aDepartment of Mechanical Engineering, Polytechnique Montréal, 2900 Boulevard Edouard-Montpetit, Montréal, QC H3T 1J4, Canada. E-mail: etienne.robert@polymtl.ca
bACSYNAM Inc., Montréal, QC H1P 1W1, Canada
cDepartment of Chemistry, McGill University, 801 Sherbrooke Street West, Montréal, QC H2L 0B7, Canada. E-mail: tomislav.friscic@mcgill.ca
dUniversity of Warsaw, 1 Pasteura Street, Warsaw, 02-093, Poland
e525 Solutions, P.O. Box 2206, Tuscaloosa, Al 35403, USA. E-mail: robin.rogers@525solutions.com
fReaction Dynamics, 45 Chemin de l’Aéroport, Saint-Jean-sur-Richelieu, QC J3B 7B5, Canada
First published on 28th February 2022
Hybrid rocket propulsion can contribute to reduce launch costs by simplifying engine design and operation. Hypergolic propellants, i.e. igniting spontaneously and immediately upon contact between fuel and oxidizer, further simplify system integration by removing the need for an ignition system. Such hybrid engines could also replace currently popular hypergolic propulsion approaches based on extremely toxic and carcinogenic hydrazines. Here we present the first demonstration for the use of hypergolic metal–organic frameworks (HMOFs) as additives to trigger hypergolic ignition in conventional paraffin-based hybrid engine fuels. HMOFS are a recently introduced class of stable and safe hypergolic materials, used here as a platform to bring readily tunable ignition and combustion properties to hydrocarbon fuels. We present an experimental investigation of the ignition delay (ID, the time from first contact with an oxidizer to ignition) of blends of HMOFs with paraffin, using White Fuming Nitric Acid (WFNA) as the oxidizer. The majority of measured IDs are under 10 ms, significantly below the upper limit of 50 ms required for functional hypergolic propellant, and within the ultrafast ignition range. A theoretical analysis of the performance of HMOFs-containing fuels in a hybrid launcher engine scenario also reveals the effect of the HMOF mass fraction on the specific impulse (Isp) and density impulse (ρIsp). The use of HMOFs to produce paraffin-based hypergolic fuels results in a slight decrease of the Isp and ρIsp compared to that of pure paraffin, similar to the effect observed with Ammonia Borane (AB), a popular hypergolic additive. HMOFs however have a much higher thermal stability, allowing for convenient mixing with hot liquid paraffin, making the manufacturing processes simpler and safer compared to other hypergolic additives such as AB.
To fulfill its potential of reduced development costs and improving mechanical simplicity, hybrid rocket propulsion is in need of novel propellant systems to be competitive for launch vehicle applications, especially regarding specific and density impulses. This can be achieved with energy-dense additives in fuel grains made of solid hydrocarbons, including metal or organic hydrides and crystalline metals.32,33 As an example, the incorporation of aluminum particles has been shown to improve the specific impulse of hybrid propellants relying on relatively weak oxidizers such as hydrogen peroxide or nitrous oxide.32 Another way of making hybrid rockets more interesting is by inducing the hypergolic ignition of its fuel. Additives such as ammonia borane (AB) can be included in a fuel matrix.25,29,33,34 On contact with the oxidizer, white fuming nitric acid (WFNA) for example, AB spontaneously ignites. A critical parameter here is the time elapsed from the first contact between the oxidizer and the fuel to the appearance of flames. This is called the ignition delay (ID) and low values are essential to ensure proper operation in hypergolic engines.
Here, we present a proof-of-principle demonstration of experimental and theoretical performance characteristics of a new class of hypergols based on a metal–organic framework (MOF) design.35–38 We have recently demonstrated how the combination of metal nodes such as Zn2+ and Co2+, with linkers based on suitably substituted imidazoles (e.g. 2-vinyl and 2-acetylene-substituted imidazoles, HVIm and HAIm, respectively, Fig. 1a), results in zeolitic imidazolate frameworks (ZIFs)39,40 exhibiting hypergolic behavior (Fig. 1b and c).
