Nayab Arif,
Ye-Zhan Lin,
Kai Wang,
Yi-Chuan Dou,
Yu Zhang,
Kui Li*,
Shiquan Liu* and
Fu-Tian Liu
School of Materials Science and Engineering, University of Jinan, Jinan 250022, China. E-mail: mse_lik@ujn.edu.cn; vctrliu@hotmail.com
First published on 1st March 2021
Bimetallic zeolite-imidazole frameworks with controllable flat band position, band gap and hydrogen evolution reaction characteristics were adopted as a photocatalytic hydrogen production catalyst. Furthermore, the g-C3N4–MoS2 2D–2D surface heterostructure was introduced to the ZnM-ZIF to facilitate the separation as well as utilization efficiency of the photo-exited charge carriers in the ZnM-ZIFs. On the other hand, the ZnM-ZIFs not only inhibited the aggregation of the g-C3N4–MoS2 heterostructure, but also improved the separation and transport efficiency of charge carriers in g-C3N4–MoS2. Consequently, the optimal g-C3N4–MoS2–ZnNi-ZIF exhibited an extraordinary photocatalytic hydrogen evolution activity 214.4, 37.5, and 3.7 times larger than that of the pristine g-C3N4, g-C3N4–ZnNi-ZIF and g-C3N4–MoS2, respectively, and exhibited a H2-evolution performance of 77.8 μmol h−1 g−1 under UV-Vis light irradiation coupled with oxidation of H2O into H2O2. This work will furnish a new MOF candidate for photocatalysis and provide insight into better utilization of porous MOF-based heterostructures for hydrogen production from pure water.
As one of the most stable metal organic frameworks in neutral and alkaline solutions,26,32,33 Zeolite Imidazole Frameworks (ZIFs) and its heterostructure has been extensively studied for the photocatalytic reaction.33,34 Especially, the bimetallic ZIFs has been widely investigated because it possesses various structures, has versatile functions and its photo-electric properties. Moreover, the bimetallic ZIF derived nanomaterials have been fabricated and used in the electrocatalytic energy conversion and storage.25,32,34–36 However, the bimetallic ZIFs itself with special merits for photocatalysis was rarely reported as photocatalyst, although this is a stirring work, and will bring out some new interesting prospects. Moreover, almost all the MOFs photocatalysts suffered from the problems of limited photocatalytic hydrogen production activity and poor photocatalytic stability even in sacrificial agent solution owing to the low photo-response, rapid recombination of photo-exited electron–hole pairs. Construction of ZIFs-based heterostructure not only resolved the problems of low porosity of semiconductors, but also improved the separation and utilization of the photo-generated charge carriers.
Graphic carbon nitride (g-C3N4), which is composed of the earth abundant carbon and nitrogen atoms through strong covalent bonds, possesses enhanced stability in solutions over a wide pH range, and suitable for the visible light absorption.37–40 The separation and utilization efficiency of the photo-generated charge carriers in g-C3N4 is very limited, resulting in poor photocatalytic activity.9,23,41 Consequently, a large number of cocatalysts were fabricated, and one of the most extensively investigated cocatalyst is MoS2.9,42–45 Due to the different work function of MoS2 compared with the semiconductor components, and its low hydrogen evolution reaction (HER) overpotential, the photo-exited electrons and holes in g-C3N4–MoS2 2D–2D surface heterostructure could be transformed into different semiconductor components with high utilization efficiency. Therefore g-C3N4–MoS2 heterostructure was adopted to incorporate on ZIFs-based heterostructure that not only resolved the problems of low porosity, but also improved the separation and utilization of the photo-generated charge carriers between g-C3N4–MoS2–ZnM-ZIF. Simultaneously, ZnM-ZIF could restrain the agglomeration of g-C3N4–MoS2 during the subsequent post annealing and photocatalytic reactions.9,46,47 However, during the fabrication process and/or the photocatalytic reaction, the g-C3N4–MoS2 nanosheet may aggregate occur and thus deteriorate its photocatalytic hydrogen production activity.34,48 Moreover, the photocatalytic hydrogen evolution in pure water for g-C3N4–MoS2 and especially MOFs photocatalyst is important and it also faces huge challenges.49
Herein, bimetallic ZIFs (ZnM-ZIF, M = Co, Ni) with controllable band were synthesized and adopted as the photocatalytic hydrogen production catalyst with a considerable photocatalytic HER activity. The g-C3N4–MoS2 nanorods were prepared by one-step hydrothermal method. Further the g-C3N4–MoS2–ZnM-ZIFs (M = Co, Ni) were prepared using the similar method with g-C3N4–MoS2 as precursor. The introduction of g-C3N4–MoS2 onto the surface of the ZnM-ZIF not only improved the utilization efficiency of photo-exited charge carriers by MoS2, but also inhibited the accumulation of g-C3N4–MoS2 heterostructure. Hence, the optimal g-C3N4–MoS2–ZnNi-ZIF (CNMZN) exhibited the extraordinary photocatalytic HER activity of 30.1 μmol h−1, being 214.4, 37.5, and 3.7 times larger than that of the pristine g-C3N4 (CN), g-C3N4–ZnNi-ZIF (CNZN) and g-C3N4–MoS2 (CNM), respectively. More importantly, even in pure water, the optimal ternary heterostructures exhibited considerable hydrogen production rate. This work provided innovation that can hopefully help in designing a novel high-performance MOF-based heterostructure photocatalyst for solar conversion.
