Plasmonic lasers offer great potential for cutting-edge, disruptive applications. However, they suffer from a high loss in metals, lack of spatial coherence in the near field, and divergent far-field emission. The challenges are even more significant for a plasmonic laser emitting more than one wavelength mode. The design complexity required for creating multiple modes often limits avenues for minimizing losses and converging far-field emission patterns. This work exploits plasmonic resonances at the junction of a merged lattice metal nanohole array (NHA) and a one-dimensional photonic crystal to achieve dual-mode lasing. The merged lattice NHA is designed by concentrically combining two simple NHAs with different periodicities to create pseudo randomness, leading to enhanced localization and confinement of light in multiple wavelength modes. The proposed structure notably produces intense dual-mode lasing at an ultra-low threshold compared to recent state-of-the-art plasmonic laser demonstrations. The wavelengths of the lasing modes and the separation between them can be tuned over a broad range by changing the structural parameters. The proposed laser also creates a highly directional far-field pattern with a divergence angle of only <0.35°.
Lasers that emit multiple distinct wavelength modes are essential for various applications, including sensing multiple target substances simultaneously, distance measurements using two-wavelength interferometry, terahertz difference frequency generation, frequency mixing, frequency division multiplexing, and wavelength division multiplexing in optical circuits.23–32 To date, multimode solid-state and semiconductor lasers have been significantly explored.33–35 Nonetheless, it is a great challenge to operate these devices at room temperature due to the temperature-sensitive gain of semiconductor lasers. The increase in the non-radiative recombination rate at room temperature severely reduces the optical gain of semiconductor lasers. By contrast, research on multimode plasmonic lasers has attracted attention only recently. The first multimode plasmonic laser, reported by Wang et al. in 2017, exploited multiple band-edge modes excited using a plasmonic superlattice.36 The designed plasmonic superlattice consisted of periodic nanoparticles on periodic patches to obtain dual-mode lasing. Wang et al. obtained an emission linewidth of <0.5 nm, a mode separation of ∼10 nm, and a divergence angle of <1° from a centimeter-squared device area.
Recently, Pourjamal et al. obtained dual-mode lasing by breaking the symmetry of a two-dimensional (2D) ferromagnetic nickel plasmonic nanodisk array using different periodicities along the x- and y-directions.37 However, different periodicities along the axes result in a destructive spatial interference in the far field, thus increasing the divergence angle and making the emission less coherent in the spatial domain than if periodicities along the axes are equal. Pourjamal et al. demonstrated dual-mode lasing in the visible wavelength range with an emission linewidth of <1 nm, a mode separation of ∼15 nm, and a divergence angle of ∼5.7°. More recently, Winkler et al. utilized a plasmonic nanoparticle lattice embedded in a viscous quantum-dot film to exhibit dual-wavelength lasing.38 They adopted two methods to produce dual-mode lasing: firstly, using a rectangular silver (Ag) nanoparticle lattice; and secondly, using a thin quantum-dot film.38 They obtained an emission linewidth of ∼1 nm, a mode separation of ∼19 nm, and a divergence angle of 11.74° and 5.6° along the x- and y-directions. These approaches for plasmonic dual-mode lasing either result in a bulky laser structure due to the two-fold symmetry36 or create a divergent far-field pattern due to different periodicities in the x- and y-directions.37,38 Furthermore, breaking the symmetry of the structure in the two in-plane directions incurs additional losses by generating off-normal spatial lasing modes. These structures have also proved to be inherently lossy, thus requiring a high threshold of pump energy.