Fig. 1 (a) Schematic representation of the ligand used in this study. (b) A general illustration of the HMOFs. (c) A Schematic diagram of the assembly of metal ions and organic linkers to form HMOFs. |
Specifically, these hypergolic MOFs (HMOFs) were found to exhibit ultrashort IDs (below 50 ms, and often below 5 ms) when in contact with traditional oxidizers such as white and red fuming nitric acids (WFNA, RFNA, respectively), along with heats of combustion (ΔHC) around −8700 kJ mol−1, with volumetric energy density (Ev) of 36.3 kJ cm−3.39 While these values are higher than for MMH (ΔHC = −1304 kJ mol−1; Ev = 24.7 kJ cm−3) or UDMH (ΔHC = −1979 kJ mol−1; Ev = 25.9 kJ cm−3),39,41 HMOFs are also attractive as readily handled solids. They are stable in extended storage and do not exhibit ignition below at least 250–325 °C,40 compared to AB who can self-ignites at temperature as low as 75 °C.42
As the next step in developing MOFs as a platform for new hypergolic systems, we demonstrate here that these HMOFs are highly effective additives to induce hypergolicity into conventional, non-hypergolic hybrid engine paraffin fuels. The hypergolic and energetic properties of HMOFs will be compared against additives currently used to bring these characteristics to hybrid fuels; AB and Al,43 respectively.
The IDs of hypergolic hybrid additives documented in the literature, including the HMOFs used here, are provided in Table 2. Previously reported RFNA and WFNA ignition drop tests on pure HMOFs samples revealed that the materials generated from HAIm exhibit the shortest ID values, at or below 5.0 ms. The HMOFs based on HVIm exhibit longer IDs, with Co(VIm)2 at 11.0 (5.0) ms, and its zinc and cadmium analogues above 10 ms. These values compare advantageously with those of currently available hypergolic propellants or additives used for blending in hydrocarbon or polymeric matrices. More specifically, the HAIm-based HMOFs exhibit IDs matching that of hydrazines and AB. Even the worst-performing Cd(VIm)2 exhibits an ID of 35.0 (1.0) ms at atmospheric pressure, notably shorter than the 50 ms target.40 Other new HMOFs technologies, namely ZZU-362 and ZZU-363, were recently explored by Wang et al.45 where hypergolic metal clusters were assembled with energetic ligands to create high density HMOFs, with IDs in the range of 26 to 60 ms.
Category | Additive | Avg. ignition delay [ms] | Standard deviation [ms] | Ref. |
---|---|---|---|---|
a Test conducted at a pressure of 0.10 MPa with analytical reagent-grade nitric acid (69.3 wt%). | ||||
Common hypergolic additive | AB | 2.0 | — | 19 |
Hydrazine | 3.1 | — | 46 | |
Lithium–aluminum-hydridea | 31.3 | 7.2 | 47 | |
Metal–organic framework | ZZU-362 | 59.0 | — | 45 |
ZZU-363 | 26.0 | — | 45 | |
Co(VIm)2 | 11.0 | 5.0 | 40 | |
Zn(VIm)2 | 29.0 | 1.0 | — | |
Co(AIm)2 | 2.0 | 1.0 | 40 | |
Zn(AIm)2 | 2.0 | 1.0 | 40 |
Ignition was investigated for three different sample configurations (configuration I, II and III), differing in how the HMOF and the FR5560 wax are combined. Configuration I was based on a fuel pellet made from homogeneous blend of 80 wt% FR5560 wax paraffin and 20 wt% HMOF. Configuration II consisted of a fuel pellet with a thin layer (ca. 10 mg by weight) of a HMOFs placed on top of it. In configuration III, a central hole was drilled in the pellets and filled with ca. 10 mg of a HMOF.
Samples for ignition testing in configuration I were made by melting the paraffin on a hot plate, followed by addition of a HMOF and gentle stirring until a homogeneous liquid is obtained. The blend was then poured into an aluminum mold and hand-pressed. Before ignition tests, the pellet surface was sanded using 80-grit sandpaper to ensure a consistent contact surface and exposure of hypergolic additives to the oxidizer droplet. Pellets were made one by one and, unless otherwise specified, ignition tests were performed in triplicate.