Transmission electron microscopy (TEM) was employed for investigating the morphology of the g-C3N4 embedded with ZnM-ZIF and/or MoS2. The dense nanosheet morphology of pristine g-C3N4 could be observed in Fig. 1d, and compared with ZIF-8 and ZnNi-ZIFs, the as-prepared ZnNi-ZIF exhibited regular truncated rhombic dodecahedron structure as confirmed by the TEM and scanning electron microscope (SEM) images (Fig. 1e and S3a–c†). For the CNZN, the microstructure of g-C3N4 nanosheet enwrapped MOF blocks is clearly observable, proved the formation of CNZN surface heterostructure (Fig. 1f), which was further confirmed by the SEM images of g-C3N4–ZnM-ZIFs as depicted in Fig. S3d–f.† The CNM was a 2D–2D surface heterostructure (Fig. 1g) as reported in the previous publication.50 Notably, the CNM nanosheet was distributed uniformly over the surface of ZnNi-ZIF as demonstrated in Fig. 1h, and the (002) lattice plane of MoS2 could be clearly observed from CNMZN (Fig. 1i), which has an enlarged interlayer spacing (0.95 nm). Moreover, the g-C3N4–MoS2–ZnM-ZIFs exhibited similar morphology on SEM images (Fig. S3g–i†). Further adopted the elemental mapping to investigate the distribution of different components in the ternary CNMZN (Fig. S4†). The result confirmed that all the C, N, Zn, Ni, S and Mo uniformly dispersed. Further verifying both the MoS2 and g-C3N4 distributed evenly on the skeleton of ZnNi-ZIF.
The visible light absorption and the bandgap of the as-prepared g-C3N4-based heterostructures were investigated via the UV-Vis diffuse absorption spectra (Fig. 2a). After embedding ZnM-ZIFs, the absorption of the g-C3N4 in the visible light region has a little enhancement (Fig. S5†), while for the g-C3N4–MoS2, the absorption rate is significantly improved (Fig. S6†). It is worth noting that the co-loading of the MoS2 and ZnM-ZIF exhibited a synergistic effect for the absorption of visible light, and the absorption intensity in the visible light region was in the order of CNMZC > CNMZN > ZNMZ. The bandgaps of g-C3N4 and MoS2 calculated according to the Kubelka–Munk (KM) method are 2.74 and 1.67 eV (Fig. 2b).52,53 As displayed in Fig. 2c, simultaneous doping of Co and Ni could increase the visible light absorption capacity of ZIF-8, as further confirmed by the bandgaps for ZIF-8, ZnCo-ZIF and ZnNi-ZIF of 5.1, 2.3 and 2.0, respectively (Fig. 2d). To determine the band structure matching and charge separation mechanism among g-C3N4, MoS2, and ZnM-ZIFs, the Mott–Schottky plot measurements were used to investigate the flat band potential of them. As shown in Fig. 2e, the ZIF-8, ZnCo-ZIF, and ZnNi-ZIF exhibited flat-band potentials of −0.89, −1.24 and −1.28 V vs. Ag/AgCl, respectively, which were lower than that of the pristine g-C3N4 (−1.46 V), while higher than that of MoS2 (−0.19 V). Therefore, the band structure matching in the ternary g-C3N4–MoS2–ZnNi-ZIF heterostructure could be inferred in Fig. 2f. This band structure indicated the transfer of photo-generated electron from the conduction band (CB) of g-C3N4 and ZnNi-ZIFs to that of MoS2. On the other hand, the holes were transferred into the valence band (VB) of ZnNi-ZIF, where the H2O2 was preferentially formed efficiently owing to the highly porous morphology of ZnNi-ZIF. The band structure matching of the g-C3N4–ZnNi–MoS2 not only facilitated the separation and utilization efficiency, but also improved the visible light absorption between g-C3N4, ZnNi-ZIF and MoS2.