This work proposes an alternative technique for dual-mode emission from a plasmonic laser. The proposed plasmonic laser comprises an organic gain medium with a distributed Bragg reflector (DBR) as a one-dimensional (1D) photonic crystal (PhC) on one side and a merged lattice metal nanohole array (NHA) on the other side. While the merged lattice configuration helps us achieve a directional dual-mode lasing, the DBR lets us control the emission directionality and the relative intensity of the lasing modes. The basic principle is to intelligently utilize states formed by holes perforated in the metal film to create the optical feedback necessary to support dual-mode emission. The DBR acts as a filter to separate the input pump frequency of the gain medium from lasing emission frequencies. Additionally, the optical Tamm state plasmons, also known as Tamm plasmons (TPs), excited at the interface between the DBR and metal NHA and the structural pseudo-randomness-mediated strong light confinement within the laser cavity contribute to enhanced lasing emission. The dual-mode lasing emissions are highly directional as the proposed structure creates only the zeroth-order mode by employing sub-wavelength hole dimensions and periodicity in the metal NHA.
The proposed merged lattice metal NHA plasmonic laser produces dual-mode lasing in the near-infrared region. The required threshold pump energy is at least two orders of magnitude smaller than that required by several state-of-the-art demonstrations. The lasing modes have a divergence angle of ≲0.35°, and a narrow linewidth of ∼3 nm for the smaller wavelength mode and ∼1.5 nm for the longer wavelength mode. The emission wavelengths can be tuned over a broad range of ∼845–883 nm for the smaller wavelength lasing mode and ∼860–886 nm for the longer wavelength lasing mode, and the mode separation becomes as much as ∼15 nm by changing the structural parameters.
We organize the rest of the paper as follows: Sec. 2 presents the proposed dual-mode plasmonic laser, including a discussion on the design principles of the merged lattice metal NHA structure that produces dual-mode emission. Section 3 describes the simulation methodology used to calculate the interactions between the incident pump pulse and the laser structure, and the lasing dynamics of the proposed laser. In Sec. 4, we present and discuss results, including the transmission spectra of the merged lattice gold (Au) NHA and passive optical cavity; and the near- and far-field emission profiles. Finally, in Sec. 5, we conclude on the findings.
Parameter | Value |
---|---|
Absorption wavelength (λ03) | 800 nm |
Emission wavelength (λ21) | 870 nm |
Index of the PU material | 1.51 |
Dye concentration | 2 × 1018 cm−3 |
Transition lifetimes | |
τ 30 = τ21 | 1 ns |
τ 32 = τ10 | 10 fs |
In the metal layer, square hole arrays with two different periodicities are superposed, as shown in Fig. 2. The square holes have dimensions of 100 nm × 100 nm on the yz-plane. In the densely placed square hole array, the hole periodicity (Λ1) is 250 nm, as shown in Fig. 2(a). On the other hand, in the sparsely placed square hole array, the hole periodicity (Λ2) is 375 nm, as shown in Fig. 2(b). In both NHAs, four corners have identical square holes in the same places. These two short-scale periodicities maintain a fixed ratio of r = Λ2/Λ1 = 3/2. The value of r is constrained by r = R/(R − 1), where R is the least integer multiple of r.39 Here, we choose R = 3 in the designed merged lattice NHA. In our proposed structure, the two square hole arrays with periodicities Λ1 and Λ2 are superposed keeping them concentric so that the merged lattice becomes a square lattice with a primitive unit cell periodicity of Λ = RΛ1 in both the y- and z-directions, as shown in Fig. 2(c). The holes at the four corners of the merged lattice overlap from both the densely and sparsely placed NHAs.
The mathematical model of the gain medium used in this work utilizes a four-level two-electron atomic system.40,41 In this model, the dye molecules embedded in the host dielectric material act as gain molecules with four discrete electron energies for each of the two interacting electrons. The electron dynamics are governed by the four-level system's coupled rate equations and Pauli's exclusion principle.40 The available charge carriers are initially at the ground level. The incident pump pulse excites the charge carriers from the ground level to the third excited level. The excited charge carriers decay non-radiatively from level 3 to 2 and from level 1 to 0. The charge carriers decay from level 2 to 1 mainly through radiative transitions. The non-radiative transition lifetimes between levels in the four-level system are given in Table 1. The absorption and emission wavelengths and the refractive index of the host PU material for IR-140 dye molecules are also given in Table 1. We use the refractive indices of TiO2 and MgF2 as 2.23 and 1.46, respectively.