Samples for ignition testing in configuration II were prepared following the same steps as configuration I, followed by of pressing ca. 10 mg of a HMOF powder on the top surface of the pellet. Samples in configuration III were prepared by following the same steps as for configuration I. After solidification, a small hole of ca. 2 mm diameter and a depth of 4 mm was drilled in the center of the pellet, into which 10 mg of HMOFs powder was placed and gently pressed. Pellets for studies in configurations II and III were based either on pure paraffin, or on a mixture containing 20 wt% HMOFs with 80 wt% paraffin. In the latter case, both propellants were mixed together in the same way as for configuration I.
Fig. 2 Droplet ignition tests on (a) pure Co(VIm)2, (b) pure Zn (VIm)2, and (c) pure Co(AIm)2 using ca. 10 mg of HMOF powder samples and WFNA as the oxidizer. The location of the first ignition is marked with the white arrow. Picture in (c) were digitally modified to remove reflections on the glass vial. The original videos are available online as ESI.† |
For the ignition tests conducted on samples containing the paraffin and a HMOF, the results are summarized in Table 4.
Fuel Additive | Chemical Formula | Density [g cm−3] | ΔH0f [kJ mol−1] |
---|---|---|---|
Co(VIm)2 | Co(C5H5N2)2 | 0.944 | −1.3 |
Zn(VIm)2 | Zn(C5H5N2)2 | 0.976 | −51.5 |
Co(AIm)2 | Co(C5H3N2)2 | 0.985 | 445.8 |
Zn(AIm)2 | Zn(C5H3N2)2 | 0.996 | 397.1 |
MOF | Configuration | Pellet content | Avg. ignition dlay [ms] | Standard deviation [ms] |
---|---|---|---|---|
a Tested in the form of powder since the mixture was too brittle to form a pellet. | ||||
Co(VIm)2 | I | 80 wt% FR5560 wax/20 wt% Co(VIm)2 | — | — |
50 wt% FR5560 wax/50 wt% Co(VIm)2 | — | — | ||
II | 100 wt% FR5560 wax | 12.9 | 10.7 | |
80 wt% FR5560 wax/20 wt% Co(VIm)2 | 13.3 | 5.3 | ||
III | 100 wt% FR5560 wax | 6.3 | 1.6 | |
80 wt% FR5560 wax/20 wt% Co(VIm)2 | 8.3 | 0.1 | ||
Zn(VIm)2 | I | 80 wt% FR5560 wax/20 wt% Zn(VIm)2 | NT | NT |
50 wt% FR5560 wax/50 wt% Zn(VIm)2 | — | — | ||
II | 100 wt% FR5560 wax | — | — | |
80 wt% FR5560 wax/20 wt% Zn(VIm)2 | — | — | ||
III | 100 wt% FR5560 wax | — | — | |
80 wt% FR5560 wax/20 wt% Zn(VIm)2 | — | — | ||
Co(AIm)2 | I | 80 wt% FR5560 wax/20 wt% Co(AIm)2 | — | — |
50 wt% FR5560 wax/50 wt% Co(AIm)2 | 7.0a | 1.8a | ||
II | 100 wt% FR5560 wax | 2.3 | 0.1 | |
80 wt% FR5560 wax/20 wt% Co(AIm)2 | NT | NT | ||
III | 100 wt% FR5560 wax | 1.8 | 0.7 | |
80 wt% FR5560 wax/20 wt% Co(AIm)2 | NT | NT |
The resulting energies were used to compute the enthalpies of formation according to the following reaction equations:
Co(VIm)2: Co(s) + 10C(s) + 2N2(g) + 5H2(g) → Co(C5H5N2)2(s) | (1) |
Zn(VIm)2: Zn(s) + 10C(s) + 2N2(g) + 5H2(g) → Zn(C5H5N2)2(s) | (2) |
Co(AIm)2: Co(s) + 10C(s) + 2N2(g) + 3H2(g) → Co(C5H3N2)2(s) | (3) |
Zn(AIm)2: Zn(s) + 10C(s) + 2N2(g) + 3H2(g) → Zn(C5H3N2)2(s) | (4) |
To achieve ignition, we explored using a single pellet containing 50 wt% Co(VIm)2 and 50 wt% paraffin wax. In this case, a strong reaction occurred on the surface of the pellets, with bubbles and gas generation 100.8 ms after the first contact with the WFNA droplet. The herein used pellet fabrication method, in which the HMOFs are mixed with melted paraffin, could hinder hypergolic ignition at low loadings, due to the paraffin completely coating the very fine particles and shielding them from the oxidant. Ignition of paraffin requires vaporization through the exothermic hypergolic ignition upon contact of the HMOF with WFNA. In configuration I, the heat produced from the weak outgassing is lost to the WFNA liquid layer resting on top of the pellet. Several seconds after the test, each pellet was thoroughly examined: a black layer of burned HMOFs was present on its surface, hinting that some HMOFs reacted with the oxidant, but that this reaction was indeed quenched before triggering the combustion of paraffin.