Notably, in sharply contrast to the negligible photocatalytic hydrogen production activity of ZIF-8 because of its large bandgap (5.1 eV), the bare bimetallic ZnM-ZIFs exhibited sizable increase in hydrogen evolution activity as displayed in Fig. 3a. The optimal photocatalytic HER performance occurs in the Zn0.5Ni0.5-ZIF, achieved 0.92 μmol h−1 under UV-Vis light irradiation, which could be comparable to that of g-C3N4 (0.71 μmol h−1). Moreover, the photocatalytic HER performance of Zn0.5Co0.5-ZIF slightly lower than that of the g-C3N4, which was 0.51 μmol h−1, which. The photocatalytic HER performance of the CNZN with different weight ratio of ZnNi-ZIF (Zn:Ni = 1:1) were compared in Fig. S7,† the optimal HER performance was obtained in the heterostructure sample containing 10 wt% ZnNi-ZIF. Notably, the further adoption of the MoS2 (optimal dosage of 6 wt%, Fig. S8†) cocatalyst remarkably improved the photocatalytic HER activity under UV-Vis (Fig. S9a†) and visible light irradiation (Fig. S9b†).
In order to better evaluate the important role of the MoS2 as well as the ZnM-ZIF, the photocatalytic hydrogen production activity is improved after embedded g-C3N4 with MoS2 and then with ZnM-ZIF. The systematic comparison of photocatalytic hydrogen production activity g-C3N4, g-C3N4–MoS2, ZnM-ZIF is showed in Fig. 3b and S10.† Under UV-Vis light irradiation, the pristine g-C3N4 and ZnNi-ZIF exhibited very limited hydrogen production rate of only 0.71 and 0.92 μmol h−1, respectively, and the adoption of MoS2 and ZnNi-ZIF both dramatically increased the hydrogen production rate of g-C3N4 due to the utilization and transport efficiency improving of the charge carriers, respectively. Co-embedding of ZnNi-ZIF and MoS2 enhanced the photocatalytic activity of 124.02 μmol h−1, which was 167.4 times larger than that of the pristine g-C3N4, and was 34.9 and 4.6-fold of that of the g-C3N4 singly loaded with ZnNi-ZIF and MoS2, respectively. Hence, the photocatalytic hydrogen production results proved that the embedding of ZnNi-ZIF and MoS2 showed obvious synergistic effect for increasing the photocatalytic HER activity. Specifically, the CNZN and the CNM exhibited photocatalytic HER performance of 5.7 and 64.2 times larger than that of pristine g-C3N4, indicating the ZnNi-ZIF and MoS2 played an important role on improving the number of exposed active sites and utilization efficiency of the charge carriers, respectively. It was worth noting that the photocatalytic hydrogen production rate of ternary CNMZN, CNMZC and CNMZ was 3.7, 1.9 and 1.2-fold in comparison with sum of photocatalytic hydrogen production of CNM and the corresponding g-C3N4–ZnM-ZIFs (Fig. S10†), which confirmed the synergistic effect of the embedding of MoS2 and ZnM-ZIF and facilitate the transportation and utilization efficiency of photo-generated charge carriers.