The proposed plasmonic laser structure, as schematically shown in Fig. 1, is simulated while surrounded by an air medium. The structure and the incident plane wave pump beam are periodic in the y- and z-directions. Therefore, we simulate only a unit cell in the y- and z-directions. As the structure is symmetric along both axes, symmetric and anti-symmetric boundary conditions are used in the y- and z-directions, respectively. In the direction of wave propagation, i.e., in the x-direction, we use the perfectly matched layer boundary conditions at the simulation boundaries. An 800 nm-wavelength plane wave pump pulse propagating in the x-direction acts as the energy source for this laser system. The pump pulse has a duration of 40 fs, with the electric field oscillating in the z-direction. The pump pulse is incident on the gain medium from the far end, i.e., via the DBR. The lasing emission occurs in the x-direction through the merged lattice metal NHA. The near-field time- and frequency-domain data are recorded at a distance of 2.6 μm from the outer surface of the metal NHA layer in the x-direction, opposite to the pump input side. We have used a non-uniform conformal meshing scheme for the entire simulation region with a minimum mesh size of 0.25 nm. We have performed convergence tests to ensure the validity of the mesh size and other simulation parameters used in this work.
In Fig. 3, we show the transmission spectra through simple NHAs with different periodicities and the designed merged lattice NHA. The periodicities of the simple NHAs are Λ1 = 250 nm and Λ2 = 375 nm, respectively, while the simple NHAs are concentrically combined in the merged lattice NHA. The simple NHAs produce a single dominant transmission peak, as shown in Fig. 3(a) at 558 nm for Λ1 = 250 nm and in Fig. 3(b) at 570 nm for Λ2 = 375 nm. For Λ2 = 375 nm, there is a weak and overlapped second transmission peak at ∼500 nm, as shown in Fig. 3(b), which does not transform into a lasing mode as it is not supported by the single-mode TP resonance, as will be discussed in the following section. By contrast, the designed merged lattice NHA results in not only an enhanced transmission but also localization of light intensity in more than one wavelength mode, dominantly at 555 and 605 nm, as shown in Fig. 3(c). The merging of simple NHAs in the merged lattice NHA causes a disruption or randomness of the periodic pattern on the short spatial scale. This randomness results in many scattering loops of light waves that cause a variety of light localization states—a pseudo-randomness mediated light localization phenomenon that lies between the complete randomness of Anderson localization and the fixed orderliness of a periodic system.39,48,49 We have exploited the naturally occurring cavity resonances due to the pseudo-randomness mediated mode localization in a merged lattice metal NHA based optical cavity to design the proposed dual-mode plasmonic laser.
The increased localization of waves directly results in a better resonator design for the multimode laser as it provides the necessary optical feedback in more than one mode for entrapping light. The designed merged lattice NHA for this structure incorporates better localization than a simple periodic system. The hole arrangement in the merged lattice is pseudo-random, as there is randomness on the short scale but a fixed periodicity on the longer scale. In this work, the simple lattices have been chosen such that they differ slightly in spatial resonances, which coalesce together to form 2D spatial beats.39 We show the transmission spectra of the designed merged lattice NHA in Fig. 3(c). The dual-mode lasing is sensitive to the hole dimensions and periodicity of the metal NHA. Therefore, they must be designed meticulously as the dual-mode lasing might cease to exist if the cavity mode is not supported by the gain lineshape. Also, our objective is to keep the lateral dimensions of the primitive unit cell to a minimum.
To keep the surface plasmon modes close to the emission peak of the gain medium, the ratio of the two short-scale periods r was selected to be 3/2, making R = 3 and Λ = 750 nm. If R is an integer greater than 3, we get Λ > 750 nm, as Λ increases linearly with R when Λ1 is a constant. We have kept R to a minimum possible value as greater values would make the structure laterally larger. Additionally, an increase in R will make the surface plasmon resonance (SPR) wavelength elude the vicinity of the gain medium emission peak, as the SPR is sensitive to Λ. To keep the lateral span of the merged lattice unit cell constant for increasing R, Λ1 could be reduced. However, a smaller Λ1 has a negative effect on the overall transmission intensity of the structure as the SPR shows a blue-shift when Λ1 decreases. Thus, Λ1 = 250 nm and Λ2 = 375 nm are the optimum parameter values that resulted in the best possible emission characteristics.