Drop tests in configuration II revealed ignition in all cases, accompanied with large bursts of flame visible in half of all the tests performed. Bursts of flame occurred mainly on top of the pellets and are attributed to the hypergolic ignition of the HMOF upon contact with WFNA. Overall, the experiments suggest that the HMOF flame did not transition to a paraffin flame and that the paraffin did not react with WFNA. The hypergolic ignition in this case also does not appear to generate enough heat to melt the paraffin and create a sustained flame, most likely because of the small particle size in the HMOF layer. Due to the impact of the WFNA droplet, part of the HMOF layer was expelled away from of the paraffin pellet, which decreased the opportunity for ignition of the paraffin. In this configuration, and using Co(VIm)2 as the HMOF, a large variation in IDs was observed, which we believe might be related to other factors not evaluated here, such as the compactness or the uniformity of the HMOF layer. These two parameters will affect the spreading of the HMOF layer upon impact with the oxidizer droplet.
To test the hypothesis of HMOF particles being too small, we explored hypergolic ignition in configuration III. In 5 out of 6 cases, using either neat paraffin or a blend of paraffin and Co(VIm)2 in respective weight ratio 80:20, sparks were produced, followed by bursts of flames resembling those observed for configuration II. However, the bursts of flame in configuration III were also followed by continuous combustion (up to 2.5 s) that was attributed to the paraffin, first reacting with the leftover WFNA and then with ambient air. This interesting result indicated that the addition of HMOFs in the fuel matrix did not significantly hinder the ignition of the paraffin, thus confirming that combustion is not affected after the hypergolic reaction. Using 5 mg Co(VIm)2 instead of 10 mg in this configuration did not lead to the ignition of the paraffin.
Notably, the ignition with Co(VIm)2 in configuration III, using either pure paraffin and or HMOF-paraffin blends as the pellet material, produced remarkably short average IDs of respectively 6.3 (1.6) ms and 8.3 (0.1) ms. These values are 52% and 37% shorter, respectively, than the IDs seen in configuration II, confirming that spatially concentrated HMOF not only enable paraffin ignition, but also reduce the ID value. One of the major differences between both configurations is the reduction of the amount of HMOF particles expelled from the pellet upon contact with the droplet in configuration III. Concentrated in the center of the pellet, the HMOF flame contributed more to the vaporization of the paraffin through longer flame and direct contact with the edges of the hole. Furthermore, eight out of twelve tests in configurations II and III were observed to ignite with IDs below 10 ms, which is considered to be the target value for dynamic altitude control systems.33
A single droplet test was performed with a pellet containing 50 wt% paraffin wax and 50 wt% Zn(VIm)2 under configuration I. Since sparks were not observed in that case, ignition of mixtures containing 20 wt% of Zn(VIm)2 was not tested.
The poor hypergolic performance of Zn(VIm)2-paraffin blends compared to those based on Co(VIm)2 did not warrant further experiments. This result was consistent with our previous observation40 of lower hypergolic reactivity for HMOFs based on zinc, compared to cobalt.
Fig. 3 Example of a ignition drop test on 50 wt% FR5560 wax/50 wt% Co(AIm)2 using WFNA as the oxidizer. The location of the first ignition is marked with the white arrow. Full sequence available on ESI.† |
Tests carried with Co(AIm)2 in configuration II all revealed rapid ignition, with an average ID of 2.3 (0.1) ms, which corresponds to a reduction of 82% compared to Co(VIm)2 in the same configuration. In addition to a remarkably short ID values, well under the 10 ms target value, paraffin ignition and burning was observed in two out of three tests (Fig. 4). Compared to Co(VIm)2, the herein observed ignition of paraffin bearing a thin layer of Co(AIm)2 may be attributed to a faster hypergolic reaction with WFNA, leading to more heat being transferred to the paraffin before the HMOF particles were expelled from the surface. Overall, these results clearly demonstrate that the heat released by hypergolic ignition of a thin layer of Co(AIm)2 can be used to ignite solid paraffin fuel underneath.
