Yong Liuab,
Yanlan Liua,
Zhao Yanga and
Jianlong Wang*bc
aCollege of Chemistry and Materials Science, Sichuan Normal University, Chengdu 610066, PR China
bCollaborative Innovation Center for Advanced Nuclear Energy Technology, INET, Tsinghua University, Energy Science Building, Beijing 100084, PR China. E-mail: wangjl@tsinghua.edu.cn; Fax: +86-10-62771150; Tel: +86-10-62784843
cBeijing Key Laboratory of Radioactive Wastes Treatment, Tsinghua University, Beijing 100084, PR China
First published on 26th October 2017
In this study, Zn-CNT composites were prepared by the infiltration fusion method and characterized by TEM, XPS and N2 adsorption/desorption experiments. The reaction of Zn-CNTs and O2 in aqueous solution was performed for the in situ generation of H2O2, which was employed to react with Fe2+ for the Fenton degradation of 4-chlorophenol (4-CP). The effect of various parameters, including the initial pH, dosage of Zn-CNTs and Fe2+ concentration on 4-CP degradation was examined. The removal efficiencies of 4-CP and TOC (total organic carbon) were 98.8% and 87.4%, respectively, when the Fe2+ concentration was 20 mg L−1, initial pH was 2.0, Zn-CNT dosage was 2 g L−1, reaction time was 20 min and O2 flow rate was 400 mL min−1. When 4-CP was spiked in the secondary effluent of a municipal wastewater treatment plant, the removal efficiency of 4-CP and TOC was 47.0% and 45.6%, respectively, under the above-mentioned conditions. The intermediate products were detected by LC-MS and IC, and the possible degradation pathway of 4-CP and the reaction mechanism of the Zn-CNTs/O2/Fe2+ system were tentatively proposed.
The in situ generation of H2O2 can be obtained by a micro-electrolysis (ME) process based on the electrochemical reaction between O2 and the ME materials, which was confirmed by the reduction of O2 on the surface of iron–carbon13,14 or bi-metals.15,16 This may be a promising way for the in situ generation of H2O2. However, ME processes with a low capacity of H2O2 generation due to the usage of unsuitable ME materials have limited the application. It has been reported that H2O2 could be generated by the reaction of Zn with O2,17–19 and the carbon nanotubes (CNTs) could improve the two-electron reduction of O2 during an electrochemical reaction because of their good electrical conductivity, high surface activity and mechanical strength.20,21 Therefore, it can be assumed that Zn-CNTs/O2 micro-electrolysis may have a high capacity of H2O2 generation. Moreover, the Zn-CNTs/O2 process has following advantages for Fenton degradation: (1) the active hydrogen [H] generated during the micro-electrolysis process has a high chemical activity;13,22 (2) the regeneration of Fe3+ can be improved by Zn0 and enables the maximal amount of ˙OH to be generated via the decompose of H2O2 by Fe2+; (3) the freshly formed Zn(OH)2 colloid through the reaction between Zn2+ and OH− during the micro-electrolysis process has a good adsorption capacity for the pollutants. In this study, 4-chlorophenol was selected as the model pollutant to assess the efficiency of the proposed Zn-CNTs/O2/Fe2+ system due to its high toxicity and extensive application.23,24
The objective of this study was to investigate the in situ generation of H2O2 from the micro-electrolysis process and its use for the degradation of 4-chlorophenol. A Zn-CNT composite was prepared, characterized and used for the reduction of dissolved O2 to generate H2O2. The generated H2O2 subsequently reacted with Fe2+, forming Fenton's reagent that oxidizes contaminants in the wastewater. The degradation of 4-CP in the secondary effluent of a municipal wastewater treatment plant was studied to examine the effect of wastewater composition on 4-CP degradation. The intermediate products were detected and the possible degradation pathway of 4-CP and the reaction mechanism of the Zn-CNTs/O2/Fe2+ process were tentatively proposed.
The morphology of Zn-CNTs was observed by using a transmission electron microscope (TEM) (HRTEM, JEM2100 and JEOL). The specific surface areas (BET) and the Barrett–Joyner–Halenda (BJH) pore size distribution of Zn-CNTs were determined by nitrogen adsorption–desorption isotherm measurements. X-ray photoelectron spectroscopy (XPS) analysis was performed by using an Al Kα X-ray (1486.6 eV) source for the excitation (NOVA 3200e).
To evaluate the effect of wastewater composition on the degradation of 4-CP, the secondary effluent of a municipal wastewater treatment plant spiked with 4-CP (25 mg L−1 or 50 mg L−1) was used. The secondary effluent of wastewater was collected at a local wastewater treatment plant (WWTP) and used as received within the next 2 days. The initial 4-CP and TOC of the secondary effluent were 0 mg L−1 and 9.17 ± 1 mg L−1, respectively.