To investigate the resonant radiative modes of the optical cavity, we consider the gain medium as a passive layer, i.e., the PU host matrix is devoid of dye molecules. We calculate the passive optical cavity's transmission spectra for an incident broad-band plane wave. The transmission spectra of the passive cavity with simple and merged lattice NHAs are shown in Fig. 4. While a single radiative mode is obtained in the transmission spectra for structures with simple NHAs, dual radiative modes are observed in the transmission spectra for the structure with the merged lattice NHA. We find that the EOT modes obtained from the bare merged lattice metal NHA, as presented in Fig. 3(c), are red-shifted to 860 and 864 nm in Fig. 4(d). The shifts in mode wavelengths are due to the change of SPR of the bare Au NHA to TP resonances in the passive optical cavity with a DBR. The red-shift of the plasmonic mode also becomes apparent due to the increase of the effective index when the DBR is attached to the PU layer. In the proposed structure, alternating layers of TiO2 and MgF2 act as a DBR, producing a band-gap stretching from ∼840 nm to ∼1200 nm, as shown in the normalized reflection spectrum of the DBR in Fig. 4(d).
We note that when the DBR is attached to the PU layer to make an optical cavity, the reflection spectrum significantly changes from that of the bare DBR. The incident light couples to TP modes at the Au–PU dielectric interface, and intense transmission peaks are obtained within the photonic band-gap of the DBR. In the proposed structure, the transmission peak wavelengths overlap with the gain bandwidth of IR-140 dye molecules. Fig. 5 shows the excited modes in the transverse and longitudinal cross-sectional planes of the passive cavity. The transverse Au–PU interface shows a high field intensity and localization at the hole edges—the shorter wavelength mode is localized at the corner hole edges, as shown in Fig. 5(b), and the longer wavelength mode is localized at the central hole edges, as shown in Fig. 5(c). The field intensities in the longitudinal cross-sectional plane along the resonant hole edges are plotted in Fig. 5(d) and (e). The -field intensity amplification at the metal–PU layer interface, and the -field intensity distribution in the cavity signify the excitation of TP modes.52,55,56 To ensure a proper resonator response for the design, the TP resonance was designed to be around 870 nm for the maximum gain. Therefore, the period span and hole dimensions of the Au–NHA have been optimized and minimized so that the cavity modes fall within the span of ∼100 nm gain medium linewidth around the peak at 870 nm. As band-edge states offer a higher quality response and better wave localization,36 the DBR has been designed to have its first band-edge close to the position of the TP wavelength and gain emission wavelength at around 870 nm.
To determine whether the emission modes are lasing modes, we have investigated the input vs. output characteristics of our designed merged lattice plasmonic laser. The existence of a threshold pump energy for emission can prove that the emission modes are indeed lasing modes. Therefore, we have varied the incident pump pulse energy and calculated the peak emission intensity, as shown in Fig. 6(c). We note that the designed plasmonic laser does not show any emission when the pump pulse energy is less than 1.20 μJ cm−2. On the contrary, the laser emits dual modes simultaneously after the pump energy crosses the threshold value. Such a dependence of both the output emission modes on the input pump energy suggests that both the emission modes are lasing modes.