Fig. 4 Example of an ignition drop test on a FR5560 wax pellet covered with a thin 10 mg layer of Co(AIm)2 (configuration II), using WFNA as the oxidizer. The location of the first ignition is marked with the white arrow. (a) Burned paraffin and HMOFs. (b) Burning HMOF. (c) Paraffin flame. Full sequence available in ESI.† |
Ignition drop tests with Co(AIm)2 in Configuration III gave the shortest ID values, leading to an average of 1.8(0.7) ms. This value represents a decrease of 71% compared to the results obtained with Co(VIm)2 in the same configuration. Notably, following the initial hypergolic ignition of Co(AIm)2, paraffin ignition was observed in all cases (Fig. 5).
Fig. 5 Drop tests on neat paraffin wax pellet with a 10 mg of Co(AIm)2 located in a hole in the center, using WFNA as the oxidizer. The location of the first ignition is marked with the white arrow. (a) Burned paraffin and HMOF. (b) Burning HMOF powder. (c) Paraffin flame. Full sequence available in ESI.† |
The Isp and density specific impulse (ρIsp) are propulsive performance parameters heavily dependent on a variety of physical factors such as engine and nozzle geometries as well as on the fuels and oxidizers used. The exhaust gas velocity Ve is a critical parameter in the calculation of the Isp. So it is a function of the temperature of combustion Tc, the mean molecular weight of the exhaust gas MW, the ratio of the exit pressure and combustion pressure and the ratio of specific heat γ:
(5) |
Thus, the higher the combustion pressure and temperature, and the lower the molecular weight of the combustion gas, the higher the performance of the engine will be.
The density specific impulse measures the performance of a given propellant by taking into account its density, with higher density specific impulse associated with higher engine performance for a given volume of propellant. It is defined by:
ρIsp = ρprpopellant·Isp | (6) |
(7) |
Finally, the C* values are a mean to assess the combustion independently of the nozzle efficiency or performance. The value of C* is proportional to the Isp and is defined by:
(8) |
The Isp and ρIsp of hybrid paraffin-based fuel mixtures containing HMOFs were calculated using the NASA-CEA software.52 The values obtained were then compared to those for paraffin fuels containing AB and aluminum for reference. AB in a paraffin matrix can yield hypergolic ignition,14,19,34 just as our proposed use of HMOFs. Although aluminum particles as fuel additives do not yield hypergolicity, they were considered here for comparison as energetic rocket fuel additives.43 The oxidizers investigated were WFNA, LOx and high-test peroxide (HTP, H2O2 at 90 wt% concentration in H2O). The absolute combustion chamber pressure considered was 6.89 MPa (1000 psia) and the exhaust gases were assumed to be in chemical equilibrium conditions and perfectly expanded to atmospheric pressure. The properties of the oxidizers were retrieved from NASA-CEA, with the densities used for calculations being 1.141 g cm−3 for LOx, 1.513 g cm−3 for WFNA and 1.392 g cm−3 for HTP. The chemical formula of the paraffin used for the analysis is C32H66 with an approximate density of 0.90 g cm−3. The properties of paraffin, aluminum and AB were extracted from the NASA-CEA library whereas those of the HMOFs were measured experimentally and reported earlier in Table 3.
Fuel | Oxidizer | O/F | I sp [s] | ρI sp [sg cm−3] |
---|---|---|---|---|
HTPB | WFNA | 4.5 | 265.1 | 360.0 |
HTPB | LOx | 2.3 | 301.2 | 321.5 |
HTPB | H2O2 90 wt% | 6.7 | 289.2 | 378.1 |
Paraffin | WFNA | 5.0 | 264.4 | 359.3 |
Paraffin | LOx | 2.6 | 301.8 | 321.0 |
Paraffin | H2O2 90 wt% | 7.4 | 289.0 | 377.7 |
Before assessing the performances of HMOFs within a paraffin fuel matrix, the Isp was calculated for their pure form and was compared to the values for aluminum and AB. These results are presented for Co(AIm)2 and Co(VIm)2 in Table 6. With all oxidizers studied, pure AB always presented the highest specific impulse. Pure Co(AIm)2 and Co(VIm)2 had slightly lower Isp values compared to AB but were always higher than pure aluminum. As expected, aluminum yielded a higher ρIsp compared to AB and the selected HMOFs because of its high density. Interestingly, the ρIsp of Co(AIm)2 and Co(VIm)2 was higher than AB when WFNA or HTP were used as the oxidizer.