The large specific surface area, caused by improved number of exposed active sites, was also an important element for the high photocatalytic activity of CNMZN,5,54 and the nitrogen adsorption/desorption isotherms (Fig. 3c) was employed to reveal the vital function of ZnNi-ZIF on increasing the porosity of the ternary heterostructure. Adopt MoS2 could increase the specific surface area (SBET) of pure g-C3N4 to a certain extent. More obviously, CNMZN exhibited much larger nitrogen uptake and SBET of 142.73 m2 g−1 than that of CNM (33.89 m2 g−1) owing to the highly porous ZnNi-ZIF (501.34 m2 g−1). In addition to the excellent photocatalytic hydrogen production activity, the CNMZN and ZNMZC exhibited very good photocatalytic stability after 30 h continuous irradiation (Fig. 3d). In comparison with the pristine ZnM-ZIFs and their heterostructures, the characteristic FTIR peaks of ZnM-ZIF could also be clearly observed in the ZnNi-ZIF and CNMZN heterostructure after the photocatalytic reaction, which further indicated the excellent photocatalytic stability of the ternary CNMZN heterostructure (Fig. S11a†), and the unchanged FTIR spectra of CNMZ as well as CNMZC were also displayed in Fig. S11b.† To further verify the improved transport, separation and utilization efficiency of the photo-generated charge carrier in g-C3N4 caused by the adoption of MoS2 and ZnM-ZIFs, the photocatalytic hydrogen production performance of the optimal CNMZN (30.1 μmol h−1) was compared with the photocatalytic hydrogen production activity of g-C3N4, or MOF-based photocatalysts in previous publication under visible light irradiation. As displayed in Fig. 3e, the optimal CNMZN exhibited very competitive photocatalytic activity in comparison with those of semiconductor-MOFs heterostructures,2,14,35,55–57 g-C3N4-loaded with different types of cocatalysts,9–11,22,23,54 and g-C3N4-based heterostructures.9,58
The optimal g-C3N4–MoS2–ZnNi-ZIF heterostructure exhibited an excellent apparent quantum yield (AQY) value of 22.0% at 420 nm. The AQY and photocatalytic hydrogen production rate of optimal g-C3N4–MoS2–ZnNi-ZIF under different specific wavelength illuminations was evaluated and exhibited (Fig. 4a and Table S1†) with the irradiation wavelengths of 420, 475, 550 and 650 (±8) nm, the HER values 18.18, 9.22, 2.76 and 1.42 μmol h−1 (Table S1†), respectively, which indicated the HER of the optimal g-C3N4–MoS2–ZnNi-ZIF (CNMZN) photocatalyst was associated with its UV-visible diffuse reflection spectra, and the electron-promoted photocatalytic hydrogen evolution reaction. Different wavelengths further assured the photocatalytic activity of the optimal g-C3N4–MoS2–ZnNi-ZIF heterostructure. The considerable photocatalytic hydrogen production in optimal g-C3N4–MoS2–ZnNi-ZIF even with the irradiation wavelengths of 650 (±8) nm also verified that g-C3N4–MoS2 not only acted as the promoter of the charge carriers and high-performance catalyst, but also facilitated the absorption capacity of visible light. These results are consistent with the DRS and PL results of the g-C3N4–MoS2 and ZnNi-ZIF-based heterostructure.
Under UV-Vis light irradiation the photocatalytic hydrogen production of the optimal ternary CNMZN heterostructure was evaluated at different atmosphere for comprehensively assessing its practical applications value (Fig. 4b). The photocatalytic HER activity of the optimal ternary heterostructure under N2 atmosphere decreased slightly due to the easier hydrogen release under vacuum. It should be noted that even in air atmosphere with oxygen facilitating the backward reaction,13 the optimal CNMZN exhibited considerably photocatalytic hydrogen evolution activity, this result revealed that the CNMZN ternary heterostructure was suitable for practical applications.
Impressively, as demonstrated in Fig. 4c, sharp contrast to the very weak hydrogen evolution of the g-C3N4–MoS2 without sacrificial agent (pure water), the CNMZ, CNMZC and CNMZN ternary heterostructures exhibited considerable H2-evolution performance of 26.7, 36.6 and 77.8 μmol h−1 g−1 under UV-Vis light irradiation with the considerable H2O2 production rate (Fig. 4d). For deeply investigate the formation process of H2O2, using 5,5-dimethyl-1-pyrroline N-oxide (DMPO) as the spin trapping agent, Electron Paramagnetic Resonance (EPR) responses were adopted to test the oxidation products during the photocatalytic reaction in pure water of CNMZN. As exhibited in Fig. 4e, the characteristic signals of –OH could be observed in the DMPO aqueous solution after the visible light irradiation, indicating the formation of –OH through singe electron oxidation of water. On the base of the above-mentioned band structure and photocatalytic activity results, the mechanism of action of photo-exited charge carriers in the CNMZN photocatalyst was proposed in Fig. 4f.