The addition of a merged lattice NHA in the proposed dual-mode plasmonic laser has significantly reduced the threshold pump energy over its simple periodic counterpart. The threshold pump energy for the proposed dual-mode laser is an order of magnitude smaller than the reported 13 μJ cm−2 for the planar single-mode plasmonic laser.21 Enhanced localization induced by the merged lattice metal NHA has reduced the threshold value of our laser. Thus, the proposed structure exhibits at least two orders of magnitude improvement in the threshold characteristics over state-of-the-art dual-mode plasmonic lasers, as summarized in Table 2. The changes in emission intensities for the smaller (λps) and longer wavelengths (λpl) show similar trends when the pump energy is ∼35 μJ cm−2. However, the λpl mode has a greater intensity than the λps mode. Above the threshold value, at first, both mode intensities increase with increasing pump energy at a high rate. We note that the lasing at the longer wavelength, which corresponds to the smaller transition energy, experiences gain saturation when the pump energy increases to ∼40 μJ cm−2. Therefore, at ∼40 μJ cm−2, the smaller lasing wavelength has more gain available, and it grows in intensity. However, for a pump energy of ∼60 μJ cm−2, the lasing emission intensities are almost saturated for both modes.
We show normalized electric field intensity profiles in the transverse and vertical cross-sections of the plasmonic laser structure in Fig. 7. In the transverse cross-section along the metal–gain medium interface, the profile shows that plasmonic modes are excited at the corner holes of a unit cell at the smaller wavelength λps, as shown in Fig. 7(b). By contrast, plasmonic modes are excited at the central holes of a unit cell at the longer wavelength λpl, as shown in Fig. 7(c). The incident plane wave is polarized along the z-direction, and the spatial modes are excited perpendicular to the direction of incidence. The SPP mode is also excited along the hole edge. Since the holes are 100 nm in size, neighboring holes along the edges of a unit cell are only separated by 25 nm. Therefore, LSPs in two neighboring holes across such a small distance couple and form stronger modes. In Fig. 7(d) and (e), we show profiles at 869 nm and 879 nm wavelengths, respectively, in the vertical cross-section along the x-direction of the structure as indicated by the vertical section plane (black border) in Fig. 7(a). We observe that plasmonic modes are excited at the hole edges along the metal–gain medium interface.
The results of the near-field mode dynamics are presented in Fig. 8 and 9. Fig. 8(a) shows the lasing emission for two sets of N and dL values: (1) N = 5 and dL = 200 nm and (2) N = 9 and dL = 180 nm. In each case, the proposed laser emits intense and distinct dual modes. However, for two different sets of N and dL values: (1) N = 5 and dL = 170 nm and (2) N = 11 and dL = 216 nm, the proposed laser does not show distinct dual modes, as shown in Fig. 8(b). For the first case, although the modes are spectrally distinct, the smaller wavelength mode is too broad and weak to be usable. By contrast, for the second case, the lasing modes are so close to each other that their spectral overlap creates a distorted mode shape, and they can no longer be distinguished as isolated modes. Therefore, to define practicable dual-mode emissions and find a tuning range of the proposed laser, we consider the emission intensity at N = 5 and dL = 200 nm in Fig. 8(a) as a reference to define the dual-mode emissions. This particular configuration of N and dL gives us clear, well-separated, and almost equally-prominent peak intensities, as will become clear in the results presented in the following paragraphs. We assume that if the peak intensity of any mode becomes less than 0.2 times the peak intensity at N = 5 and dL = 200 nm, the emission is too weak and less than the minimum acceptable value. On the other hand, if the separation between the two lasing modes is smaller than their combined linewidths, the modes significantly overlap and result in a distorted single-mode, with possible adjacent side lobes. Such a case of distorted mode shape is also not considered as dual-mode lasing.
The mode intensities, peak wavelengths, separations, and linewidths vary when N and dL change. We find that the mode separation (Δλ) of the lasing modes shows a non-monotonic dependence on N and dL, as shown in Fig. 8(c). When dL increases with a fixed N, we find that Δλ decreases. Similarly, Δλ shows a decreasing trend as N increases. Because of the complex geometry of the merged lattice NHA and the mode competition between the lasing modes, the output behavior is substantially non-linear. Fig. 8(d)–(g) show 2D surface plots for the emission intensity of the proposed laser against wavelength and dL. The proposed structure can be tuned to emit in the smaller wavelength mode in the range of ∼845–883 nm and in the longer wavelength mode in the range of ∼860–886 nm by changing dL and N. When dL ≳ 210 nm for any N, we find that Δλ becomes too small to support the linewidth of the two individual modes, and the dual modes get distorted and become indistinguishable due to the spectral overlap. With a decreasing Δλ, the dual modes merge and emerge as a broader and distorted single mode.
