4 illustrates the emission color changing from green to yellow to dark red as I− precursors were gradually introduced into the dispersion of CsPbBr3/PbSe NWs in hexane, providing a series of tunable PL signals from 516 to 660 nm with a narrow band (FWHM in the range of 15–40 nm). Anion exchange of CsPbBr3/PbSe NWs with I− ions occurred rapidly at room temperature, whereas exchange with Cl− ions was hindered. The emission color remained unchanged when Cl− precursors were added to the dispersion of CsPbBr3/PbSe NWs at room temperature (Fig. S9†). Similarly, the emission color of the CsPbBr3 QD dispersion quickly shifted from green to blue. This unusual phenomenon may be linked to internal strain within the CsPbBr3/PbSe NWs. Incorporation of PbSe nanoparticles into the CsPbBr3 matrix resulted in a 4.8% lattice mismatch, producing internal strain. Gradual release of this strain occurred upon anion exchange with I− ions due to a decreased mismatch (2.9%) with CsPbI3, making the reaction easily achievable. Conversely, the 8.8% lattice mismatch between PbSe and the CsPbCl3 lattice generated strong internal strain, hindering the anion exchange of CsPbBr3/PbSe NWs with Cl− ions.
The integration of PbSe nanoparticles into the CsPbBr3 NWs significantly enhanced their humidity stability. Fig. 5 illustrates the stability of two CsPbBr3/PbSe NW samples. The sample labeled “in air” consisted of a CsPbBr3/PbSe NW film coated on a glass slide and exposed to air, whereas the other sample labeled “in water” comprised centrifuged CsPbBr3/PbSe NW powders immersed in a tube filled with deionized water. The CsPbBr3/PbSe NWs demonstrated robust stability in both air and water (Fig. 5a). The PL intensity of the CsPbBr3/PbSe NW film exposed to air retained approximately 95% of its original intensity after 30 days, while the fluorescence intensity of the CsPbBr3/PbSe NW film powders immersed in deionized water retained approximately 80% of its original PL intensity after the same duration. Fig. 5b presents photographs of the two CsPbBr3/PbSe NW samples under excitation by 365 nm lamps. The CsPbBr3/PbSe NW sample retained its original shape when exposed to air or immersed in water for 30 days, exhibiting strong green fluorescence under the 365 nm lamp. Notably, the PL of perovskite nanocrystals is typically completely quenched within several hours of immersion in water. The results depicted in Fig. 5 indicate the excellent humidity stability of the CsPbBr3/PbSe NWs. In previous research, core–shell CsPbBr3/MoO3 NWs have been developed to enhance the stability of CsPbBr3 NWs.25 The mobility of the CsPbBr3/MnO3 NWs was maintained at 80% after 7 days’ storage at 65% relative humidity. Another strategy to enhance the stability of CsPbBr3 NWs was to passivate their surfaces with thiourea. The passivated CsPbBr3 NWs retained approximately 80% of their original performance after 2 hours of water treatment.32 Comparatively, the CsPbBr3/PbSe NWs in this work demonstrated superior stability. However, a direct comparison of the stability between CsPbBr3/PbSe NWs and pure CsPbBr3 NWs is not feasible due to the current process's inability to produce pure CsPbBr3 NWs. To shed light on this, we refer to CsPbX3 QDs. Previous studies have highlighted that the stability of CsPbX3 QDs can be enhanced by incorporating metal chalcogenides such as ZnS,33 PbS,34 and PbTe.35 Density functional theory (DFT) calculations36 have revealed that the augmented stability of CsPbX3 QDs primarily stems from the strong interaction and high binding energy at the interface between the perovskite and the metal chalcogenide. Additionally, in the CsPbBr3 NWs passivated by thiourea,32 the enhanced stability was attributed to the surface passivation effect of thiourea, which forms a relatively stable Pb2+–thiourea complex with Pb2+. In the CsPbBr3/PbSe NWs, the incorporation of PbSe nanoparticles into the CsPbBr3 matrix led to the formation of a stable complex and high binding energy at the interface, thus improving the stability of the CsPbBr3 NWs.
Footnote |
† Electronic supplementary information (ESI) available. See DOI: https://doi.org/10.1039/d4nr03554b |
This journal is © The Royal Society of Chemistry 2024 |