The photo-induced electrons transferred from the CB of g-C3N4 and ZnNi-ZIFs to that of MoS2, being beneficial for the photocatalytic hydrogen production owing to the low HER overpotential and large current density of MoS2. Simultaneously, the photo-exited holes were transferred into the VB of ZnNi-ZIF, where the holes could be timely consumed by sacrificial agent due to the highly porous morphology of the ZnNi-ZIF. For investigating the important role of ZnM-ZIF and/or MoS2 on suppressing the recombination of the photo-generated electron–hole pairs of the g-C3N4 based heterostructure, the room temperature photoluminescence (PL) spectra excited at 360 nm (Fig. 5a) was employed. In contrast to the very strong PL peak of the pristine g-C3N4 (around 450 nm), the dramatically quenched PL signals were observed against the g-C3N4–ZnM-ZIF (M = Co, Cu, Ni) and CNM (Fig. S12†), owing to the increased porosity and separation as well as utilization efficiency of the charge carriers, respectively and the relative order of PL peaks for g-C3N4–ZnM-ZIF samples was found to be; g-C3N4 > g-C3N4–ZnCo > g-C3N4–ZnCu > g-C3N4–ZnNi. Notably, the ternary samples, co-embedded with ZnM-ZIF and MoS2, showed very weak PL peaks, and the relative order of PL response intensity for the samples with different types of ZnM-ZIF was found to be: CNMZ > CNMZC > CNMZN, which was consistent with the trend of the photocatalytic hydrogen evolution activity.
The g-C3N4 based photocatalysts were investigated through the transient photocurrent and electrochemical impedance spectroscopy (EIS) measurements to explore the transport and excitation behavior of the photo-exited charge carriers. As shown in Fig. 5b, with the repeated on/off cycles of UV-Vis light irradiation, all the g-C3N4 based samples exhibited the steady and reproducible photocurrent responses. The rapid recombination of charge carriers made the photocurrent density of the pristine g-C3N4 very weak. Both the g-C3N4–ZnM-ZIF (Fig. S13†) and CNM demonstrated stronger photocurrent response owing to the increased specific surface area and separation as well rapid consumed electrons, respectively. The relative order for the photocurrent density for the g-C3N4–ZnM-ZIF samples was found to be; g-C3N4 > g-C3N4–ZnCo > g-C3N4–ZnCu > g-C3N4–ZnNi, which showed that after incorporation of ZnM-ZIF (M = Cu, Co, Ni) the photocurrent density increase that was consistent with photocatalytic HER activity. Impressively, for the ternary heterostructure, the co-loading of ZnM-ZIF and MoS2 exhibited the synergistic effect for facilitating the photocurrent response, and the value of the photo-current for the ternary heterostructures with different type of ZnM-ZIF was consistent with the photocatalytic HER activity.
The EIS results of the g-C3N4, ZnM-ZIF g-C3N4–ZnM-ZIF and g-C3N4–MoS2–ZnM-ZIF were exhibited in Fig. 5c, the ternary g-C3N4–MoS2–ZnM-ZIF displayed much smaller semicircle radius than that of and pristine g-C3N4, ZnNi-ZIF, g-C3N4–ZnCo-ZIF and g-C3N4–ZnCu-ZIF (Fig. S14†), indicating that the interfacial transfer of the charge carriers was dramatically enhanced as verified by the smaller arc radius, which is normally the evidence of a lower electron transfer resistance. Notably, the CNMZN owning the optimal photocatalytic HER performance showed the smallest arc radius. In addition, the hydrogen evolution behaviors were evaluated by the Mott–Schottky plots and electrocatalytic HER and OER measurements. As depicted in Fig. 5d, the CNM displayed a more negative flat-band potentials than that of the pristine g-C3N4, indicating its improved reduction capacity. Notably, after the embedding of ZnM-ZIF, the sample exhibited higher reduction capacity as confirmed by their further upward shift in the flat-band potential, and the CNMZN with the optimal photocatalytic activity possessed the most negative flat-band potential. It was extensively reported that the cocatalyst with low electrocatalytic HER and/or oxygen evolution reaction (OER) overpotential and high current density could boost the utilization efficiency of charge carriers, thereby improve the photocatalytic activity. Moreover, the HER and OER cocatalyst could play a synergistic effect by co-loading to enhance the photocatalytic activity.59 The HER and OER capacity of the g-C3N4-based heterostructure with MoS2 and/or ZnM-ZIF were evaluated using HER and OER measurements. As could be observed from Fig. 5e and f, the embedding of both MoS2 and ZnNi-ZIF could dramatically promote the electrocatalytic HER and OER performance, and the co-embedding of MoS2 and ZnM-ZIF over g-C3N4 further facilitated the electrocatalytic HER and OER performance, and the ternary CNMZN displayed the smallest HER and OER overpotential, and the largest current density, being consistent with the photocatalytic HER performance of the g-C3N4–MoS2–ZnM-ZIFs.
Footnote |
† Electronic supplementary information (ESI) available. See DOI: 10.1039/d1ra00781e |
This journal is © The Royal Society of Chemistry 2021 |