Fig. 9 shows the full-width at half-maximum (FWHM) linewidths and peak intensities of the two wavelength modes when dL varies between 160 and 220 nm for N = 5, 7, 9, and 11. FWHM linewidths show a non-monotonic decreasing trend with dL, especially for the smaller wavelength mode, as shown in Fig. 9(a) and (b). When N = 5, the smaller wavelength mode has a broader linewidth compared to that of the longer wavelength mode. However, for N > 5, the smaller wavelength mode has a narrower linewidth than that of the longer wavelength mode for a significant range of dL. The smaller wavelength mode's linewidth decreases with increasing N, while the longer wavelength mode's linewidth shows a less significant variation with N.
Fig. 9(c) and (d) show the intensities of the lasing modes against dL for different N. For N = 5 and 7, the two wavelength modes are in significantly good shape and of similar relative prominence in intensity. However, for N = 9 and 11, we get a much greater intensity for the smaller wavelength mode compared to that of the longer wavelength mode, especially when dL varies in the range of ∼195–210 nm. Fig. 9(c) and (d) show that the peak intensity of the smaller wavelength mode has a maximum around dL ≈ 200 nm and increases non-monotonically with N. The longer wavelength mode shows only a little variation in its peak intensity. We note that a greater N favors stronger emissions from the smaller wavelength mode, making it more prominent than the longer wavelength mode. The peak intensity and linewidth of the longer wavelength mode remain almost unaffected with the change of N.
The tendencies of the separation, spectral position, linewidth, and peak intensities of the two lasing modes presented in Fig. 8 and 9 primarily depend on the physics of the tuning mechanism of TP modes for varying dL and N. The trends observed in the near-field mode dynamics conform to the existing theoretical formulations of Tamm resonance behavior at the metal–DBR interface.50,61 A 1D “double period” patterning of the top metal layer has been shown to create a Tamm plasmonic band-gap with two modes and control their tuning characteristics.64 The merged lattice metal NHA on top of the gain medium also contributes to the tuning behaviour besides exciting Tamm resonances. Through such an in-depth analysis of the lasing mode dynamics, we have determined a range of values for N and dL that would create an intense and spectrally well-separated dual-mode emission. The calculated ranges for limiting structural parameter values for dual-mode lasing are given in Table 3. Within these ranges, the intensities of the lasing modes are high and comparable to those of other reported plasmonic lasers; the linewidths are narrow, and the lasing modes do not overlap each other.
N | 5 | 7 | 9 | 11 |
d L | ∼179–209 nm | ∼171–213 nm | ∼170–211 nm | ∼170–212 nm |
We have calculated the far-field patterns of the proposed merged lattice plasmonic laser for a device area of 150 μm × 150 μm in the yz-plane. The far-field intensity profile is obtained by projecting the near-field profile away to a distance of 1 m. Then the obtained far-field distribution profiles have been normalized using the intensity of the pump pulse. The far-field analyses for both the lasing modes show similar results, as shown in Fig. 10. The long-range periodicity of the lattice and the two-fold symmetry in the merged lattice configuration cause a more significant constructive interference in the far field. The proposed laser produces a far-field divergence angle of <0.35°, which is much smaller than that of other dual-mode plasmonic lasers.36–38 The far-field divergence angle of the proposed laser is also significantly smaller than the reported 1° divergence angle of the planar single-mode laser in ref. 21. Therefore, the addition of a merged lattice NHA has notably improved the performance of our dual-mode plasmonic laser in the far field compared to the planar single-mode laser in ref. 21 and dual-mode lasers reported in ref. 36–38. Our design is thus highly coherent in the near-field spatial domain and directional in the far field.
Footnote |
† These authors contributed equally. |
This journal is © The Royal Society of Chemistry 2022 |