The intermediate products were identified by HPLC-MS equipped with the above-mentioned column coupled to a Shimadzu 2010EV mass spectrometer with an ESI ion source (LC-MS 2010, Columbia, USA). It was equipped with a photo diode array (PDA) detector, and operated in a negative mode. The analysis of the intermediate products was performed under the aforementioned solvent conditions. The injected volume was 30 μL. The organic acids were determined by ion-exclusion chromatography.
Fig. 2 illustrates the N2 adsorption–desorption isotherms and BJH pore size distribution plots, which were determined from the adsorption branch of the N2 isotherms for the newly prepared and the used Zn-CNTs. The isotherms were identified as type IV and the hysteresis loops as type H3, which are the characteristics of mesoporous materials and have a slit pore of plate structure.
Fig. 2 N2 adsorption/desorption isotherms and pore size distributions of the newly prepared Zn-CNTs (a) and the used Zn-CNTs (b). |
The pore-size distribution obtained from the isotherm indicated that most of the pores were in the range 2 to 10 nm, and the average pore size was calculated to be 17 nm and 14 nm for the newly prepared and the used Zn-CNT composites, respectively. The BET specific surface areas were calculated from N2 isotherms, and were about 27 m2 g−1 and 63 m2 g−1 for the newly prepared and the used Zn-CNTs, respectively. The total pore volume was 0.12 cm3 g−1 for the newly prepared Zn-CNTs and 0.23 cm3 g−1 for the used Zn-CNTs. The extremely high BET surface area and large total pore volume strongly supported the fact that Zn-CNT composite had a porous structure, which was consistent with the result of the TEM images. Compared with the newly prepared Zn-CNTs, the increase of the BET specific surface area and total volume of the pores for the used Zn-CNTs may be due to the formation of small pores caused by the corrosion of zinc and the deposition of zinc oxide on the surface of Zn-CNTs during the reaction between Zn-CNTs and oxygen. The similar average pore size of the newly prepared Zn-CNTs and the used Zn-CNTs indicated that the pores of the Zn-CNTs were not seriously blocked by the formed precipitates during the reaction.
Surface analysis of the newly prepared Zn-CNTs and the used Zn-CNTs was carried out using XPS (Fig. 3). The peaks for O 1s and O KLL were observed at 529.6 and 995.0 eV, respectively. Additional peaks (525.9 and 535.4 eV) for Zn 2p indicated different chemical environments. The peak for C 1s at approximately 284.8 eV was observed. Compared with the newly prepared Zn-CNTs, Fe 2p peaks were observed, indicating that a lot of iron was deposited on the surface of the Zn-CNTs after the reaction of Zn-CNTs with Fe2+.
Fig. 3 XPS full survey spectra (a), Zn Auger KE spectra of the newly prepared Zn-CNTs (b), Zn Auger KE spectra of the used Zn-CNTs (c), Fe 2p spectra of the used Zn-CNTs (d). |
Fig. 3(b) and (c) exhibit the Auger KE of Zn in the newly prepared and the used Zn-CNT composites. From the standard data, the Auger KE of Zn0 was about 992.1 eV, while ZnO was at 987.7–988.5 eV. Thus, the peak at 991.7 eV could be assigned to Zn0,25 and the peak at 988.5 eV could be assigned to ZnO.26 Compared with the newly prepared Zn-CNTs, the peak at 986.4 eV was assigned to Zn(OH)2,27 which was observed for the used Zn-CNTs, demonstrating the interaction between Zn2+ and OH− species. The formation of Zn(OH)2 was consistent with the result of the TEM analysis. The Fe state in the used Zn-CNTs is shown in Fig. 3(d). The coexistence of Fe(0), Fe(I) and Fe(II) was evidenced by four shoulders. The main peak at 717.9 eV was assigned to the Fe(0) species.28 The higher binding energy Fe 2p3/2 peak at 710.7 eV and its shake-up satellites at 724.3 eV (2p1/2) were reported for Fe3O4.29 The peak at 712.5 eV corresponds to a satellite transition that is the characteristic feature of Fe2+,30 indicating that the interaction occurred between Zn0, Fe2+ and the oxidant.