Oxidizer | Fuel | O/F | I sp [s] | ρI sp [sg cm−3] |
---|---|---|---|---|
WFNA | AB | 1.00 | 288.67 | 297.14 |
Aluminum | 2.00 | 231.88 | 411.05 | |
Co(VIm)2 | 2.50 | 242.01 | 312.35 | |
Zn(VIm)2 | 2.50 | 241.83 | 316.17 | |
Co(AIm)2 | 2.25 | 245.24 | 318.50 | |
LOx | AB | 1.75 | 316.62 | 309.22 |
Aluminum | 2.25 | 228.32 | 316.79 | |
Co(VIm)2 | 1.25 | 261.16 | 272.69 | |
Zn(VIm)2 | 1.25 | 264.04 | 280.21 | |
Co(AIm)2 | 1.25 | 263.48 | 280.86 | |
H2O2 90 wt% | AB | 1.25 | 298.04 | 307.61 |
Aluminum | 2.75 | 269.86 | 431.37 | |
Co(VIm)2 | 3.75 | 271.13 | 343.13 | |
Zn(VIm)2 | 3.75 | 270.95 | 346.10 | |
Co(AIm)2 | 3.50 | 272.80 | 347.81 |
Oxidizer | Additive | O/F | C* [m s−1] | T C [K] | M W [g mol−1] |
---|---|---|---|---|---|
WFNA | AB | 4.1 | 1616.1 | 3105.95 | 24.729 |
Aluminum | 3.4 | 1614.5 | 2905.89 | 23.916 | |
Co(VIm)2 | 4.5 | 1571.8 | 3131.48 | 27.299 | |
Zn(VIm)2 | 4.5 | 1573.9 | 3139.94 | 27.351 | |
Co(AIm)2 | 4.0 | 1585.8 | 3123.26 | 26.029 | |
LOx | AB | 2.1 | 1836.1 | 3503.93 | 21.942 |
Aluminum | 1.7 | 1814.9 | 3623.51 | 22.662 | |
Co(VIm)2 | 2.4 | 1771.5 | 3660.30 | 26.021 | |
Zn(VIm)2 | 2.3 | 1781.9 | 3652.10 | 25.388 | |
Co(AIm)2 | 2.1 | 1789.9 | 3594.36 | 24.232 | |
H2O2 90 wt% | AB | 5.8 | 1754.4 | 3065.08 | 20.805 |
Aluminum | 5.0 | 1749.0 | 3164.18 | 21.496 | |
Co(VIm)2 | 5.7 | 1730.1 | 3062.22 | 21.441 | |
Zn(VIm)2 | 5.7 | 1732.4 | 3070.17 | 21.467 | |
Co(AIm)2 | 5.7 | 1732.2 | 3075.78 | 21.538 |
As shown in Fig. 7a and b, both Isp and ρIsp are slightly lower when HMOFs were added to the fuel mixture compared to pure paraffin reacting with WFNA, decreasing approximately linearly with increasing MOF loading. This contrasts with the use of AB, which resulted in a slight increase in Isp. The addition of aluminum also yielded an increase in Isp, an effect scaling approximately linearly with increased additive mass loading (an increase of 3.3% at a mass load of 50 wt%). Although there was a minor reduction in Isp on the order of 2.0% at a mass load of 50 wt% for the HMOF-containing fuels compared to pure paraffin as well as paraffin-AB or -Al mixtures, this modest performance tradeoff implied that HMOFs could be useful as additives to impart hypergolicity to an otherwise non-hypergolic fuel.