Fig. 4 Variation of H2O2 concentration with reaction time at different initial pH values. Experimental conditions: O2 flow rate = 400 mL min−1, [Zn-CNTs] = 2.0 g L−1, T = 25 °C. |
It was noted that at the initial pHs of 2.0 and pH 6.0, the reaction of Zn-CNTs with O2 led to the formation of H2O2 and the concentration of H2O2 increased with reaction time. The concentration of H2O2 within 20 min was 19.5 and 103 mg L−1 at the initial pHs of 2.0 and 6.0, respectively. The formation of H2O2 was due to the micro-electrolysis process. In Zn-CNTs, Zn0 adhered to the surface of the CNTs and the numerous corrosion cells were formed between Zn0 particles and CNTs when they contacted wastewater. If dissolved O2 existed in the solution, H2O2 was generated due to the reduction of O2 in the cathode of the Zn0-CNT corrosion cells and the reactions are listed as follows (eqn (1)–(3)):
Anode:
Zn − 2e− → Zn2+ | (1) |
Cathode:
O2 + 2H+ + 2e− → H2O2 | (2) |
2H+ + 2e− → H2 | (3) |
In the acid solution, the competition of the reduction between H+ and O2 (shown in eqn (3)) led to a lower concentration of accumulated H2O2 at an initial pH of 2.0 than at an initial pH of 6.0.
It was reported that a certain concentration of H2O2 was found in the Zn0/O2 or Al0/O2 systems. However, the concentration of the generated H2O2 in the Zn0/O2 system was below 18 mg L−1 with a stoichiometry of the same dosage as that of Zn in a neutral solution.17–19 In the Al0/O2 process, the concentration of H2O2 was only 180 μM at an Al0 dosage of 5.0 g L−1 and reaction time of 250 min.15 Therefore, the in situ generation of H2O2 can be improved by the electrode reaction in the corrosion cell with Zn0 as the anode and the CNTs as the cathode, which favored the two-electron reduction of O2.
Fig. 5(b) shows that neither the Zn-CNTs/O2 nor the Fe2+/H2O2 system was efficient for TOC removal, with only 14.0% and 9.94% of TOC removed, respectively, after 20 min of reaction. Compared with the Zn-CNTs/O2 and Fe2+/H2O2 systems, the Zn-CNTs/O2/Fe2+ system led to an 87.4% TOC removal within 20 min, which clearly indicated that the combination of Zn-CNTs/O2 and Fe2+ had a synergetic effect. The 4-CP removal efficiency was quite similar to the TOC removal efficiency in the Zn-CNTs/O2 system, suggesting that a low degradation of 4-CP occurred in the Zn-CNTs/O2 system and the removal of 4-CP in the Zn-CNTs/O2 process was due to the adsorption of 4-CP by Zn-CNTs, which exhibited an excellent adsorption capacity for 4-CP and enhanced its degradation.
Therefore, the Zn-CNTs/O2/Fe2+ system is one of the most efficient electrochemical AOPs, consistent with the continuous production of ˙OH using Fenton oxidation with micro-electrolysis generated H2O2. The oxidation mechanisms of the Fenton oxidation process are shown in the following equations:
O2 +2H+ + 2e− → H2O2 | (4) |
H2O2 + Fe2+ → Fe3+ + OH− + ˙OH | (5) |
Fe3+ + H2O2 → Fe2+ + HO2˙ + H+ | (6) |
2Fe3+ + Zn → 2Fe2+ + Zn2+ | (7) |
It was reported that the rate of reaction (5) (k = 63–76 M−1 s−1) was more rapid than that of reaction (6) (k = (0.1–1.0) × 10−2 M−1 s−1), and the oxidative capability of ˙OH was higher than that of HO2˙.31,32 So, the regeneration of Fe2+ from Fe3+ played a key role in increasing the degradation rate of 4-CP by the Fenton oxidation process.33,34 In the Zn-CNTs/O2/Fe2+ process, the regeneration of the catalytic species (Fe2+ ions) was expected to occur via reactions (6) and (7). The regeneration of Fe2+ could be obtained from the intensification reduction of Fe3+ by Zn (eqn (6)), which produced enough Fe2+ to catalyze the H2O2 dissociation, which increased the mineralization rate of the pollutants. This was one of the reasons for the higher degradation efficiency of 4-CP in the Zn-CNTs/O2/Fe2+ system than in the Fe2+/H2O2 system. Moreover, in the Zn-CNTs/O2/Fe2+ system, the dissolved oxygen could improve the production of the ortho–para chlorophenolperoxyl radical (ClPP˙) and increase the extent of benzene ring cleavage. Therefore, 4-CP degradation in the Fenton/O2 system was better than that in the Fenton/N2 system.35,36
The high concentration of H2O2, the rapid regeneration of Fe2+ from the reduction of Fe3+ by Zn and the good adsorption capability of Zn-CNTs for 4-CP all contributed to the higher oxidative capability of the Zn-CNTs/O2/Fe2+ system. It was reported that 50 mg L−1 of 4-CP was completely degraded after 2 h in the bimetallic Al–Fe/O2 process, while after 20 min in the Zn-CNTs/O2/Fe2+ process, many active intermediate species of H2O2 could be generated.16 This result proved the effectiveness of the Zn-CNTs/O2/Fe2+ process, which might be a promising alternative for the degradation of recalcitrant organic pollutants in wastewaters.
In order to explain the effect of the initial pH on the removal efficiency of 4-CP, the variation of pH during the Zn-CNTs/O2/Fe2+ process was determined and is shown in Fig. 7(b). It was noted that the pH value increased gradually to be stable with a prolonged reaction time. The final pH was 2.1, 5.0, 5.3 and 6.6, respectively, when the initial pH was 1.0, 2.0, 3.0 and 4.0, respectively. Several processes performed simultaneously in the Zn-CNTs/O2/Fe2+ system, including the hydrolysis of the Zn(II) species or the Fe(III) species, the production of small-molecule organic acids, and the generation of H2O2 or H2 by the reduction of O2 or H+. H+ was released into the solution in the first two processes and consumed in the third process. At the beginning, the generation rate of H2O2 or H2 was faster than the consumption rate of H+, which led to the increase of pH. When the generation rate of H+ was equal to its consumption rate, the solution pH was kept stable in a relative narrow range. This variation trend of the solution pH during the Zn-CNTs/O2/Fe2+ process could lead to a low pH environment for pollutant degradation and high pH conditions for neutralization without chemical addition, which is an important advantage for its practical application.
˙OH + H2O2 → HO2˙/O2˙− + H2O | (8) |
As shown in reaction (8), if H2O2 was excess, a less oxidative radicals (HO2˙ and O2˙−) might be produced and a highly oxidative radical (˙OH) was consumed.40,41 The optimal Zn-CNTs dosage was 2.0 g L−1 in this experiment.
Fe2+ + H2O2 → Fe3+ + ˙OH | (9) |
Fe2+ + ˙OH → Fe3+ + OH− | (10) |
The intermediate products generated during the 4-CP degradation process by the Zn-CNTs/O2/Fe2+ system were determined by LC-MS analysis. Intermediates at m/z 143, m/z 191 and m/z 195 were observed in the aqueous phase, which indicated that the substitution reaction of ˙OH and the addition reaction of ˙OH were involved in the Zn-CNTs/O2/Fe2+ process. The appearance of intermediates at m/z 199 and m/z 91 suggested the occurrence of the opening ring of aromatics and dehalogenation in the degradation process. The intermediate at m/z 189 might be the oxidized product of the intermediate at m/z 199 by O2. Benzoquinone (BQ) was not detected, which indicated that the direct dechlorination of 4-CP by ˙OH attack could be neglected and 4-CP degradation was mainly by the 4-chlorocatechol (4CC) pathway in the Zn-CNTs/O2/Fe2+ system.23,35
As a result, the main degradation pathway is proposed in Fig. 10. According to previous studies, 4-chlorocatechol was rapidly formed when the reaction was initiated by the attack of ˙OH at the ortho-position of the hydroxyl group. 4-Chlorocatechol was attacked by the addition or substitution reaction of ˙OH to form chlorinated intermediates D2 and D3. D2 can be easily transformed into quinine D5. Then, the CC bond in the aromatic rings was cleaved by the attack of ˙OH to yield D4 and D6, which were oxidized to aliphatic carboxylic acid intermediates (e.g., formic acid, acetic acid, oxalic acid, etc.) that would be further mineralize into CO2 and H2O.
During the Zn-CNTs/O2/Fe2+ process, the formed Fe3+ ions could be reduced to Fe2+ via reactions (6) and (7). The transformation of Fe3+ into Fe2+ was enhanced by Zn0 in Zn-CNTs, which made enough Fe2+ to catalyze the H2O2 dissociation and improve the Fenton process.
Zn is classified as a low toxicity metal, and a very small amount of Zn2+ remained in the aqueous solution at the end of the reaction. During the Zn-CNTs/O2/F 2+ process, Zn2+ in solution could be converted into the low solubility Zn(OH)2 with a solubility product constant of 1.2 × 10−17 at pH 7 and 25 °C via the combination with the OH− generated due to the reduction of H+ and O2 (Fig. 7). Therefore, the secondary pollution of Zn2+ could be avoided. The newly formed Zn(OH)2 colloids with large specific surface areas had a high adsorption capacity for pollutants and improved the removal of pollutants.
The Zn-CNTs/O2/Fe2+ system was developed in this study in order to in situ generate H2O2 and directly supply it to the Fenton reaction, because H2O2 is not stable, and it is not convenient to transport and store it for practical industrial applications. The preparation of Zn-CNTs was very simple and could be easily scaled up, which makes the Zn-CNTs/O2/Fe2+ system available for large-scale wastewater treatment. In the Zn-CNTs/O2/Fe2+ system, CNTs were not consumed during the wastewater treatment; although H2O2 is an inexpensive chemical and CNTs may be expensive, the cost of wastewater treatment using this system should be evaluated compared to the conventional Fenton process in the future.
This journal is © The Royal Society of Chemistry 2017 |