The performance parameters were also calculated using LOx as an oxidizer, with the results shown in Fig. 8a, yielding higher values compared to WFNA. Additionally, the decrease in Isp and ρIsp values associated with increasing the HMOF mass loading was less pronounced when LOx was used in calculations. For instance, when using LOx the decrease of Isp for Zn(AIm)2 at a fixed mass load of 20 wt%, was 2.15% and 1.18% compared to AB and Al, respectively. Corresponding values were 1.53% and 1.84%, respectively, when WFNA was used. Interestingly, behavior of the calculated Isp as a function of the O/F ratio for the HMOFs revealed a very similar combustion behavior to the fuel blends using AB and Al as additives, again considering a case with 20% mass loading (Fig. 8c). The curves were all similar in profile, with maxima close to an O/F ratio of 2.5 in all cases. Notably, the Isp values for Zn(AIm)2 and AB are almost equal and just under 300 s at an O/F ratio of approximately 2.5.
Finally, the same parameters were calculated using HTP as an oxidizer (Fig. 9). Overall, the Isp of the hypergols was similar to those obtained when using LOx as an oxidizer. However, there was a smaller drop in Isp with increasing HMOF mass loading. At a mass loading of 20 wt%, the decrease was of 0.98% and of 1.07% when compared to AB and Al, respectively, at the same mass loading. However, the ρIsp with 90% HTP was higher than that when using WFNA as the oxidizer. The trends for the variation of the Isp as a function of the O/F again showed very similar combustion behavior between the HMOFs, AB and Al additives.
In addition to the Isp and ρIsp calculated using the NASA-CEA software, the C* values were also computed. The values are reported in Table 7 for a mass loading of 20 wt% in a paraffin matrix, in each case for the O/F ratio that provides the maximum C* value. The combustion temperature corresponds to the temperature inside the combustion chamber, whereas the molecular weight was computed at the exit of the nozzle and took into account products in condensed phases.
The results presented here showed that for the HMOF considered, the C* and optimal O/F were similar. The latter was also comparable to the optimal O/F when AB was used as the additive. Interestingly, when LOx was used as the oxidizer, every paraffin-additive mixtures had a higher C* than the previously mentioned RP1-LOx (1774 m s−1) and N2O4-UMDH/hydrazine (1711 m s−1) fuel–oxidizer combinations. When considering 90% HTP as the oxidizer, the C* values for the HMOFS were also higher than for the N2O4-UMDH/hydrazine combinations. In general, combustion of paraffin and HMOFs yielded a higher combustion temperature compared to AB, while surpassing aluminum when WFNA was used as the oxidizer. Even though the temperature of combustion of HMOFs was higher than AB, the specific impulse of the latter was higher, primarily due to the lower molecular weight of the exhaust gases.
A hybrid engine relying on HMOFs to provide hypergolicity to paraffin or other hydrocarbon fuel matrices would therefore lose slightly in Isp, but gains in having a simple ignition, eliminating the need for more complex external ignition systems. Hypergolic propellants can also add flexibility with regards to possible mission profiles, as they could enable reliable restartability, a feature not possible for solid rockets and adding complexity to non-hypergolic hybrids. A caveat is the difficult ignition observed when the very fine HMOF powders were evenly mixed with paraffin. In droplet ignitions test shown here, the mixture composition surrounding MOF particles immersed in the fuel matrix is very lean and as a result the hot outgassing that might initiate the combustion can be quenched by the local overabundance of oxidizer. In engine conditions, careful tuning of the O/F ratio during the transient ignition phase of operation could avoid this problem, but this observation highlights the necessity to carefully assess the importance of granulometry of the additives on the hypergolic ignition phenomena in hybrid engines.
Compared to the reference hypergolic additive for hybrid rocket propulsion, AB, HMOFs have the potential to be much easier to mix with paraffin and other hydrocarbons. This is explained by the presence of organic ligands and by their much higher temperature of decomposition, determined by thermogravimetric analysis to be 250–325 °C (ref. 40) for the HMOFs considered here, and 80–100 °C for AB.42 HMOFs also have lower toxicity compared to hypergolic fuels based on hydrazine, meaning they offer a safer and less toxic alternative additive that is easier to handle. Finally, HMOFs have the ability to be tailored as needed by including other metals or chemical compounds in their porous structure, making them suitable for a wide range of needs.
Footnote |
† Electronic supplementary information (ESI) available. See DOI: 10.1039/d1sc05975k |
This journal is © The Royal Society of Chemistry 2022 |